# US 2024/0342822 A1 · Joining Method to Perform Defect-Free, Electron Beam Welds Using a Slope-Out Technique

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0342822 A1
- Document ID: US20240342822A1
- Status: Published application
- Kind: A1
- Application number: 18/746,249
- Filed: 2024-06-18
- Published: 2024-10-17
- Earliest claimed: 2020-04-28
- Inventors: Thomas Dutilleul
- Web page: https://patentgrep.com/patent/US20240342822A1

## CPC

- B23K 15/0053: {Seam welding}
- B23K 15/0013: {Positioning or observing workpieces, e.g. with respect to the impact; Aligning, aiming or focusing electron beams}
- B23K 15/006: {of rectilinear seams}
- B23K 15/04: for welding annular seams
- B23K 15/10: Non-vacuum electron beam-welding or cutting
- B23K 2101/12: Vessels
- B23K 2103/04: Steel {or steel} alloys
- B23K 2103/05: {Stainless steel}
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM

## Abstract

The present invention provides a modification to the EBW process, which is referred to as a slope-out methodology, the results in the formation of a “slope-out portion” located generally in that region of the overall weldment located at the end of the ordinary EBW welding process for joining two components. The slope-out portion overlaps with the initial weld of the workpiece for a given distance or length along the weld and effectively eliminates the keyhole and provides a weldment that has minimal to no defects, particularly in the slope-out portion. The slope-out methodology begins by adjusting various parameters related to the electron beam to essentially decay the beam. In general, the focus position of the electron beam is moved from under-focused (focal position in the bulk of the material) to over-focused (focal position ahead of the workpiece surface) as the overlapping weld is made.

## Claims

### Claim 1

A method for welding two components together, comprising:
welding two components using electron beam welding comprising an electron beam, wherein said welding is performed over a first period of time;
adjusting a focus of the electron beam from within the bulk of the two components to above the two components continuously and throughout a second period of time; and
adjusting a shape of an oscillation pattern of the electron beam within the second period of time;
wherein the second period of time starts within the first period of time and wherein the first period of time and the second period of time end concurrently.

### Claim 2 (depends on 1)

The method of claim 1, where said adjusting the focus of the electron beam comprises a linear rate of change.

### Claim 3 (depends on 1)

The method of claim 1, where said adjusting the focus of the electron beam comprises a non-linear rate of change.

### Claim 4 (depends on 1)

The method of claim 1, wherein said adjusting the shape of the oscillation pattern of the electron beam oscillation comprises widening the oscillation pattern.

### Claim 5 (depends on 1)

The method of claim 1, wherein the oscillation pattern comprises an elliptical pattern and wherein said adjusting the shape of the oscillation pattern comprises elongating the elliptical pattern.

### Claim 6 (depends on 5)

The method of claim 5, wherein the elliptical pattern is elongated perpendicular to a direction of said welding.

### Claim 7 (depends on 6)

The method of claim 6, further comprising:
elongating the elliptical pattern in the direction of said welding.

### Claim 8 (depends on 1)

The method of claim 1, further comprising:
reducing a current of the electron beam continuously during the second period of time.

### Claim 9 (depends on 8)

The method of claim 8, wherein said reducing the current of the electron beam comprises a linear rate of change.

### Claim 10 (depends on 8)

The method of claim 8, wherein said reducing the current of the electron beam comprises a non-linear rate of change.

### Claim 11

A method for circumferential welding of two components using electron beam welding, comprising:
forming a first weld portion using an electron beam that extends from a first position along the joint between two components to a second position adjacent to the first position;
forming a slope-out weld portion by forming a second weld portion that overlaps the first weld portion formed at the first position by a predetermined length;
adjusting a focus of the electron beam from within the bulk of the two components to above the two components continuously during said forming of the slope-out weld portion; and
adjusting a shape of an oscillation pattern of the electron beam during said forming of the slope-out weld portion.

### Claim 12 (depends on 11)

The method of claim 11, wherein the oscillation pattern comprises an elliptical pattern and wherein said adjusting the shape of the oscillation pattern comprises elongating the elliptical pattern.

### Claim 13 (depends on 12)

The method of claim 12, wherein the elliptical pattern is elongated perpendicular to a direction of welding.

### Claim 14 (depends on 13)

The method of claim 13, further comprising:
elongating the elliptical pattern in the direction of said welding.

### Claim 15 (depends on 11)

The method of claim 11, further comprising:
reducing a current of the electron beam continuously during said forming of the slope-out weld portion.

### Claim 16 (depends on 11)

The method of claim 11, wherein the second weld portion comprises a length of approximately 2-12 inches.

### Claim 17

A method for welding two components together, comprising:
welding a joint between two components using an electron beam, wherein said welding forms a weld having an initial portion formed at a start of said welding;
forming a slope-out weld portion that overlaps the initial portion of the weld;
adjusting a focus of the electron beam from within the bulk of the two components to above the two components continuously during said forming of the slope-out weld portion;
adjusting a shape of an oscillation pattern of the electron beam during said forming of the slope-out weld portion; and
reducing a current of the electron beam continuously during said forming of the slope-out weld portion.

### Claim 18 (depends on 17)

The method of claim 17, wherein the oscillation pattern comprises an elliptical pattern and wherein said adjusting the shape of the oscillation pattern comprises elongating the elliptical pattern.

### Claim 19 (depends on 18)

The method of claim 18, wherein the elliptical pattern is elongated perpendicular to a direction of welding.

### Claim 20 (depends on 19)

The method of claim 19, further comprising:
elongating the elliptical pattern in the direction of said welding.