# US 2024/0342787 A1 · Improved foundry core for manufacturing a hollow metal aeronautical part

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0342787 A1
- Document ID: US20240342787A1
- Status: Published application
- Kind: A1
- Application number: 18/579,343
- Filed: 2022-07-12
- Published: 2024-10-17
- Earliest claimed: 2021-07-16
- Assignees: Safran
- Applicants: Safran
- Inventors: Pierre Jean SALLOT; Mirna BECHELANY
- Web page: https://patentgrep.com/patent/US20240342787A1

## CPC

- B22C 1/00: Compositions of refractory mould or core materials; Grain structures thereof (refractory materials in general C04B35/00); Chemical or physical features in the formation or manufacture of moulds
- B22C 9/04: Use of lost patterns
- B22C 9/10: Cores; Manufacture or installation of cores {(breaker cores B22C9/084)}
- B22C 9/18: Finishing
- B22D 29/002: {by leaching, washing or dissolving}
- B22D 29/003: {using heat}
- B22C: FOUNDRY MOULDING (moulding refractory materials in general B28B)
- B22D: CASTING OF METALS; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES (shaping of plastics or substances in a plastic state B29C; metallurgical processing, selection of substances to be added to metal C21, C22)

## Abstract

Casting core for the manufacture of hollow metal aeronautical parts, in particular high-pressure turbine parts by lost-wax casting, including a composite material including on the one hand a first phase of formula Mn+1AlCn, where n=1 to 3 and M being a transition metal selected from the group consisting of titanium and/or niobium and/or molybdenum, the composite material including on the other hand a second phase of formula Al4C3.

## Claims

### Claim 1

A casting core for the manufacture of hollow metal aeronautical parts, in particular high-pressure turbine parts by lost-wax casting, comprising a composite material comprising on the one hand a first phase of formula Mn+1AlCn, where n=1 to 3 and M being a transition metal selected from the group consisting of titanium and/or niobium and/or molybdenum, the composite material comprising on the other hand a second phase of formula Al4C3.

### Claim 2 (depends on 1)

The casting core according to claim 1, wherein the first phase is of one of the formulae among Nb4AlC3, Nb2AlC, Mo2TiAlC2 or Ti2AlC.

### Claim 3 (depends on 1)

The casting core according to claim 1, wherein the composite material comprises between 1 and 50% second phase by volume of the composite material, preferably between 1 and 20%.

### Claim 4 (depends on 1)

The casting core according to claim 1, wherein an outer surface of the casting core is covered by a layer of alumina.

### Claim 5 (depends on 4)

The casting core according to claim 4, wherein the alumina layer has a thickness of between 1 and 50 μm.

### Claim 6

A method of manufacturing a casting core for making a hollow metal aeronautical part, in particular a high-pressure turbine part, by lost-wax casting, the casting core comprising a composite material comprising, on the one hand, a first phase of the formula Mn+1AlCn, where n=1 to 3 and M being a transition metal selected from the group consisting of titanium and/or niobium and/or molybdenum, the composite material also comprising a second phase of formula Al4C3, the casting core being obtained by a powder metallurgy process comprising a mixing step in which powders for obtaining the composite material are mixed, and a shaping step.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the mixing step comprises mixing pure powders constituting the first phase so as to obtain the first phase in powder form, then mixing said first phase in powder form with an Al4C3 powder so as to obtain the second phase.

### Claim 8 (depends on 6)

The method according to claim 6, wherein the mixing step comprises mixing pure powders constituting the first phase with excess Al4C3 powder so as to form the composite material in a single operation.

### Claim 9 (depends on 6)

The method according to claim 6, wherein the first phase is of the formula Ti2AlC, the method comprising, after the casting core shaping step, a core oxidation step enabling the formation of an alumina layer on a core surface.

### Claim 10 (depends on 6)

The method according to claim 6, in which the first phase is of one of the formulae Nb4AlC3, Nb2AlC and Mo2TiAlC2, the method comprising, after the step of shaping the casting core, a step of depositing an aluminoforming coating, followed by a step of oxidizing the coating to form a layer of alumina on a surface of the core.

### Claim 11 (depends on 6)

A lost-wax casting method for manufacturing a hollow metal aeronautical part, in particular a high-pressure turbine part, using a casting core obtained by the method according to claim 6 the method comprising, after steps of casting a molten metal around the casting core and solidifying said metal, a step of knockout the casting core by steaming.

### Claim 12 (depends on 11)

The method according to claim 11, comprising, prior to the knockout step, a step in which an opening is made in the part.

### Claim 13 (depends on 11)

The method according to claim 11, comprising, after the knockout step, a recovery step, in which the material knocked out by steaming is recovered so as to be reused for the manufacture of another casting core starting again from the mixing step.

### Claim 14 (depends on 6)

A method of manufacturing a ceramic-matrix composite hollow aeronautical part using a core obtained by the method according to claim 6, the method comprising, after steps of inserting the core into a fibrous preform, impregnating a ceramic matrix into the fibrous preform and solidifying the matrix, a step of knockout the core by steaming.