# US 2024/0339687 A1 · Serviceable Batteries with Reusable Electrodes

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0339687 A1
- Document ID: US20240339687A1
- Status: Published application
- Kind: A1
- Application number: 18/293,962
- Filed: 2022-07-25
- Published: 2024-10-10
- Earliest claimed: 2021-08-03
- Assignees: QuanVerge Inc.
- Applicants: QuanVerge Inc.
- Inventors: Stephen Robert Clarke
- Web page: https://patentgrep.com/patent/US20240339687A1

## CPC

- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- H01M 4/043: {involving compressing or compaction}
- H01M 4/14: Electrodes for lead-acid accumulators
- H01M 4/21: Drying of pasted electrodes
- H01M 4/48: of inorganic oxides or hydroxides
- H01M 4/626: {Metals}
- H01M 4/661: {Metal or alloys, e.g. alloy coatings (H01M4/669 take precedence)}
- H01M 10/0468: {Compression means for stacks of electrodes and separators}
- H01M 10/0486: {Frames for plates or membranes}
- H01M 10/08: Selection of materials as electrolytes
- H01M 10/10: Immobilising of electrolyte
- H01M 10/14: Assembling a group of electrodes or separators
- H01M 10/16: Suspending or supporting electrodes or groups of electrodes in the case
- H01M 10/18: with bipolar electrodes
- H01M 50/437: Glass
- H01M 50/494: Tensile strength
- H01M 2004/029: {Bipolar electrodes}
- Y02E 60/50: Fuel cells
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Various systems and methods are presented in which lead acid batteries are serviced by removal, reconditioning, and refilling reconditioned battery paste into an assembly of typically bipolar electrodes that may be retained in a reusable housing and/or compression mechanism. Preferably, such batteries will include electrodes having a layer of a Magneli phase of a transition metal suboxide to so provide enhanced electrochemical and mechanical strength. and the battery paste may further include porous particles a Magneli phase of a transition metal suboxide to so provide enhanced electrolyte performance.

## Claims

### Claim 1

An axial current flow battery, comprising:
a plurality of bipole electrodes, wherein each bipole electrode is in contact with positive active material (PAM) on a first surface area and negative active material (NAM) on a second surface area opposite the first surface area;
wherein each bipole electrode comprises a conductive substrate that is coated with a continuous layer of a Magneli phase transition metal to so form the first and second surface areas;
wherein each bipole electrode further comprises a seal that circumferentially encloses the PAM and/or the NAM;
a plurality of separators, each being disposed between the PAM of one bipole electrode and the NAM of another bipole electrode;
a frame and/or a housing, wherein the frame and/or the housing includes a compression mechanism that retains and compresses the plurality of bipole electrodes in a stacked configuration; and
wherein the conductive substrate and the continuous layer of the Magneli phase transition metal maintain structural and functional integrity over a plurality of disassembly-NAM/PAM replacement-reassembly cycles for the axial current flow battery.

### Claim 2 (depends on 1)

The axial current flow battery of claim 1, wherein the conductive substrate is stainless steel, copper, aluminum, or titanium.

### Claim at position 3

3-14. (canceled)

### Claim 15 (depends on 1)

The axial current flow battery of claim 1, wherein the conductive substrate has a thickness of between 0.5 mm and 5 mm, and/or wherein the continuous layer of the Magneli phase transition metal has a thickness of between about 10 and 500 nm.

### Claim 16 (depends on 1)

The axial current flow battery of claim 1, wherein the first and second surface areas each have an area of between 50 cm2 and 50,000 cm2.

### Claim 17 (depends on 1)

The axial current flow battery of claim 1, wherein the Magneli phase transition metal is TinO(2n-1) where (4≤n≤10) or VnO2n-1 (3≤n≤9).

### Claim 18 (depends on 1)

The axial current flow battery of claim 1, wherein at least 80% of a surface area of the conductive substrate is coated with the Magneli phase transition metal.

### Claim 19 (depends on 1)

The axial current flow battery of claim 1, wherein the continuous layer of the Magneli phase transition metal further comprises a metal catalyst selected from the group consisting of platinum, palladium, vanadium, ruthenium, and silver.

### Claim 20 (depends on 1)

The axial current flow battery of claim 1, wherein the seal is an elastomeric seal, and optionally wherein the seal is coupled to the bipole electrode via a seal retaining structure in the bipole electrode.

### Claim 21 (depends on 1)

The axial current flow battery of claim 1, wherein the plurality of disassembly-NAM/PAM replacement-reassembly cycles is at least ten cycles.

### Claim 22 (depends on 1)

The axial current flow battery of claim 1, wherein the separator comprises a compression resistant material.

### Claim 23 (depends on 1)

The axial current flow battery of claim 1, wherein the separator comprises an absorbent glass mat.

### Claim 24 (depends on 1)

The axial current flow battery of claim 1, wherein the separator comprises a liquid or gelled electrolyte.

### Claim 25 (depends on 1)

The axial current flow battery of claim 1, wherein the frame and/or the housing is configured to retain between 5 and 50 bipole electrodes.

### Claim 26 (depends on 1)

The axial current flow battery of claim 1, wherein the compression mechanism comprises a plurality of tension rods or one or more compression rams or compression levers.

### Claim at position 16

27-55. (canceled)

### Claim 56 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26)

A method of servicing an axial current flow battery, comprising:
providing an axial current flow battery of any one of claims 1-26;
using the compression mechanism of the frame and/or the housing to decompress and release the plurality of bipole electrodes;
replacing
(a) the PAM and/or NAM with new or reconditioned PAM and/or NAM;
(b) the seal;
(c) the separator; and/or
(d) the bipole electrode
stacking the bipole electrodes with the new or reconditioned PAM and/or NAM, the replaced seal, and/or the replaced separator; and
placing the stacked bipole electrodes into the frame and/or the housing and using the compression mechanism to retain and compress the bipole electrodes in the stacked configuration.

### Claim 57 (depends on 56)

The method of claim 56, wherein at least two of (a), (b), (c), and (d) are replaced.

### Claim 58 (depends on 56)

The method of claim 56, wherein at least three of (a), (b), (c), and (d) are replaced.

### Claim 59 (depends on 56)

The method of claim 56, wherein the new or reconditioned PAM and/or NAM are provided as pre-shaped PAM and/or NAM wafers.

### Claim 60 (depends on 1, 2, 3, 4, 5, 6, 7, 8, 9, 10, 11, 12, 13, 14, 15, 16, 17, 18, 19, 20, 21, 22, 23, 24, 25, 26)

A method of servicing an energy consuming entity, wherein at least some of the energy used by the entity is provided by a lead acid battery, comprising:
locating a lead acid battery in the entity, and optionally removing the lead acid battery from the entity, wherein the lead acid battery is a battery according to any one of claims 1-26;
replacing at least some active material of the lead acid battery with reconditioned active material;
where the lead acid battery was removed,
installing the lead acid battery with the reconditioned active material, or
installing a different replacement lead acid battery that contains reconditioned active material; and
optionally recharging the lead acid battery or replacement battery; and
wherein physical integrity of the housing or housing portions and the electrodes of the lead acid battery is maintained in a disassembly process while the active material is removed and replaced with the reconditioned active material.

### Claim 61

(canceled)

### Claim 62 (depends on 60)

The method of claim 60, wherein in the step of replacing at least some of the active material of the battery with reconditioned active material, the reconditioned material is prepared from the active material of the battery, or the reconditioned material is prepared from an active material of a different lead acid battery.

### Claim at position 24

63-75. (canceled)