# US 2024/0336491 A1 · Methods for extracting lithium from brines

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0336491 A1
- Document ID: US20240336491A1
- Status: Published application
- Kind: A1
- Application number: 18/295,443
- Filed: 2023-04-04
- Published: 2024-10-10
- Earliest claimed: 2023-04-04
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: Peng LU; Pan LUO
- Web page: https://patentgrep.com/patent/US20240336491A1

## CPC

- C01D 15/08: Carbonates; Bicarbonates
- C01D 3/06: Preparation by working up brines; seawater or spent lyes
- C01D 15/04: Halides
- C01F 5/00: Compounds of magnesium
- C01F 5/22: from magnesium compounds with alkali hydroxides or alkaline- earth oxides or hydroxides
- C01F 5/34: Dehydrating magnesium chloride containing water of crystallisation
- C01F 11/00: Compounds of calcium, strontium, or barium (C01F7/00 takes precedence)
- C01F 11/18: Carbonates
- C01F 11/46: Sulfates (dehydration of gypsum {for the production of calcium sulfate cements} C04B11/02)
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 26/10: Obtaining alkali metals
- C22B 26/12: Obtaining lithium
- C22B 26/20: Obtaining alkaline earth metals or magnesium
- C22B 26/22: Obtaining magnesium
- C01D: COMPOUNDS OF ALKALI METALS, i.e. LITHIUM, SODIUM, POTASSIUM, RUBIDIUM, CAESIUM, OR FRANCIUM (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides C01B17/22; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia and cyanogen, containing nitrogen and other non-metals C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; phosphides C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS

## Abstract

Methods for extracting lithium from brines may include evaporating at least a portion of a brine using a number of one or more solar evaporation ponds to form a first slurry. A first solid may be separated from the first slurry and combined with an amount of a first precipitation additive to form a second slurry. A first liquid may be separated from the second slurry and at least a portion of the first liquid may be evaporated in a solar evaporation pond to form a third slurry. A second liquid may be separated from the third slurry and combined with an amount of a second precipitation additive to form a fourth slurry. A second solid may be separated from the fourth slurry and rehydrated, forming a fifth slurry. About 90 wt % or more of a salt in a solid product separated from the fifth slurry may be lithium carbonate.

## Claims

### Claim 1

A method comprising:
evaporating at least a portion of a brine using a number of one or more solar evaporation ponds to form a first slurry;
wherein a concentration of magnesium in the brine is about 100 ppm to about 50,000 ppm and a concentration of lithium in the brine is about 0.01 ppm to about 5,000 ppm;
wherein the number of one or more solar evaporation ponds is a first output of a geochemical prediction model;
separating a first solid from the first slurry;
combining the first solid with an amount of a first precipitation additive comprising soda ash, slaked lime, or a combination thereof, to form a second slurry comprising magnesium hydroxide, magnesium carbonate, or a combination thereof;
wherein the amount of the first precipitation additive is a second output of the geochemical prediction model;
separating a first liquid from the second slurry;
evaporating at least a portion of the first liquid in a solar evaporation pond to form a third slurry;
separating a second liquid from the third slurry;
combining the second liquid with an amount of a second precipitation additive comprising soda ash to form a fourth slurry comprising lithium carbonate;
wherein the amount of the second precipitation additive is a third output of the geochemical prediction model;
separating a second solid from the fourth slurry;
rehydrating the second solid to form a fifth slurry; and
separating a solid product from the fifth slurry, wherein about 90 wt % or more of a salt in the solid product is lithium carbonate.

### Claim 2 (depends on 1)

The method of claim 1, wherein a ratio of total dissolved solids concentration to lithium concentration in the brine is about 1,500 ppm to about 1,000,000 ppm and a concentration of sodium in the brine is less than about 90,000 ppm.

### Claim 3 (depends on 1)

The method of claim 1, wherein the geochemical prediction model is a Harvie-Møller-Weare model.

### Claim 4 (depends on 1)

The method of claim 1, wherein the first precipitation additive further comprises caustic soda.

### Claim 5 (depends on 1)

The method of claim 1, wherein the first slurry has a concentration of total dissolved solids of about 200,000 ppm to about 500,000 ppm.

### Claim 6 (depends on 1)

The method of claim 1, wherein the third slurry has a concentration of total dissolved solids of about 200,000 ppm to about 1,000,000 ppm.

### Claim 7 (depends on 1)

The method of claim 1, wherein the brine further comprises calcium, sodium, potassium, chloride, bicarbonate, sulfate, or any combination thereof.

### Claim 8

A method comprising:
evaporating at least a portion of a brine using a number of one or more solar evaporation ponds to form a first slurry;
wherein a concentration of magnesium in the brine is about 100 ppm to about 50,000 ppm and a concentration of lithium in the brine is about 0.01 ppm to about 5,000 ppm;
wherein the number of one or more solar evaporation ponds is a first output of a geochemical prediction model;
separating a first liquid from the first slurry;
combining the first liquid with an amount of a first precipitation additive comprising soda ash, slaked lime, or a combination thereof, to form a second slurry comprising magnesium hydroxide, magnesium carbonate, or a combination thereof;
wherein the amount of the first precipitation additive is a second output of the geochemical prediction model;
separating a second liquid from the second slurry;
evaporating at least a portion of the second liquid in a solar evaporation pond to form a third slurry;
separating a third liquid from the third slurry;
combining the third liquid with an amount of a second precipitation additive comprising soda ash to form a fourth slurry comprising lithium carbonate;
wherein the amount of the second precipitation additive is a third output of the geochemical prediction model;
separating a first solid from the fourth slurry;
rehydrating the first solid to form a fifth slurry; and
separating a solid product from the fifth slurry, wherein about 90 wt % or more of a salt in the solid product is lithium carbonate.

### Claim 9 (depends on 8)

The method of claim 8, wherein a ratio of total dissolved solids concentration to lithium concentration in the brine is about 1,500 ppm to about 1,000,000 ppm and a concentration of sodium in the brine is about 90,000 ppm to about 1,000,000 ppm.

### Claim 10 (depends on 8)

The method of claim 8, wherein the geochemical prediction model is a Harvie-Møller-Weare model.

### Claim 11 (depends on 8)

The method of claim 8, wherein the first precipitation additive further comprises caustic soda.

### Claim 12 (depends on 8)

The method of claim 8, wherein the first slurry has a concentration of total dissolved solids of about 200,000 ppm to about 500,000 ppm.

### Claim 13 (depends on 8)

The method of claim 8, wherein the third slurry has a concentration of total dissolved solids of about 200,000 ppm to about 1,000,000 ppm.

### Claim 14 (depends on 8)

The method of claim 8, wherein the brine further comprises calcium, sodium, potassium, chloride, bicarbonate, sulfate, or any combination thereof.

### Claim 15

A method comprising:
evaporating at least a portion of a brine using a number of one or more solar evaporation ponds to form a first slurry;
wherein a concentration of magnesium in the brine is about 100 ppm to about 50,000 ppm and a concentration of lithium in the brine is about 0.01 ppm to about 5,000 ppm;
wherein the number of one or more solar evaporation ponds is a first output of a geochemical prediction model;
separating a first liquid from the first slurry;
combining the first liquid with an amount of a first precipitation additive comprising soda ash, slaked lime, or a combination thereof, to form a second slurry comprising magnesium hydroxide, magnesium carbonate, or a combination thereof;
wherein the amount of the first precipitation additive is a second output of the geochemical prediction model;
separating a second liquid from the second slurry;
combining the second liquid with an amount of a second precipitation additive comprising soda ash to form a third slurry comprising lithium carbonate;
wherein the amount of the second precipitation additive is a third output of the geochemical prediction model;
separating a first solid from the third slurry;
rehydrating the first solid to form a fourth slurry; and
separating a solid product from the fourth slurry, wherein about 90 wt % or more of a salt in the solid product is lithium carbonate.

### Claim 16 (depends on 15)

The method of claim 15, wherein a ratio of total dissolved solids concentration to lithium concentration in the brine is less than about 1,500 ppm.

### Claim 17 (depends on 15)

The method of claim 15, wherein the geochemical prediction model is a Harvie-Møller-Weare model.

### Claim 18 (depends on 15)

The method of claim 15, wherein the first precipitation additive further comprises caustic soda.

### Claim 19 (depends on 15)

The method of claim 15, wherein the first slurry has a concentration of total dissolved solids of about 200,000 ppm to about 500,000 ppm.

### Claim 20 (depends on 15)

The method of claim 15, wherein the brine further comprises calcium, sodium, potassium, chloride, bicarbonate, sulfate, or any combination thereof.