# US 2024/0327940 A1 · A method and associated system to characterize an alloy's hardenability for finite element analysis

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0327940 A1
- Document ID: US20240327940A1
- Status: Published application
- Kind: A1
- Application number: 18/579,332
- Filed: 2022-07-14
- Published: 2024-10-03
- Earliest claimed: 2021-07-15
- Assignees: Integrated Heat Treating Solutions, LLC
- Applicants: Integrated Heat Treating Solutions, LLC
- Inventors: Joseph A Powell; William Stuehr
- Web page: https://patentgrep.com/patent/US20240327940A1

## CPC

- C21D 1/55: Hardenability tests, e.g. end-quench tests
- C21D 1/56: characterised by the quenching agents
- G01N 33/20: Metals
- C21D: MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUS METALS OR ALLOYS; MAKING METAL MALLEABLE, e.g. BY DECARBURISATION OR TEMPERING (surface treatment of metallic material involving at least one process provided for in class C23 and at least one process covered by this subclass C23F17/00; unidirectional solidification of eutectic materials or unidirectional demixing of eutectoid materials C30B)
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

A system and apparatus for conducting a modified Jominy end-quench test of a metal composition having an Austenitizing temperature and a critical cooling rate may comprise a bar, comprising the metal composition, said bar having a hemispherical tip and a bar length. The system may also comprise a bar receptacle. The system may also comprise a quenchant. Additionally, the system may also comprise a quenchant discharge apparatus as a quenchant nozzle. In the system a portion of the hemispherical tip of the bar passes through a portion of the bar receptacle, exposing it to a quenchant exiting the quenchant nozzle with a gap existing between the quenchant nozzle and the hemispherical tip of the bar. This is useful in characterizing an alloy's hardenability and residual stresses for finite element analysis and part design.

## Claims

### Claim 1

A system for conducting a modified Jominy end-quench test of a metal composition having an Austenitizing temperature and a critical cooling rate comprising:
a bar comprising the metal composition, said bar having a hemispherical tip and a bar length;
a bar receptacle comprising a rigid collar with a top surface, a bottom surface opposite the top surface, a through hole from the top surface through the bottom surface, and a brace;
a quenchant;
a quenchant discharge apparatus comprising a quenchant nozzle; and
wherein a portion of the hemispherical tip of the bar passes through the through hole to form an exposed portion of the hemispherical tip of the bar which is located between the bar receptacle and the quenchant nozzle with a gap existing between the quenchant nozzle and the hemispherical tip.

### Claim 2 (depends on 1)

The system of claim 1, wherein the quenchant nozzle is configured to discharge the quenchant to cool at least the exposed portion of the hemispherical tip of the bar at a cooling rate equal to or greater than a critical cooling rate of the metal composition of the bar.

### Claim 3 (depends on 1)

The system of of claim 1, further comprising a shield attached to the bar receptacle.

### Claim 4 (depends on 1)

The system of claim 1, further comprising a reinforcement, connecting the bar receptacle and the shield.

### Claim 5 (depends on 1)

The system of claim 1, wherein the gap between the quenchant nozzle and the hemispherical tip is between 5 millimeter and 5 centimeters.

### Claim 6 (depends on 1)

The system of claim 1, wherein the gap between the quenchant nozzle and the hemispherical tip is between 5 millimeter and 2.5 centimeters.

### Claim 7 (depends on 1)

The system of claim 1, wherein the system is configured to cool the exposed portion of the hemispherical tip without film boiling.

### Claim 8 (depends on 1)

A method using the system of claim 1 to determine at least one property of the metal composition, said method comprising:
A. heating at least a surface of the bar at the exposed portion of the hemispherical tip of the bar to a temperature greater than or equal to the Austenitizing temperature;
B. passing at least a portion of the hemispherical tip of the bar through the through hole of the bar receptacle;
C. shielding all but the exposed portion of the hemispherical tip of the bar to keep the quenchant from contacting any surface of the bar other than the exposed portion of the hemispherical tip of the bar;
D. contacting the exposed portion of the hemispherical tip of the bar with the quenchant; and
E. analyzing the bar for the at least one property.

### Claim 9 (depends on 8)

The method of claim 8, wherein the exposed portion of the hemispherical tip of the bar is contacted with the quenchant at a pressure greater than a boiling pressure of the quenchant at the through temperature of the bar and at a quenchant flow renewal rate for a time.

### Claim 10 (depends on 8)

The method of claim 8, wherein the at least one property is selected from a group consisting of ultimate hardenability, compressive stresses, tensile stresses, crystal structure, grain size, hardness, and combinations thereof.

### Claim 11 (depends on 8)

The method of claim 8, wherein the metal composition is in the shape of a bar is heated to at least the Austenitizing temperature using induction heating.

### Claim 12 (depends on 8)

The method of claim 8, wherein the hemispherical tip is cooled by the quenchant at an initial cooling rate equal to or greater than the critical cooling rate of the metal composition.

### Claim 13 (depends on 8)

The method of claim 8, wherein the quenchant exiting the quenchant nozzle is located between 5 millimeters and 5 centimeters from the hemispherical tip.

### Claim 14 (depends on 8)

The method of claim 8, wherein the quenchant exiting the quenchant nozzle is located between 5 millimeters and 2.5 centimeters from the hemispherical tip.

### Claim 15 (depends on 8)

The method of claim 8, wherein the method further comprises analyzing compressive surface stresses along the bar length.

### Claim 16 (depends on 8)

The method of claim 8, wherein the method further comprises determining the ultimate hardenability of the metal composition of the bar through measuring hardness at a plurality of depths.