# US 2024/0327284 A1 · Admixture for cement

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0327284 A1
- Document ID: US20240327284A1
- Status: Published application
- Kind: A1
- Application number: 18/294,416
- Filed: 2022-09-08
- Published: 2024-10-03
- Earliest claimed: 2021-09-13
- Assignees: Sika Technology AG
- Applicants: Sika Technology AG
- Inventors: Liucheng ZHOU; Hailang GAO; Linyue YANG; Yalei CHEN
- Web page: https://patentgrep.com/patent/US20240327284A1

## CPC

- C04B 24/2605: {containing polyether side chains}
- C04B 24/2647: {containing polyether side chains}
- C04B 7/13: Mixtures thereof with inorganic cementitious materials, e.g. Portland cements
- C04B 7/323: {Calcium aluminosulfate cements, e.g. cements hydrating into ettringite}
- C04B 7/52: Grinding {; After-treatment of ground cement}
- C04B 28/001: {containing unburned clay (polymer binder - clay mixtures used in well cementing C09K8/44)}
- C04B 28/04: Portland cements
- C04B 28/06: Aluminous cements (monolithic refractories or refractory mortars C04B35/66)
- C04B 28/065: {Calcium aluminosulfate cements, e.g. cements hydrating into ettringite}
- C04B 40/0039: {Premixtures of ingredients}
- C04B 2103/006: {Comb polymers}
- C04B 2103/308: {Slump-loss preventing agents}
- C04B 2103/52: Grinding aids; Additives added during grinding
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

An admixture for cement, including: A) a comb polymer comprising the following partial structural units or consisting thereof: a) a mole fractions of a partial structural unit S1 of formula (I) b) b mole fractions of a partial structural unit S2 of formula (II) where M, Ru, Rv, m and R1 are as defined in the invention; and B) optionally, alkanol amine. The admixture for cement can provide remarkable improvement effects, particularly in milling aid effect, water-reducing properties, slump, fluidity and strength, for cements containing inferior or cheap mineral aggregate.

## Claims

### Claim 1

Admixture for cement, comprising:
A) a comb polymer comprising the following partial structural units or consisting thereof:
a) a mole fractions of a partial structural unit S1 of formula (I)
b) b mole fractions of a partial structural unit S2 of formula (II)
where M independently of one another represents H+, an alkali metal ion, alkaline earth metal ion, a bivalent or trivalent metal ion, an ammonium ion or an organic ammonium group,
each Ru independently of one another stands for hydrogen or a methyl group,
each Rv independently of one another stands for hydrogen or COOM,
m=0, 1 or 2,
R1 independently of one another stands for —Y—R4,
where
Y stands for a divalent poly(alkyleneoxy) group containing a moiety of -[EO]n—, in which E is a C2-alkylene group and n=35 to 85, and
R4 stands for H, a C1 to C20-alkyl group or -alkylaryl, or cyclohexyl group,
with the proviso that a/b is in a range of (2.6-3.8): 1; and
B) optionally, alkanol amine.

### Claim 2 (depends on 1)

Admixture according to claim 1, wherein the comb polymer comprise no more than 5 wt % of any other partial structural unit.

### Claim 3 (depends on 1)

Admixture according to claim 1, wherein Y stands for a poly(alkyleneoxy) group consisting of (C2- to C4-alkylene-O—) units wherein the molar ratio of C2-alkylene-O-units (EO) is at least 90% based on the total poly(alkyleneoxy) group.

### Claim 4 (depends on 1)

Admixture according to claim 1, wherein Y stands for a poly(alkyleneoxy) group consisting of the moiety of -[EO]n—.

### Claim 5 (depends on 1)

Admixture according to claim 1, wherein the comb polymer is consisting of the partial structures S1 and S2.

### Claim 6 (depends on 1)

Admixture according to claim 1, wherein the alkanol amine is selected from diethanol isopropanol amine (DEIPA), ethanol diisopropanol amine (EDIPA), triisopropanol amine (TIPA), triethanol amine (TEA), diethanol amine (DEA), methyldiethanol amine (MDEA).

### Claim 7 (depends on 1)

Admixture according to claim 1, wherein the admixture contains 0-50 wt % of the alkanol amine and 10-65 wt % of the comb polymer, based on the total weight of the admixture.

### Claim 8 (depends on 1)

Admixture according to claim 1, wherein the admixture contains further defoamers and/or diols.

### Claim 9 (depends on 1)

Cement composition, characterized by comprising a cement and an admixture for cement as defined in claim 1.

### Claim 10 (depends on 9)

Cement composition according to claim 9, wherein the cement is selected from sulphoaluminate cement and masonry cement.

### Claim 11 (depends on 9)

Cement composition according to claim 9, wherein the cement is Portland cement and the cement composition additionally comprises limestone and at least one clay mineral.

### Claim 12 (depends on 11)

Cement composition according to claim 11, wherein a weight ratio of Portland cement to at least one clay mineral is from 33:1 to 1:1.

### Claim 13 (depends on 11)

Cement composition according to claim 11, wherein a weight ratio of Portland cement to limestone is from 20:1 to 1:4.

### Claim 14 (depends on 11)

Cement composition according to claim 11, wherein a weight ratio of at least one clay mineral to limestone is from 10:1 to 1:33.

### Claim 15 (depends on 9)

Cement composition according to claim 9, wherein the dosage of the admixture for cement is in a range of 0.01 to 0.50 wt %, based on the weight of the cement.

### Claim 16 (depends on 9)

Cement composition according to claim 9, wherein the amount of the comb polymer is in a range of 150 ppm to 1400 ppm, based on the weight of the cement.

### Claim 17 (depends on 9)

Cement composition according to claim 9, wherein the cement contains less than 70 wt % of clinker, based on the weight of the cement.

### Claim 18 (depends on 9)

Cement composition according to claim 9, wherein the cement contains more than 17 wt % of limestone, based on the total weight of the cement.

### Claim 19 (depends on 1)

A method for preparing a cement mixture, wherein the method comprises milling in presence of an admixture for cement as defined in claim 1 in a mill at least one main cement constituent or all of the main cement constituents.

### Claim 20 (depends on 19)

Method according to claim 19, wherein the dosage of the admixture for cement is 0.01-0.50 wt % based on the weight of the cement.

### Claim 21 (depends on 1)

A method for reducing the fluidity loss of a cement, comprising adding the comb polymer as defined in claim 1 into the cement in a dosage of 150 ppm to 1400 ppm, based on the weight of the cement, before or during milling.

### Claim 22 (depends on 21)

Method according to claim 21, wherein the cement is selected from sulphoaluminate cement and masonry cement or is a combination of Portland cement, limestone, and at least one clay mineral.

### Claim 23 (depends on 21)

Method according to claim 21, wherein the cement contains less than 70 wt % of clinker, based on the weight of the cement.

### Claim 24 (depends on 21)

Method according to claim 21, wherein the cement contains more than 17 wt % of limestone, based on the weight of the cement.