# US 2024/0322373 A1 · High power density and low-cost lithium-ion battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0322373 A1
- Document ID: US20240322373A1
- Status: Published application
- Kind: A1
- Application number: 18/572,853
- Filed: 2022-06-29
- Published: 2024-09-26
- Earliest claimed: 2021-06-30
- Assignees: Ten Incorporated,
- Applicants: |-Ten
- Inventors: Fabien GABEN
- Web page: https://patentgrep.com/patent/US20240322373A1

## CPC

- H01M 4/0404: {by coating on electrode collectors}
- H01M 50/46: Separators, membranes or diaphragms characterised by their combination with electrodes
- H01M 4/0407: {by coating on an electrolyte layer}
- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/5825: {Oxygenated metallic salts or polyanionic structures, e.g. borates, phosphates, silicates, olivines}
- H01M 4/625: {Carbon or graphite}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/0568: characterised by the solutes
- H01M 10/0569: characterised by the solvents
- H01M 10/347: {with solid electrolyte}
- H01M 50/11: having a chip structure, e.g. micro-sized batteries integrated on chips
- H01M 50/431: Inorganic material
- H01M 50/491: Porosity
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2220/20: Batteries in motive systems, e.g. vehicle, ship, plane
- H01M 2300/0028: characterised by the solvent
- H01M 2300/0071: Oxides
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Lithium-ion battery comprising at least one stack which comprises successively: a first electronic current collector, a first porous electrode made of a material selected from the group formed by Nb2−xM1xO5−δM3δ, Nb18−xM1xW16−yM2yO93−δM3δ, Nb16−xM1xW5−yM2yO55−δM3δ, Nb2O5−δ with 0≤δ≤2, Nb18W16O93−δ with 0≤δ≤2, Nb16W5O55−δ with 0≤δ≤2, Li4Ti5O12 and Li4Ti5−xMxO12 with M=V, Zr, Hf, Nb, Ta and 0≤x≤0.25, a porous separator made of an electronically insulating inorganic material, a second porous electrode made of a phosphate or a lithium oxide, and a second electronic current collector, knowing that the electrolyte of said battery is a liquid charged with lithium ions confined in said porous layers, each of the three porous layers being free of binder and having a porosity comprised between 20% and 70% by volume.

## Claims

### Claim 1

A lithium-ion battery comprising at least one stack,
the stack comprises successively: a first electronic current collector, a first porous electrode, a porous separator, a second porous electrode, and a second electronic current collector,
the battery comprises an electrolyte which is a liquid charged with lithium ions,
the electrolyte is confined in the porous layers,
wherein in said battery:
said first electrode is an anode and comprises a porous layer made of a material PA selected from the group formed by:
Nb2−xM1xO5−δM3δ wherein
M1 is at least one element selected from the group consisting of Nb, V, Ta, Fe, Co, Ti, Bi, Sb, As, P, Cr, Mo, W, B, Na, Mg, Ca, Ba, Pb, Al, Zr, Si, Sr, K, Ge, Ce, Cs and Sn;
M3 is at least one halogen,
and where 0≤x≤1 and 0≤δ≤2,
Nb18−xM1xW16−yM2yO93−δM3δ wherein
M1 and M2 are at least one element selected from the group consisting of Nb, V, Ta, Fe, Co, Ti, Bi, Sb, As, P, Cr, Mo, W, B, Na, Mg, Ca, Ba, Pb, Al, Zr, Si, Sr, K, Ge, Ce, Cs and Sn;
M1 and M2 can be identical or different from each other,
M3 is at least one halogen,
and where 0≤x≤1, 0≤y≤2 and 0≤δ≤2,
Nb16−xM1xW5−yM2yO55−δM3δ wherein
M1 and M2 are at least one element selected from the group consisting of Nb, V, Ta, Fe, Co, Ti, Bi, Sb, As, P, Cr, Mo, W, B, Na, Mg, Ca, Ba, Pb, Al, Zr, Si, Sr, K, Ge, Ce, Cs and Sn;
M1 and M2 can be identical or different from each other,
M3 is at least one halogen,
and where 0≤x≤1, 0≤y≤2 and 0≤δ≤2,
Nb2O5−δ with 0≤δ≤2, Nb18W16O93−δ with 0≤δ≤2, Nb16W5O55−δ with 0≤δ≤2, Li4Ti5O12 and Li4Ti5−xMxO12 with M=V, Zr, Hf, Nb, Ta and 0≤x≤0.25 and wherein a part of the oxygen atoms can be substituted by halogen atoms and/or which can be doped by halogen atoms, and said layer being free of binder, having a porosity comprised between 20% and 70% by volume,
said separator comprises a porous inorganic layer made of an electronically insulating inorganic material E, preferably selected from:
Al2O3, SiO2, ZrO2, and/or
a material selected from lithiated phosphates, optionally containing at least one element from: Al, Ca, B, Y, Sc, Ga, Zr; or from lithiated borates which may optionally contain at least one element from: Al, Ca, Y, Sc, Ga, Zr;
said material preferably being selected from the group formed by lithiated phosphates, preferably selected from: lithiated phosphates of the NaSICON type, Li3PO4; LiPO3; Li3Al0.4Sc1.6(PO4)3 called «LASP»; Li1+xZr2−xCax(PO4)3 with 0≤x≤0.25; Li1+2xZr2−xCax(PO4)3 with 0≤x<0.25 such as Li1.2Zr1.9Ca0.1(PO4)3 or Li1.4Zr1.8Ca0.2(PO4)3; LiZr2(PO4)3; Li1+3xZr2(P1−xSixO4)3 with 1.8<x<2.3; Li1+6xZr2(P1−xBxO4)3 with 0≤x≤0.25; Li3(Sc2−xMx)(PO4)3 with M=Al or Y and 0≤X≤1; Li1+xMx(Sc)2−x(PO4)3 with M=Al, Y, Ga or a mixture of these three elements and 0≤x<0.8; Li1+xMx(Ga1−yScy)2−x(PO4)3 with 0≤x≤0.8; 0≤y≤1 and M=Al and/or Y; Li1+xMx(Ga)2−x(PO4)3 with M=Al and/or Y and 0≤x≤0.8; Li1+xAlxTi2−x(PO4)3 with 0≤x≤1 called «LATP»; or Li1+xAlxGe2−x(PO4)3 with 0≤x≤1 called «LAGP»; or Li1+x+2Mx(Ge1−yTiy)2−xSizP3−zO12 with 0≤x≤0.8 and 0≤y≤1.0 and 0≤z≤0.6 and M=Al, Ga or Y or a mixture of two or three of these elements; Li3+y(Sc2−xMx)QyP3−yO12 with M=Al and/or Y and Q=Si and/or Se, 0≤x≤0.8 and 0≤y≤1; or Li1+x+yMxSc2−xQyP3−yO12 with M=Al, Y, Ga or a mixture of these three elements and Q=Si and/or Se, 0≤x≤0.8 and 0≤y≤1; or Li1+x+y+zMx(Ga1−yScy)2−xQzP3−zO12 with 0≤x≤0.8, 0≤y≤1, 0≤z≤0.6 with M=Al and/or Y and Q=Si and/or Se; or Li1+xZr2−xBx(PO4)3 with 0≤x≤0.25; or Li1+xM3xM2−xP3O12 with 0≤x≤1 and M3=Cr, V, Ca, B, Mg, Bi and/or Mo, M=Sc, Sn, Zr, Hf, Se or Si, or a mixture of these elements;
said porous inorganic layer being free of binder, having a porosity comprised between 20% and 70% by volume;
said second electrode is a cathode and comprises a porous layer made of a material PC selected from the group formed by:
LiFePO4,
phosphates of formula LiFeMPO4 where M is selected from Mn, Ni, Co, V,
oxides LiMn2O4, Li1+xMn2−xO4 with 0<x<0.15, LiCoO2, LiNiO2, LiMn1.5Ni0.5O4, LiMn1.5Ni0.5−xXxO4 where X is selected from Al, Fe, Cr, Co, Rh, Nd, other rare earths such as Sc, Y, Lu, La, Ce, Pr, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, and wherein 0<x<0.1, LiMn2−xMxO4 with M=Er, Dy, Gd, Tb, Yb, Al, Y, Ni, Co, Ti, Sn, As, Mg or a mixture of these compounds and wherein 0<x<0.4, LiFeO2, LiMn1/3Ni1/3Co1/3O2, LiNi0.8Co0.15Al0.05O2, LiAlxMn2−xO4 with 0≤x<0.15, LiNi1/xCo1/yMn1/2O2 with x+y+z=10;
oxides LixMyO2 where 0.6≤y≤0.85 and 0≤x+y≤2, and M is selected from Al, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Zr, Nb, Mo, Ru, Sn, and Sb or a mixture of these elements; Li1.20Nb0.20Mn0.60O2;
Li1+xNbyMezApO2 where A and Me are each at least one transition metal selected from: Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Y, Zr, Nb, Mo, Tc, Ru, Rh, Pd, Ag, Cd, Hf, Ta, W, Re, Os, Ir, Pt, Au, Hg, and wherein 0.6<x<1; 0<y<0.5; 0.25≤z<1; with A≠Me and A≠Nb, and 0≤p≤0.2;
LixNby−aNaMz−bPbO2−cFc where 1.2<x≤1.75; 0≤y<0.55; 0.1<z<1; 0≤a<0.5; 0≤b<0.1; 0≤c<0.8; and where M, N, and P are each at least one of the elements selected from the group consisting of Ti, Ta, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Al, Zr, Y, Mo, Ru, Rh, and Sb;
oxides Li1.25Nb0.25Mn0.50O2; Li1.3Nb0.3Mn0.40O2; Li1.3Nb0.3Fe0.40O2; Li1.3Nb0.43 Ni0.27O2; Li1.3Nb0.43Co0.27O2; Li1.4Nb0.2Mn0.53O2;
oxides LixNi0.2Mn0.6Oy where 0.00≤x≤1.52; 1.07≤y<2.4; Li1.2Ni0.2Mn0.6O2;
compounds Li1.9Mn0.95O2.05F0.95, LiVPO4F, FeF3, FeF2, CoF2, CuF2, NiF2, Fe1−xMxOF where 0<x<0.2 and M is at least one element selected from the group consisting of Co, Ni, Mn and Cu,
oxides LiNixCoyMn1−x−yO2 where 0≤x and y≤0.5; LiNixCezCoyMn1−x−yO2 where 0≤x and y≤0.5 and 0≤z,
said porous layer being free of binder, having a porosity comprised between 20% and 70% by volume, said separator comprising a porous inorganic layer deposited on said first and/or second electrode, said porous inorganic layer being free of binder, having a porosity comprised between 20% and 70% by volume.

### Claim 2 (depends on 1)

The battery according to claim 1, wherein at least one of the two porous layers includes, on and inside its pores, an electronically conductive material coating, said electronically conductive material preferably being carbon or an electronically conductive oxide material, and more preferably an electronically conductive oxide material selected from:
tin oxide (SnO2), zinc oxide (ZnO), indium oxide (In2O3), gallium oxide (Ga2O3), a mixture of two of these oxides such as indium-tin oxide corresponding to a mixture of indium oxide (In2O3) and tin oxide (SnO2), a mixture of three of these oxides or a mixture of these four oxides,
doped oxides based on zinc oxide, the doping being preferably with gallium (Ga) and/or with aluminium (Al) and/or with boron (B) and/or with beryllium (Be), and/or with chromium (Cr) and/or with cerium (Ce) and/or with titanium (Ti) and/or with indium (In) and/or with cobalt (Co) and/or with nickel (Ni) and/or with copper (Cu) and/or with manganese (Mn) and/or with germanium (Ge),
doped oxides based on indium oxide, the doping being preferably with tin (Sn), and/or with gallium (Ga) and/or with chromium (Cr) and/or with cerium (Ce) and/or with titanium (Ti) and/or with indium (In) and/or with cobalt (Co) and/or with nickel (Ni) and/or with copper (Cu) and/or with manganese (Mn) and/or with germanium (Ge),
doped tin oxides, the doping being preferably with arsenic (As) and/or with fluorine (F) and/or with nitrogen (N) and/or with niobium (Nb) and/or with phosphorus (P) and/or with antimony (Sb) and/or with aluminium (Al) and/or with titanium (Ti), and/or with gallium (Ga) and/or with chromium (Cr) and/or with cerium (Ce) and/or with indium (In) and/or with cobalt (Co) and/or with nickel (Ni) and/or with copper (Cu) and/or with manganese (Mn) and/or with germanium (Ge).

### Claim 3 (depends on 2)

The battery according to claim 2, wherein said electronically conductive material coating is coated with a layer which is electronically insulating and which has ionic conductivity, the thickness of said layer preferably being comprised between 1 nm and 20 nm.

### Claim 4 (depends on 1)

The battery according to claim 1, wherein the pores of said first electrode have an average diameter of less than 50 nm.

### Claim 5 (depends on 1)

The battery according to claim 1, wherein said stack including a first porous electrode layer, a porous separator and a second porous electrode layer, is impregnated with an electrolyte.

### Claim 6 (depends on 5)

The battery according to claim 5, wherein said electrolyte is selected from the group formed by:
an electrolyte composed of at least one aprotic solvent and at least one lithium salt;
an electrolyte composed of at least one ionic liquid or ionic polyliquid and at least one lithium salt;
a mixture of at least one aprotic solvent and at least one ionic liquid or ionic polyliquid and at least one lithium salt;
a polymer made ionically conductive by the addition of at least one lithium salt; and
a polymer made ionically conductive by the addition of a liquid electrolyte, either in the polymer phase or in the mesoporous structure.

### Claim 7 (depends on 1)

The battery according to claim 1, wherein said material PA is Li4Ti5O12 and/or in that said material PC is LiFePO4 and/or in that said material E is Li3PO4.

### Claim 8 (depends on 1)

The battery according to claim 1, wherein said material PA is Li4Ti5O12, said material PC is LiMn2O4 and said material E is Li3PO4.

### Claim 9 (depends on 1)

The battery according to claim 1, wherein said material PA is Li4Ti5O12, said material PC is LiMn1.5Ni0.5O4 and said material E is Li3PO4.

### Claim 10 (depends on 1)

The battery according to claim 1, wherein said material PA is Li4Ti5O12, said material PC is LiNi1/xCo1/yMn1/2O2 with x+y+z=10, and said material E is Li3PO4.

### Claim 11 (depends on 1)

A method for manufacturing a lithium-ion battery, according to claim 1, wherein:
said battery comprising comprises at least one stack;
the stack comprises successively: a first electronic current collector, a first porous electrode, a porous separator, a second porous electrode, and a second electronic current collector;
the battery comprises an electrolyte which is a liquid charged with lithium ions;
the electrolyte is confined in said porous layers;
said manufacturing method implementing a method for manufacturing an assembly including a first porous electrode and a porous separator;
said first electrode comprising a porous layer deposited on a substrate, said layer being free of binder, having a porosity comprised between 20% and 70% by volume, said separator comprising a porous inorganic layer deposited on said electrode, said porous inorganic layer being free of binder, having a porosity comprised between 20% and 70% by volume, wherein in said manufacturing method being characterised in that:
(a) a first porous electrode layer is deposited on said substrate,
(a1) said first electrode layer being deposited from a first colloidal suspension;
(a2) said layer obtained in step (a1) then being dried and consolidated, by pressing and/or heating, to obtain a first porous electrode; and, optionally,
(a3) said porous layer obtained in step (a2) then receiving, on and inside its pores, an electronically conductive material coating;
being understood that:
said first porous electrode layer may have been deposited on said first electronic current collector by carrying out the sequence of steps (a1) and (a2), and if necessary step (a3), or
said layer of a first electrode may have been previously deposited on an intermediate substrate in step (a1), dried and then detached from said intermediate substrate to be subjected to consolidation by pressing and/or heating to obtain a first porous electrode, then placed on said first electronic current collector, and said first porous electrode may have been subjected to step (a3);
(b) a porous inorganic layer of an inorganic material E which must be an electronic insulator is deposited on said first porous electrode deposited or placed in step (a),
(b1) said layer of a porous inorganic layer being deposited from a second colloidal suspension of particles of material E;
(b2) said layer obtained in step (b1) then being dried, preferably under a flow of air, and a heat treatment is carried out at a temperature below 600° C., preferably below 500° C., to obtain a porous inorganic layer, in order to obtain said assembly consisting of a porous electrode and a porous separator;
being understood that
the porous inorganic layer may have been deposited on said first electrode layer, by carrying out the sequence of steps (b1) and (b2), or the inorganic layer may have been previously deposited on an intermediate substrate in step (b1), dried and then detached from said intermediate substrate to be subjected, before or after being placed on said first electrode layer, to consolidation by pressing and/or heating to obtain a porous inorganic layer;
said first porous electrode layer and said porous inorganic layer are deposited by a technique selected from the group formed by: electrophoresis, extrusion, a printing method, preferably selected from ink-jet printing and flexographic printing, and a coating method, preferably selected from roll coating, curtain coating, doctor blade coating, extrusion slot die coating, dip-coating;
said first porous electrode layer and said porous inorganic layer are deposited from colloidal solutions including either
aggregates or agglomerates of monodisperse primary nanoparticles of at least one active material PA or PC of first electrode, or of at least one inorganic material E, respectively, with an average primary diameter D50 comprised between 2 nm and 100 nm, said aggregates or agglomerates having an average diameter D50 comprised between 50 nm and 300 nm, or
non-agglomerated or non-aggregated primary particles of at least one active material PA or PC of first electrode, or of at least one inorganic material E, respectively, with a primary diameter D50 comprised between 200 nm and 10 μm,
knowing that:
if said first porous electrode is intended to be used in said battery as an anode, said material PA is selected from the group formed by:
Nb2−xM1xO5−δM3δ wherein
M1 is at least one element selected from the group consisting of Nb, V, Ta, Fe, Co, Ti, Bi, Sb, As, P, Cr, Mo, W, B, Na, Mg, Ca, Ba, Pb, Al, Zr, Si, Sr, K, Ge, Ce, Cs and Sn;
M3 is at least one halogen, preferably selected from F, Cl, Br, I or a mixture thereof
and wherein 0≤x≤1 and 0≤δ≤2,
Nb18−xM1xW16−yM2yO93−δ M3δ wherein
M1 and M2 are at least one element selected from the group consisting of Nb, V, Ta, Fe, Co, Ti, Bi, Sb, As, P, Cr, Mo, W, B, Na, Mg, Ca, Ba, Pb, Al, Zr, Si, Sr, K, Ge, Ce, Cs and Sn;
M1 and M2 can be identical or different from each other,
M3 is at least one halogen, preferably selected from F, Cl, Br, I or a mixture thereof,
and wherein 0≤x≤1, 0≤y≤2 and 0≤δ≤2,
Nb16xM1xW5−yM2yO55−δ M3δ wherein
M1 and M2 are at least one element selected from the group consisting of Nb, V, Ta, Fe, Co, Ti, Bi, Sb, As, P, Cr, Mo, W, B, Na, Mg, Ca, Ba, Pb, Al, Zr, Si, Sr, K, Ge, Ce, Cs and Sn;
M1 and M2 can be identical or different from each other,
M3 is at least one halogen, preferably selected from F, Cl, Br, I or a mixture thereof,
and wherein 0≤x≤1, 0≤y≤2 and 0≤δ≤2,
Nb2O5−δ with 0≤δ≤2, Nb18W16O93−δ with 0≤δ≤2, Nb16W5O55−δ with 0≤δ≤2, Li4Ti5O12 and Li4Ti5−xMxO12 with M=V, Zr, Hf, Nb, Ta and 0≤x≤0.25 and wherein a part of the oxygen atoms can be substituted by halogen atoms and/or which can be doped by halogen atoms;
and if said first porous electrode is intended to be used in said battery as a cathode, said material PC is selected from the group formed by:
LiFePO4,
phosphates of formula LiFeMPO4 where M is selected from Mn, Ni, Co, V,
oxides LiMn2O4, Li1+xMn2−xO4 with 0<x<0.15, LiCoO2, LiNiO2, LiMn1.5Ni0.5O4, LiMn1.5Ni0.5−xXxO4 where X is selected from Al, Fe, Cr, Co, Rh, Nd, other rare earths such as Sc, Y, Lu, La, Ce, Pr, Pm, Sm, Eu, Gd, Tb, Dy, Ho, Er, Tm, Yb, and wherein 0<x<0.1, LiMn2−xMxO4 with M=Er, Dy, Gd, Tb, Yb, Al, Y, Ni, Co, Ti, Sn, As, Mg or a mixture of these compounds and wherein 0<x<0.4, LiFeO2, LiMn1/3Ni1/3Co1/3O2, LiNi0.8Co0.15Al0.05O2, LiAlxMn2−xO4 with 0≤x<0.15, LiNi1/xCo1/yMn1/2O2 with x+y+z=10;
oxides LixMyO2 where 0.6≤y<0.85 and 0≤x+y≤2, and M is selected from Al, Ti, Cr, Mn, Fe, Co, Ni, Cu, Zn, Zr, Nb, Mo, Ru, Sn, and Sb or a mixture of these elements; Li1.20Nb0.20Mn0.60O2;
Li1+xNbyMezApO2 where A and Me are each at least one transition metal selected from: Sc, Ti, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Y, Zr, Nb, Mo, Tc, Ru, Rh, Pd, Ag, Cd, Hf, Ta, W, Re, Os, Ir, Pt, Au, Hg, and wherein 0.6<x<1; 0<y<0.5; 0.25≤z<1; with A≠Me and A≠Nb, and 0≤p≤0.2;
LixNby−aNaMz−bPbO2−cFc where 1.2<x≤1.75; 0≤y<0.55; 0.1<z<1; 0≤a<0.5; 0≤b<0.1; 0≤c<0.8; and where M, N, and P are each at least one of the elements selected from the group consisting of Ti, Ta, V, Cr, Mn, Fe, Co, Ni, Cu, Zn, Al, Zr, Y, Mo, Ru, Rh, and Sb;
oxides Li1.25Nb0.25Mn0.50O2; Li1.3Nb0.3Mn0.40O2; Li1.3Nb0.3Fe0.40O2; Li1.3Nb0.43 Ni0.27O2; Li1.3Nb0.43Co0.27O2; Li1.4Nb0.2Mn0.53O2;
oxides LixNi0.2Mn0.6Oy where 0.00≤x≤1.52; 1.07≤y<2.4; Li1.2Ni0.2Mn0.6O2;
compounds Li1.9Mn0.95O2.05F0.95, LiVPO4F, FeF3, FeF2, CoF2, CuF2, NiF2, Fe1−xMxOF where 0≤x<0.2 and M is at least one element selected from the group consisting of Co, Ni, Mn and Cu,
oxides LiNixCoyMn1−x−yO2 where 0≤x and y≤0.5; LiNixCezCoyMn1−x−yO2 where 0≤x and y≤0.5 and 0≤z.

### Claim 12 (depends on 11)

The method according to claim 11, wherein a second porous electrode layer is deposited on said porous inorganic layer, in a step (c), to obtain a stack comprising a first porous electrode layer, a porous inorganic layer and a second porous electrode layer,
(c1) said second porous electrode layer being deposited from a third colloidal suspension by a technique preferably selected from the group formed by: electrophoresis, extrusion, a printing method, preferably selected from ink-jet printing and flexographic printing, and a coating method, preferably selected from roll coating, curtain coating, doctor blade coating, extrusion slot die coating, dip-coating, said third colloidal suspension comprising either aggregates or agglomerates of monodisperse primary nanoparticles of at least one active material PA or PC of the second electrode, with an average primary diameter D50 comprised between 2 nm and 100 nm, preferably between 2 nm and 60 nm, said aggregates or agglomerates having an average diameter D50 comprised between 50 nm and 300 nm, that is to say non-agglomerated or non-aggregated primary particles of at least one active material PA or PC of the second electrode, with a primary diameter D50 comprised between 200 nm and 10 μm; and
(c2) said layer obtained in step (c1) having then been consolidated, by pressing and/or heating, to obtain a porous layer; and, optionally,
(c3) said porous layer obtained in step (c2) then receiving, on and inside its pores, an electronically conductive material coating, so as to form said second porous electrode;
it being understood that said second porous electrode layer may have been deposited on said second electronic current collector by carrying out the sequence of steps (c1) and (c2), and where appropriate (c3), or said layer of a second electrode may have been deposited beforehand on an intermediate substrate by carrying out the sequence of steps (c1) and (c2), and if necessary (c3), and then has been detached from said intermediate substrate to be placed on said porous inorganic layer,
and it being understood that in the case where said first electrode layer has been made from a material PA, said second electrode layer is made with a material PC, and that in the case where said first electrode layer was made from a material PC, said second electrode layer is made with a material PA.

### Claim 13 (depends on 11)

The method according to claim 11, wherein a second assembly consisting of a second porous electrode and a second layer of porous separator is deposited on a first assembly including a first porous electrode and a first layer of porous separator, so that said second separator layer is deposited or placed on said first separator layer, to obtain a stack comprising a first porous electrode layer, a porous inorganic layer and a second porous electrode layer.

### Claim 14 (depends on 11)

The method according to claim 11, wherein the deposition of said electronically conductive material coating is carried out by the atomic layer deposition technique, or by immersion in a liquid phase including a precursor of said electronically conductive material, followed by the transformation of said precursor into an electronically conductive material.

### Claim 15 (depends on 11)

The method according to claim 11, wherein said electronically conductive material is carbon or in that said electronically conductive material is selected from In2O3, SnO2, ZnO, Ga2O3 and a mixture of one or several of these oxides.

### Claim 16 (depends on 15)

The method according to claim 15, wherein said precursor is a carbon-rich compound, such as a carbohydrate, and in that said transformation into electronically conductive material is pyrolysis, preferably under an inert atmosphere.

### Claim 17 (depends on 11)

The method according to claim 11, wherein a layer of an electronic insulator having ionic conductivity is deposited above said electronically conductive material coating.

### Claim 18 (depends on 11)

The method according to claim 11, wherein said porous layer of a first electrode has a thickness comprised between 4 μm and 400 μm.

### Claim 19 (depends on 11)

The method according to claim 11, wherein said porous inorganic layer has a thickness comprised between 3 μm and 20 μm, and preferably between 5 μm and 10 μm.

### Claim 20 (depends on 11)

The method according to claim 11, wherein said porous layer of a first electrode has a specific surface comprised between 10 m2/g and 500 m2/g.

### Claim 21 (depends on 11)

The method according to claim 11, wherein said inorganic material E comprises an electronically insulating material, preferably selected from:
Al2O3, SiO2, ZrO2, and/or
a material selected from lithiated phosphates, optionally containing at least one element from: Al, Ca, B, Y, Sc, Ga, Zr; or from lithiated borates which may optionally contain at least one element from: Al, Ca, Y, Sc, Ga, Zr;
said material preferably being selected from the group formed by lithiated phosphates, preferably selected from: lithiated phosphates of the NaSICON type, Li3PO4: LiPO3; Li3Al0.4Sc1.6(PO4)3 called «LASP»; Li1+xZr2−xCax(PO4)3 with 0≤x≤0.25; Li1+2xZr2−xCax(PO4)3 with 0≤x≤0.25 such as Li1.2Zr1.9Ca0.1(PO4)3 or Li1.4Zr1.8Ca0.2(PO4)3; LiZr2(PO4)3; Li1+3xZr2(P1−xSixO4)3 with 1.8<x<2.3; Li1+6xZr2(P1−xBxO4)3 with 0≤x≤0.25; Li3(Sc2−xMx)(PO4)3 with M=Al or Y and 0≤x≤1; Li1+xMx(Sc)2−x(PO4)3 with M=Al, Y, Ga or a mixture of these three elements and 0≤x≤0.8; Li1+xMx(Ga1−yScy)2−x(PO4)3 with 0≤x≤0.8; 0≤y≤1 and M=Al and/or Y; Li1+xMx(Ga)2−x(PO4)3 with M=Al and/or Y and 0≤x≤0.8; Li1+xAlxTi2−x(PO4)3 with 0≤x≤1 called «LATP»; or Li1+xAlxGe2−x(PO4)3 with 0≤x≤1 called «LAGP»; or Li1+x+zMx(Ge1−yTiy)2−xSizP3−zO12 with 0≤x≤0.8 and 0≤y≤1.0 and 0≤z≤0.6 and M=Al, Ga or Y or a mixture of two or three of these elements; Li3+y(Sc2−xMx)QyP3−yO12 with M=Al and/or Y and Q=Si and/or Se, 0≤x≤0.8 and 0≤y≤1; or Li1+x+yMxSc2−xQyP3−yO12 with M=Al, Y, Ga or a mixture of these three elements and Q=Si and/or Se, 0≤x≤0.8 and 0≤y≤1; or Li1+x+y+zMx(Ga1−yScy)2−xQzP3−zO12 with 0≤x≤0.8, 0≤y≤1, 0≤z≤0.6 with M=Al and/or Y and Q=Si and/or Se; or Li1+xZr2−xBx(PO4)3 with 0≤x<0.25; or Li1+xM3xM2−xP3O12 with 0≤x≤1 and M3=Cr, V, Ca, B, Mg, Bi and/or Mo, M=Sc, Sn, Zr, Hf, Se or Si, or a mixture of these elements.

### Claim 22 (depends on 11)

The method according to claim 11, wherein the cathode current collector is made of a material selected from the group formed by: Mo, W, Ti, Cr, Ni, Al, stainless steel, electronically conductive carbon and/or the anode current collector is made of a material selected from the group formed by: Cu, Mo, W; Ta, Ti, Cr, stainless steel, electronically conductive carbon.

### Claim 23 (depends on 11)

The method according to claim 11, wherein said stack including a first porous electrode layer, a porous separator and a second porous electrode layer is impregnated with an electrolyte, preferably a lithium-ion carrier phase, selected from the group formed by:
an electrolyte composed of at least one aprotic solvent and at least one lithium salt;
an electrolyte composed of at least one ionic liquid or ionic polyliquid and at least one lithium salt;
a mixture of at least one aprotic solvent and at least one ionic liquid or ionic polyliquid and at least one lithium salt;
a polymer made ionically conductive by the addition of at least one lithium salt; and
a polymer made ionically conductive by the addition of a liquid electrolyte, either in the polymer phase or in the mesoporous structure,
said polymer preferably being selected from the group formed by poly(ethylene oxide), poly(propylene oxide), polydimethylsiloxane, polyacrylonitrile, poly(methyl methacrylate), poly(vinyl chloride), poly(vinylidene fluoride), PVDF-hexafluoropropylene.

### Claim 24 (depends on 1)

A method implementing the battery according to claim 1, wherein the battery is used at a temperature below −10° C. and/or at a temperature above +80° C.

### Claim 25 (depends on 1)

The battery according to claim 1, the pores of said inorganic layer have an average diameter of less than 50 nm.

### Claim 26 (depends on 1)

The battery according to claim 1, wherein the pores of said second electrode have an average diameter of less than 50 nm.

### Claim 27 (depends on 3)

The battery according to claim 3, wherein the thickness of the layer is comprised between 1 nm and 20 nm.