# US 2024/0322074 A1 · Semiconductor element and manufacturing method for semiconductor element

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0322074 A1
- Document ID: US20240322074A1
- Status: Published application
- Kind: A1
- Application number: 18/260,980
- Filed: 2022-01-11
- Published: 2024-09-26
- Earliest claimed: 2021-01-12
- Assignees: Nichia Corporation
- Applicants: Nichia Corporation
- Inventors: Takuya KADOWAKI; Tadashi KAWAZOE
- Web page: https://patentgrep.com/patent/US20240322074A1

## CPC

- H10H 20/8215: {characterised by crystalline imperfections, e.g. dislocations; characterised by the distribution of dopants, e.g. delta-doping}
- H10H 20/8262: {characterised by the dopants}
- H10F 30/221: the potential barrier being a PN homojunction
- H10F 77/206: {for devices having potential barriers}
- H10H 20/014: {having light-emitting regions comprising only Group IV materials}
- H10H 20/831: characterised by their shape
- H10H: INORGANIC LIGHT-EMITTING SEMICONDUCTOR DEVICES HAVING POTENTIAL BARRIERS
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION

## Abstract

A method of manufacturing a semiconductor element includes: providing a semiconductor stack including: a silicon substrate containing a first impurity of a first conductivity type that is one of p-type and n-type, at a first concentration, and a silicon semiconductor layer provided on the silicon substrate, the silicon semiconductor layer including: a first silicon semiconductor layer containing a second impurity of the first conductivity type at a second concentration that is lower than the first concentration, and a second silicon semiconductor layer containing a third impurity of a second conductivity type that is the other of p-type and n-type; and irradiating the silicon semiconductor layer with light having a predetermined peak wavelength in a presence of a forward current flowing through the silicon semiconductor layer such that the third impurity is diffused. The predetermined peak wavelength is longer than a wavelength corresponding to a magnitude of a bandgap of silicon.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A method of manufacturing a semiconductor element, the method comprising:
providing a semiconductor stack comprising:
a silicon substrate containing a first impurity of a first conductivity type that is one of p-type and n-type, at a first concentration, and
a silicon semiconductor layer provided on the silicon substrate, the silicon semiconductor layer comprising:
a first silicon semiconductor layer containing a second impurity of the first conductivity type at a second concentration that is lower than the first concentration, and
a second silicon semiconductor layer containing a third impurity of a second conductivity type that is the other of p-type and n-type; and
irradiating the silicon semiconductor layer with light having a predetermined peak wavelength in a presence of a forward current flowing through the silicon semiconductor layer such that the third impurity is diffused; wherein:
the predetermined peak wavelength is longer than a wavelength corresponding to a magnitude of a bandgap of silicon.

### Claim 15 (depends on 14)

The method of claim 14, wherein:
providing the semiconductor stack comprises:
providing the silicon substrate containing a first impurity of a first conductivity type that is one of p-type and n-type, at a first concentration,
forming the silicon semiconductor layer on the silicon substrate, the silicon semiconductor layer comprising the first silicon semiconductor layer containing a second impurity of the first conductivity type at a second concentration that is lower than the first concentration, and
introducing, into a surface of the silicon semiconductor layer, a third impurity of a second conductivity type that is the other of p-type and n-type, thereby forming the second silicon semiconductor layer.

### Claim 16 (depends on 14)

The method of claim 14, further comprising:
reducing a thickness of the silicon substrate before irradiating the silicon semiconductor layer with the light having the predetermined peak wavelength such that the third impurity is diffused.

### Claim 17 (depends on 15)

The method of claim 15, further comprising:
reducing a thickness of the silicon substrate before irradiating the silicon semiconductor layer with the light having the predetermined peak wavelength such that the third impurity is diffused.

### Claim 18 (depends on 14)

The method of claim 14, wherein:
the irradiating of the silicon semiconductor layer with the light having the predetermined peak wavelength comprises irradiating the silicon semiconductor layer with the light having the predetermined peak wavelength in the presence of the forward current flowing through the silicon semiconductor layer while the silicon substrate is located on a heat dissipation plate.

### Claim 19 (depends on 15)

The method of claim 15, wherein:
the irradiating of the silicon semiconductor layer with the light having the predetermined peak wavelength comprises irradiating the silicon semiconductor layer with the light having the predetermined peak wavelength in the presence of the forward current flowing through the silicon semiconductor layer while the silicon substrate is located on a heat dissipation plate.

### Claim 20 (depends on 14)

The method of claim 14, wherein:
the first concentration is equal to or higher than 1×1017 cm−3 and equal to or lower than 1×1021 cm−3, and
the second concentration is equal to or higher than 1×1014 cm−3 and equal to or lower than 1×1016 cm−3.

### Claim 21 (depends on 17)

The method of claim 17, wherein:
the first concentration is equal to or higher than 1×1017 cm−3 and equal to or lower than 1×1021 cm−3, and
the second concentration is equal to or higher than 1×1014 cm−3 and equal to or lower than 1×1016 cm−3.

### Claim 22 (depends on 14)

The method of claim 14, comprising:
after forming the second silicon semiconductor layer and before irradiating the silicon semiconductor layer with the light having the predetermined peak wavelength, forming a first upper electrode on a surface of the silicon semiconductor layer, the first upper electrode comprising a light-transmitting region configured to transmit the light having the predetermined peak wavelength.

### Claim 23 (depends on 21)

The method of claim 21, comprising:
after forming the second silicon semiconductor layer and before irradiating the silicon semiconductor layer with the light having the predetermined peak wavelength, forming a first upper electrode on a surface of the silicon semiconductor layer, the first upper electrode comprising a light-transmitting region configured to transmit the light having the predetermined peak wavelength.

### Claim 24 (depends on 22)

The method of claim 22, further comprising:
removing the first upper electrode; and
forming a second upper electrode for use in operation of the semiconductor element on a part of the surface of the silicon semiconductor layer.

### Claim 25 (depends on 14)

The method of claim 14, wherein:
the semiconductor element is a semiconductor photodetector or a semiconductor light-emitting element.

### Claim 26

A semiconductor element comprising:
a silicon substrate containing a first impurity of a first conductivity type that is one of p-type and n-type, at a first concentration; and
a silicon semiconductor layer provided on the silicon substrate, wherein:
the silicon semiconductor layer comprises a first silicon semiconductor layer and a second silicon semiconductor layer in this order from the silicon substrate side, the first silicon semiconductor layer containing a second impurity of the first conductivity type at a second concentration that is lower than the first concentration, the second silicon semiconductor layer containing a third impurity of a second conductivity type that is the other of p-type and n-type,
the silicon semiconductor layer comprises a pn junction located between the first silicon semiconductor layer and the second silicon semiconductor layer, and
in a region including the pn junction, the semiconductor element has a photosensitivity for light whose peak wavelength is longer than a wavelength corresponding to a magnitude of a bandgap of silicon, or the semiconductor element emits light whose peak wavelength is longer than the wavelength corresponding to the magnitude of the bandgap of silicon.

### Claim 27 (depends on 26)

The semiconductor element of claim 26, wherein:
the first concentration is equal to or higher than 1×1017 cm−3 and equal to or lower than 1×1021 cm−3, and
the second concentration is equal to or higher than 1×1014 cm−3 and equal to or lower than 1×1016 cm−3.

### Claim 28 (depends on 26)

The semiconductor element of claim 26 wherein:
at zero bias, the photosensitivity for light whose peak wavelength is equal to or longer than 1.2 μm and equal to or shorter than 2.0 μm is equal to or higher than 2.0×10−6 W and equal to or lower than 7.0×10−6 A/W.

### Claim 29 (depends on 27)

The semiconductor element of claim 27 wherein:
at zero bias, the photosensitivity for light whose peak wavelength is equal to or longer than 1.2 μm and equal to or shorter than 2.0 μm is equal to or higher than 2.0×10−6 A/W and equal to or lower than 7.0×10−6 A/W.

### Claim 30 (depends on 26)

The semiconductor element of claim 26 wherein:
in a case where a temperature of an object under measurement is 25° C., an absolute value of a ratio of a change in differential resistance of the semiconductor element to a temperature in a temperature range from 30° C. to 40° C. is equal to or higher than 5 Ω/° C. and equal to or lower than 100 Ω/° C.

### Claim 31 (depends on 27)

The semiconductor element of claim 27 wherein:
in a case where a temperature of an object under measurement is 25° C., an absolute value of a ratio of a change in differential resistance of the semiconductor element to a temperature in a temperature range from 30° C. to 40° C. is equal to or higher than 5 Ω/° C. and equal to or lower than 100 Ω/° C.