# US 2024/0319434 A1 · Optical fiber with wide bandwidth and high gains in o+e band and regulation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0319434 A1
- Document ID: US20240319434A1
- Status: Published application
- Kind: A1
- Application number: 18/439,137
- Filed: 2024-02-12
- Published: 2024-09-26
- Earliest claimed: 2023-03-23
- Assignees: Shanghai University
- Applicants: Shanghai University
- Inventors: Tingyun WANG; Jianxiang WEN; Yanhua DONG; Xiaobei ZHANG; Yi HUANG; Weiqi WANG
- Web page: https://patentgrep.com/patent/US20240319434A1

## CPC

- G02B 6/02042: {Multicore optical fibres}
- G02B 6/02223: {Dual window fibres, i.e. characterised by dispersion properties around 1550 nm and in at least another wavelength window, e.g. 1310 nm}
- G02B 6/02342: {characterised by cladding features, i.e. light confining region}
- G02B 6/028: with core or cladding having graded refractive index {(G02B6/02033, G02B6/02295 take precedence)}
- G02B 6/03688: {having 5 or more layers}
- Y02P 40/57: Improving the yield, e-g- reduction of reject rates
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

An optical fiber with wide bandwidth and high gain in an O+E band and a regulation method thereof are disclosed. The optical fiber includes a core and a cladding (0). The core includes a first loose layer (1), a first core layer (2), a second loose layer (3), a second core layer (4) and an inner core (5) from outside to inside. The first loose layer (1) and the second loose layer (3) are made of a silica material doped with high-refractive-index GeO2 and P2O5. In the first core layer (2) and the second core layer (4), Al2O3, bismuth oxide and PbO are sequentially doped. The gain performance of the optical fiber is controlled by adjusting doping molar ratios of Al2O3, bismuth oxide and PbO. The co-doped silica optical fiber maintains fiber gains exceeding 15 dB in a wavelength range of 1260 to 1460 nm.

## Claims

### Claim 1

An optical fiber with wide bandwidth and high gains in an O+E band, comprising a core and a cladding (0), wherein the core comprises a first loose layer (1), a first core layer (2), a second loose layer (3), a second core layer (4), and an inner core (5) from outside to inside; the first loose layer (1) and the second loose layer (3) are made of a silica material doped with high-refractive-index GeO2 and P2O5, and in the first core layer (2) and the second core layer (4), Al2O3, bismuth oxide and PbO are sequentially doped.

### Claim 2 (depends on 1)

The optical fiber with wide bandwidth and high gains in an O+E band according to claim 1, wherein in the first core layer (2) and the second core layer (4), a molar ratio of Al2O3 to bismuth oxide is varied from 0.5 to 20 and a molar ratio of bismuth oxide to PbO is varied from 0.2 to 30.

### Claim 3 (depends on 2)

The optical fiber with wide bandwidth and high gains in an O+E band according to claim 2, wherein in the first core layer (2) and the second core layer (4), the molar ratio of Al2O3 to bismuth oxide is varied from 1 to 3, and the molar ratio of bismuth oxide to PbO is varied from 1.2 to 2.

### Claim 4 (depends on 2)

The optical fiber with wide bandwidth and high gains in an O+E band according to claim 2, wherein the cladding (0) of the optical fiber has a diameter of 120 to 130 μm, the core has a diameter of 8 to 12 μm, and a refractive index difference between the cladding (0) and the core is 0.005 to 0.0012.

### Claim 5

A method for regulating fiber bandwidth and gain in an O+E band, comprising: depositing a SiO2 material doped with GeO2 and P2O5 on an inner wall of a substrate tube to form a first loose layer (1); sequentially depositing Al2O3, bismuth oxide, and PbO on the first loose layer (1); then depositing the SiO2 material doped with GeO2 and P2O5 again to form a second loose layer; sequentially depositing Al2O3, bismuth oxide, and PbO on the second loose layer; and finally, depositing a silica material doped with GeO2 and P2O5 and performing preform collapsing and fiber drawing to form an optical fiber, wherein gain performance of the optical fiber is regulated by controlling doping molar ratios of Al2O3, bismuth oxide and PbO.

### Claim 6 (depends on 5)

The method for regulating fiber bandwidth and gain in an O+E band according to claim 5, wherein a molar ratio of Al2O3 to bismuth oxide is 0.5 to 20 and a molar ratio of bismuth oxide to PbO is 0.2 to 30.

### Claim 7 (depends on 5)

The method for regulating fiber bandwidth and gain in an O+E band according to claim 5, wherein when an atomic layer deposition (ALD) technology is used to sequentially deposit Al2O3, bismuth oxide and PbO, an O-source precursor material is ozone or deionized water, an Al-source precursor is trimethylaluminum, a Bi-source precursor is tris(2,2,6,6-tetramethyl-3,5-heptanedionato) bismuth (Bi(tmhd)3) and a Pb-source precursor is bis(2,2,6,6-tetramethyl-3,5-heptanedionato) lead (Pb(tmhd)2).

### Claim 8 (depends on 7)

The method for regulating fiber bandwidth and gain in an O+E band according to claim 7, wherein a Bi-source heating temperature is controlled at 200 to 300° C. with a pulse time of 200 to 400 ms; a Pb-source heating temperature is controlled at 100 to 200° C. with a pulse time of 200 to 400 ms; an O-source pulse time is 200 to 1000 ms; an Al-source pulse time is 50 to 300 ms; an entire reaction chamber maintains a uniform temperature, with a reaction temperature of 200 to 400° C. and a gas flow rate controlled at 50 to 800 sccm.

### Claim 9 (depends on 5)

The method for regulating fiber bandwidth and gain in an O+E band according to claim 5, comprising the following specific steps:
1) depositing a SiO2 loose layer, which is doped with GeO2 and P2O5 for increasing an refractive index, on an inner wall of a quartz tube by using a modified chemical vapor deposition (MCVD) technology, controlling a temperature to semi-vitrify the layer and creating an ALD deposition environment to form the first loose layer (1);
2) sequentially depositing doping materials based on a sequence of Al2O3, bismuth oxide and PbO by using the ALD technology to form a first core layer (2);
3) depositing a SiO2 material doped with GeO2 and P2O5 by using the MCVD technology and semi-vitrifying the SiO2 material to form a second loose layer (3);
4) placing the substrate tube in a direction reverse to that in step 2) and performing deposition by using the ALD technology: depositing Al2O3, bismuth oxide, and PbO materials again on the second loose layer based on the deposition sequence and doping molar ratios in step 2), to form a second core layer (4);
5) by using the MCVD technology, depositing a SiO2 material doped with GeO2 and P2O5 for increasing the refractive index, semi-vitrifying the deposited material to form an inner core (5), finally, performing high-temperature preform collapsing and drawing a fiber preform into an optical fiber by using a drawing tower.

### Claim 10 (depends on 6)

The method for regulating fiber bandwidth and gain in an O+E band according to claim 6, comprising the following specific steps:
1) depositing a SiO2 loose layer, which is doped with GeO2 and P2O5 for increasing an refractive index, on an inner wall of a quartz tube by using a modified chemical vapor deposition (MCVD) technology, controlling a temperature to semi-vitrify the layer and creating an ALD deposition environment to form the first loose layer (1);
2) sequentially depositing doping materials based on a sequence of Al2O3, bismuth oxide and PbO by using the ALD technology to form a first core layer (2);
3) depositing a SiO2 material doped with GeO2 and P2O5 by using the MCVD technology and semi-vitrifying the SiO2 material to form a second loose layer (3);
4) placing the substrate tube in a direction reverse to that in step 2) and performing deposition by using the ALD technology: depositing Al2O3, bismuth oxide, and PbO materials again on the second loose layer based on the deposition sequence and doping molar ratios in step 2), to form a second core layer (4);
5) by using the MCVD technology, depositing a SiO2 material doped with GeO2 and P2O5 for increasing the refractive index, semi-vitrifying the deposited material to form an inner core (5), finally, performing high-temperature preform collapsing and drawing a fiber preform into an optical fiber by using a drawing tower.

### Claim 11 (depends on 7)

The method for regulating fiber bandwidth and gain in an O+E band according to claim 7, comprising the following specific steps:
1) depositing a SiO2 loose layer, which is doped with GeO2 and P2O5 for increasing an refractive index, on an inner wall of a quartz tube by using a modified chemical vapor deposition (MCVD) technology, controlling a temperature to semi-vitrify the layer and creating an ALD deposition environment to form the first loose layer (1);
2) sequentially depositing doping materials based on a sequence of Al2O3, bismuth oxide and PbO by using the ALD technology to form a first core layer (2);
3) depositing a SiO2 material doped with GeO2 and P2O5 by using the MCVD technology and semi-vitrifying the SiO2 material to form a second loose layer (3);
4) placing the substrate tube in a direction reverse to that in step 2) and performing deposition by using the ALD technology: depositing Al2O3, bismuth oxide, and PbO materials again on the second loose layer based on the deposition sequence and doping molar ratios in step 2), to form a second core layer (4);
5) by using the MCVD technology, depositing a SiO2 material doped with GeO2 and P2O5 for increasing the refractive index, semi-vitrifying the deposited material to form an inner core (5), finally, performing high-temperature preform collapsing and drawing a fiber preform into an optical fiber by using a drawing tower.

### Claim 12 (depends on 8)

The method for regulating fiber bandwidth and gain in an O+E band according to claim 8, comprising the following specific steps:
1) depositing a SiO2 loose layer, which is doped with GeO2 and P2O5 for increasing an refractive index, on an inner wall of a quartz tube by using a modified chemical vapor deposition (MCVD) technology, controlling a temperature to semi-vitrify the layer and creating an ALD deposition environment to form the first loose layer (1);
2) sequentially depositing doping materials based on a sequence of Al2O3, bismuth oxide and PbO by using the ALD technology to form a first core layer (2);
3) depositing a SiO2 material doped with GeO2 and P2O5 by using the MCVD technology and semi-vitrifying the SiO2 material to form a second loose layer (3);
4) placing the substrate tube in a direction reverse to that in step 2) and performing deposition by using the ALD technology: depositing Al2O3, bismuth oxide, and PbO materials again on the second loose layer based on the deposition sequence and doping molar ratios in step 2), to form a second core layer (4);
5) by using the MCVD technology, depositing a SiO2 material doped with GeO2 and P2O5 for increasing the refractive index, semi-vitrifying the deposited material to form an inner core (5), finally, performing high-temperature preform collapsing and drawing a fiber preform into an optical fiber by using a drawing tower.