# US 2024/0318722 A1 · Rubber sealing gasket with excellent compression performance and low-temperature performance, and preparation method and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0318722 A1
- Document ID: US20240318722A1
- Status: Published application
- Kind: A1
- Application number: 18/613,029
- Filed: 2024-03-21
- Published: 2024-09-26
- Earliest claimed: 2023-03-22
- Assignees: Xuzhou College of Industrial Technology
- Applicants: Xuzhou College of Industrial Technology
- Inventors: Yunhui XU; Shuangyuan XU; Tongyu ZHANG; Yating XU; Jiayao LI; Zefeng SHAO; Zaixue WANG; Yanan ZANG; Houluo CONG; Dazhi ZHANG; Peipei LI; Lianxiang ZHOU
- Web page: https://patentgrep.com/patent/US20240318722A1

## CPC

- F16J 15/022: {characterised by structure or material}
- C08L 15/005: {Hydrogenated nitrile rubber}
- C08L 2666/02: Organic macromolecular compounds, natural resins, waxes or and bituminous materials
- C08L 2666/55: Carbon
- C08L 2666/68: Plasticizers; Solvents
- C08L 2666/72: Fillers; Inorganic pigments; Reinforcing additives
- F16J: PISTONS {(specially adapted for dampers F16F9/32)}; CYLINDERS; SEALINGS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)

## Abstract

The present disclosure belongs to the technical field of polymer rubber composites, and specifically relates to a rubber sealing gasket with excellent compression performance and low-temperature performance, and a preparation method and use thereof. The rubber sealing gasket is prepared from the following raw materials in parts by mass: a hydrogenated nitrile butadiene rubber (HNBR): 100 parts; a processing aid: 12.3 parts to 13.7 parts; a reinforcing filler: 45 parts to 65 parts; a vulcanizing agent: 4.8 parts to 5.2 parts; and a co-crosslinking agent: 4.8 parts to 5.2 parts. The rubber sealing gasket prepared by the present disclosure has excellent compression performance and low-temperature performance, meets the performance requirements of rubber sealing gaskets for automobile air-conditioning systems, and can be used in sealing components of automobile air-conditioning systems.

## Claims

### Claim 1

A rubber sealing gasket with excellent compression performance and low-temperature performance, characterized in that the rubber sealing gasket is prepared from the following raw materials in parts by mass:
hydrogenated nitrile butadiene rubber
100 parts;
processing aid
12.3 parts to 13.7 parts;
reinforcing filler
45 parts to 65 parts;
vulcanizing agent
4.8 parts to 5.2 parts; and
co-crosslinking agent
4.8 parts to 5.2 parts.

### Claim 2 (depends on 1)

The rubber sealing gasket with excellent compression performance and low-temperature performance according to claim 1, characterized in that the hydrogenated nitrile butadiene rubber is hydrogenated nitrile butadiene rubber 2020L with an acrylonitrile content of 36% to 38%, a Mooney viscosity of 50 to 65, a specific gravity of 0.94 g/cm3 to 0.96 g/cm3, a hydrogenation rate of 90% to 91%, and an iodine index of 27 to 28.

### Claim 3 (depends on 2)

The rubber sealing gasket with excellent compression performance and low-temperature performance according to claim 2, characterized in that the processing aid is a mixture of an activating agent, an anti-aging agent, and a plasticizing agent, wherein the activating agent comprises zinc oxide and stearic acid, the anti-aging agent comprises anti-aging agents MB and RD, and the plasticizing agent is TP-95.

### Claim 4 (depends on 3)

The rubber sealing gasket with excellent compression performance and low-temperature performance according to claim 3, characterized in that the reinforcing filler is a mixture of carbon black N220 and carbon black N990.

### Claim 5 (depends on 4)

The rubber sealing gasket with excellent compression performance and low-temperature performance according to claim 4, characterized in that the vulcanizing agent is dicumyl peroxide (DCP), and the co-crosslinking agent is triallyl isocyanurate (TAIC).

### Claim 6 (depends on 5)

The rubber sealing gasket with excellent compression performance and low-temperature performance according to claim 5, characterized in that based on 100 parts by mass of the hydrogenated nitrile butadiene rubber, the stearic acid is used in 0.9 parts to 1.1 parts, the zinc oxide is used in 4.8 parts to 5.2 parts, the anti-aging agent MB is used in 0.9 parts to 1.1 parts, the anti-aging agent RD is used in 0.9 parts to 1.1 parts, the plasticizing agent TP-95 is used in 4.8 parts to 5.2 parts, the carbon black N220 is used in 20 parts to 30 parts, the carbon black N990 is used in 25 parts to 35 parts, the dicumyl peroxide is used in 4.8 parts to 5.2 parts, and the triallyl isocyanurate is used in 4.8 parts to 5.2 parts.

### Claim 7 (depends on 1)

A preparation method of the rubber sealing gasket with excellent compression performance and low-temperature performance according to claim 1, characterized by comprising the following steps:
S1. subjecting the hydrogenated nitrile butadiene rubber, the processing aid, and the reinforcing filler to first internal mixing to obtain a masterbatch;
S2. subjecting the masterbatch obtained in the S1 to second internal mixing with the vulcanizing agent and the co-crosslinking agent to obtain a hydrogenated nitrile butadiene rubber mixture; and
S3. vulcanizing the hydrogenated nitrile butadiene rubber mixture obtained in the S2 twice to obtain the rubber sealing gasket with excellent compression performance and low-temperature performance.

### Claim 8 (depends on 7)

The preparation method of the rubber sealing gasket with excellent compression performance and low-temperature performance according to claim 7, characterized in that in the S3, the vulcanizing is conducted twice as follows: conducting a first vulcanization for 12 min to 22 min at a first temperature of 170° C. to 175° C. and a pressure of 10 MPa to 20 MPa; and conducting a second vulcanization for 3 h to 5 h at a second temperature of 150° C. to 155° C.

### Claim 9 (depends on 8)

The preparation method of the rubber sealing gasket with excellent compression performance and low-temperature performance according to claim 8, characterized in that the first vulcanization is conducted by a plate vulcanizing machine or an injection vulcanizing machine, and the second vulcanization is conducted by an atmospheric pressure layered vulcanization process, an atmospheric pressure hot-air vulcanization process, or an atmospheric pressure salt-bath hot vulcanization process.

### Claim 10 (depends on 1)

A use of the rubber sealing gasket with excellent compression performance and low-temperature performance according to claim 1 in a sealing component of an automobile air-conditioning system.