# US 2024/0316859 A1 · Method of additive manufacture of porous gas-permeable shaped bodies having controllable porosity

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0316859 A1
- Document ID: US20240316859A1
- Status: Published application
- Kind: A1
- Application number: 18/575,585
- Filed: 2022-06-30
- Published: 2024-09-26
- Earliest claimed: 2021-06-30
- Assignees: Rheinisch-Westfälische Technische Hochschule (RWTH) Aachen
- Applicants: Rheinisch-WestfäLische Technische Hochschule (Rwth) Aachen
- Inventors: Patrick BONGARTZ; Moritz MEYER; Matthias WESSLING; Alexander SCHEELE
- Web page: https://patentgrep.com/patent/US20240316859A1

## CPC

- B29C 64/153: using layers of powder being selectively joined, e.g. by selective laser sintering or melting
- B01F 27/053: characterised by their materials
- B29C 64/268: using laser beams; using electron beams [EB]
- B33Y 30/00: Apparatus for additive manufacturing; Details thereof or accessories therefor
- B33Y 40/10: Pre-treatment
- B01F 27/0725: {on the free end of the rotating axis}
- B01F 27/1125: with vanes or blades extending parallel or oblique to the stirrer axis
- B01F 27/1145: ribbon shaped with an open space between the helical ribbon flight and the rotating axis
- B01F 27/1191: {with a bent rod of non-helical configuration supported at one end}
- B29K 2077/00: Use of {PA, i.e.} polyamides, e.g. polyesteramides {or derivatives thereof}, as moulding material
- B33Y 10/00: Processes of additive manufacturing
- B33Y 70/00: Materials specially adapted for additive manufacturing
- B33Y 80/00: Products made by additive manufacturing
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B01F: MIXING, e.g. DISSOLVING, EMULSIFYING OR DISPERSING (mixing paints B44D3/06)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A process for the additive manufacturing of porous gas-permeable shaped articles by selective laser sintering of a polymer powder may include a) Providing a layer of polymer powder within an construction space; b) Heating a polymer layer to a temperature greater than or equal to 0.5° C. and less than or equal to 2.5° C. below the melting point of the polymer powder; c) Spatially resolved melting of a powder bed by means of the introduction of laser energy; wherein steps a-c) are carried out one or more times in the same construction space on consecutively superimposed powder layers and the surface energy contribution to be introduced in process step c) is greater than or equal to 1.7 times and less than or equal to 4.25 times the product of the melting enthalpy, polymer powder filling density and layer thickness of the powder filling.

## Claims

### Claim 1

A process for the additive manufacturing of porous gas-permeable shaped articles by selective laser sintering of a polymer powder comprising the steps of:
a) Providing a layer of polymer powder within a construction space;
b) Heating the polymer powder bed to a temperature greater than or equal to 0.5° C. and less than or equal to 2.5° C. below the melting point of the polymer powder;
c) Spatially resolved melting of a powder layer by means of laser energy;
wherein steps a-c) are carried out one or more times in the same construction space on consecutively superimposed powder layers;
characterized in that the surface energy contribution to be introduced in process step c) is greater than or equal to 1.7 times and less than or equal to 4.25 times the product of the melting enthalpy, polymer powder bulk density and layer thickness of the powder bed.

### Claim 2 (depends on 1)

The process according to claim 1, wherein the heating of the polymer powder bed is carried out to a temperature of greater than or equal to 0.1° C. and less than or equal to 0.5° C. below the melting point of the polymer powder.

### Claim 3 (depends on 1)

The process according to claim 1, wherein the laser energy introduced in process step c) is greater than or equal to 2.5 times and less than or equal to 3.5 times the product of the melting enthalpy, the polymer powder bulk density and the layer thickness of the powder bulk.

### Claim 4 (depends on 1)

The process according to claim 1, wherein the layer thickness of the powder layer applied in method step a) is greater than or equal to 0.075 mm and less than or equal to 0.25 mm.

### Claim 5 (depends on 1)

The process according to claim 1, wherein the total layer thickness of the sintered porous gas-permeable shaped article is greater than or equal to 2.5 times and less than or equal to 25 times the powder layer thickness provided in method step a), respectively.

### Claim 6 (depends on 1)

The process according to claim 1, wherein the polymer powder used comprises greater than or equal to 80% by weight and less than or equal to 100% by weight polyamide 12 (PA12).

### Claim 7 (depends on 6)

The process according to claim 6, wherein the powder consists of a proportion of greater than or equal to 15 wt.-% and less than or equal to 100 wt.-% of new powder not yet used in a laser sintering process.

### Claim 8 (depends on 1)

The use of a process according to claim 1 for manufacturing devices selected from the group consisting of filters, gassing and/or stirring devices or combinations of at least two devices from this group.

### Claim 9 (depends on 8)

The use according to claim 8, wherein the device is a gassing and stirring device, wherein the geometry of the gassing and stirring device is selected from the group consisting of spiral stirrer, inclined blade stirrer, paddle stirrer, disk stirrer, toothed disk stirrer, anchor stirrer, Rushton turbine or a combination of at least two geometries from this group.

### Claim 10

A porous shaped body produced by selective laser sintering (SLS) for gas flushing or filtration of a process liquid, characterized in that the shaped body consists of greater than or equal to 75% by weight and less than or equal to 100% by weight of polyamide 12 and has an open porosity of greater than or equal to 14% by volume and less than or equal to 16% by volume.

### Claim 11 (depends on 10)

The shaped body according to claim 10, wherein the shaped body comprises polyamide 12 in a weight proportion of greater than or equal to 90 wt.-% and less than or equal to 100 wt.-%.

### Claim 12 (depends on 10)

The shaped body according to claim 10, wherein the shaped body has an oxygen flow rate at a pressure difference of 500 mbar of greater than or equal to 2.0 L/min and less than or equal to 7.5 L/min.

### Claim 13 (depends on 10)

The shaped body according to claim 10, wherein the shaped body comprises pores of a size of greater than or equal to 6.0 μm and less than or equal to 8.3 μm determined by capillary flow porometry.