# US 2024/0316834 A1 · Method for Manufacturing Moulded Parts

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0316834 A1
- Document ID: US20240316834A1
- Status: Published application
- Kind: A1
- Application number: 18/278,092
- Filed: 2022-02-22
- Published: 2024-09-26
- Earliest claimed: 2021-02-22
- Assignees: Siempelkamp Maschinen- und Anlagenbau GmbH & Co. KG
- Applicants: Siempelkamp Maschinen- Und Anlagenbau GmbH
- Inventors: Fabian Köffers; Michael Schöler
- Web page: https://patentgrep.com/patent/US20240316834A1

## CPC

- B29C 43/3607: {with sealing means or the like}
- B29C 33/0038: {with sealing means or the like (seals on envelopes used in tyre retreading B29D30/542; for injection moulding footwear B29D35/0045)}
- B29C 33/3828: {Moulds made of at least two different materials having different thermal conductivities}
- B29C 43/10: Isostatic pressing, i.e. using non-rigid pressure-exerting members against rigid parts or dies
- B29C 43/12: using bags surrounding the moulding material {or using membranes contacting the moulding material}
- B29C 43/361: {with pressing members independently movable of the parts for opening or closing the mould, e.g. movable pistons (transfer moulding B29C45/02; injection-compression moulding B29C45/561)}
- B29C 70/44: using isostatic pressure, e.g. pressure difference-moulding, vacuum bag-moulding, autoclave-moulding or expanding rubber-moulding
- B29C 43/52: Heating or cooling
- B29C 2043/3238: {pressurized liquid acting directly or indirectly on the material to be formed}
- B29K 2105/08: of continuous length, e.g. cords, rovings, mats, fabrics, strands or yarns
- B29C: SHAPING OR JOINING OF PLASTICS; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDED FOR; AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING (making preforms B29B11/00; making laminated products by combining previously unconnected layers which become one product whose layers will remain together B32B37/00 - B32B41/00)
- B29K: INDEXING SCHEME ASSOCIATED WITH SUBCLASSES B29B, B29C OR B29D, RELATING TO MOULDING MATERIALS OR TO MATERIALS FOR {MOULDS, } REINFORCEMENTS, FILLERS OR PREFORMED PARTS, e.g. INSERTS

## Abstract

A method for production of molded parts, in particular parts consisting of a fiber composite material, is illustrated and described. In order to reduce the load on the membrane, the membrane according to the invention can be slipped past the seal and the membrane can at least in part be slipped past the seal as a result of the expansion force.

## Claims

### Claim 1

A method for manufacturing moulded parts, in particular from fibre composite material, comprising the following steps:
a) providing a device comprising:
a first pressing tool,
a second pressing tool,
at least one membrane, and
at least one seal,
wherein the first pressing tool and the second pressing tool can be moved relative to one another between an open position and a closed position,
wherein a working space for a workpiece is formed between the first pressing tool and the second pressing tool,
wherein the membrane is arranged at least in sections between the first pressing tool and the second pressing tool,
wherein the membrane is arranged at least in sections in the working space,
wherein at least one cavity for a working medium is formed between the membrane and the first pressing tool and/or the second pressing tool at least in the closed position,
wherein the cavity can be sealed by the seal least in sections at least in the closed position,
wherein, in order to seal the cavity, a sealing force (FD) can be applied to the membrane by means of the seal, and
wherein the membrane and the first pressing tool and/or the second pressing tool have different thermal expansion coefficients,
b) applying a sealing force (FD) by means of the seal to the membrane,
wherein the cavity is sealed at least in sections by applying the sealing force (FD) to the membrane, and
wherein a frictional force; (FR) is applied between the membrane and the seal by the sealing force (FD),
c) applying pressure and/or temperature to the membrane, preferably by means of a working medium in the cavity,
wherein the membrane extends at least in sections at least in the working space, preferably more strongly than the first pressing tool and/or the second pressing tool,
wherein pressure is applied to the membrane, preferably by means of the working medium in the cavity,
wherein the pressure counteracts an expansion of the membrane into the cavity and thereby effects an expansion force (FA) along the membrane surface, and
wherein the expansion force (FA) counteracts the frictional force (FR) between the membrane and the seal at least adjoining the seal,
wherein
the membrane can be passed by the seal and in that in step c), the membrane is passed by the seal at least in sections due to the expansion force (FA).

### Claim 2 (depends on 1)

The method for manufacturing moulded parts according to claim 1, wherein step b) and step c) overlap at least in time.

### Claim 3 (depends on 1)

The method for manufacturing moulded parts according to claim 1, wherein the expansion force (FA) is greater than the frictional force (FR) between the membrane and the seal.

### Claim 4 (depends on 1)

The method for manufacturing moulded parts according to claim 1, comprising the following steps, which take place after step a) and preferably before step b) and/or before step c):
a1) providing at least one workpiece,
a2) inserting the workpiece into the device, in particular into the working space, and
a3) moving the first pressing tool and/or the second pressing tool into the closed position.

### Claim 5 (depends on 1)

The method for manufacturing moulded parts according to claim 1, wherein the device provided in step a) comprises at least one device for changing the pretension of the membrane.

### Claim 6 (depends on 5)

The method for manufacturing moulded parts according to claim 5, comprising the following step, which takes place after step a) and, preferably, before step b) and/or before step c):
a4) pretensioning the membrane by means of the device for changing the pretension.

### Claim 7 (depends on 6)

The method for manufacturing moulded parts according to claim 6, wherein a pretension force (FV) is applied to the membrane through the pretensioning of the membrane according to step a4) and, preferably in that the pretension force (FV), in particular during step b) and/or during step c), is smaller than the frictional force (FR) between the membrane and the seal.

### Claim 8 (depends on 7)

The method for manufacturing moulded parts according to claim 7, wherein during step b) and/or during step c), the pretension force (FV) applied to the membrane is changed, in particular reduced, by the device for changing the pretension.

### Claim 9 (depends on 7)

The method for manufacturing moulded parts according to claim 7, wherein the sum of expansion force (FA) and pretension force (FV), in particular during step b) and/or during step c), is greater than the frictional force (FR) between the membrane and the seal.

### Claim 10 (depends on 1)

The method for manufacturing moulded parts according to claim 1, wherein during step b) and/or during step c), the pressure and/or the temperature of the working medium in the cavity are changed.

### Claim 11 (depends on 1)

The method for manufacturing moulded parts according to claim 1, wherein the device provided in step a) comprises at least one device for changing the sealing force, preferably adjoining the seal.

### Claim 12 (depends on 1)

The method for manufacturing moulded parts according to claim 1, wherein the device provided in step a) comprises at least one second membrane,
wherein at least one second cavity for a working medium is formed between the at least second membrane and the first pressing tool and/or the second pressing tool at least in the closed position,
wherein, in order to seal the second cavity, a sealing force can be applied to the second membrane by means of at least one second seal, and
wherein the second membrane can be passed by the second seal.

### Claim 13 (depends on 1)

The method for manufacturing moulded parts according to claim 1, wherein in step b) and/or in step c), the pressure of the working medium located in the cavity is raised at least to 1.2 bar, in particular to 2 bar, and preferably in that in step b) and/or in step c), the pressure of the working medium located in the cavity is raised up to a maximum pressure in the range of between 10 bar and 50 bar, in particular of between 15 bar and 30 bar.

### Claim 14 (depends on 1)

The method for manufacturing moulded parts according to claim 1, wherein in step b) and/or in step c), the temperature of the working medium located in the cavity is raised to a maximum temperature in the range of between 280° C. and 500° C., in particular of between 310° C. and 410° C.

### Claim 15 (depends on 1)

The method for manufacturing moulded parts according to claim 1, comprising the following step, which takes place after step b) and/or after step c):
c) opening the device and removing the workpiece.