# US 2024/0313520 A1 · JOINT OF MgB2 SUPERCONDUCTING WIRES

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0313520 A1
- Document ID: US20240313520A1
- Status: Published application
- Kind: A1
- Application number: 18/576,526
- Filed: 2022-07-04
- Published: 2024-09-19
- Earliest claimed: 2021-07-06
- Assignees: NV Bekaert SA; Epoch Wires Limited
- Applicants: NV Bekaert SA; Epoch Wires Limited
- Inventors: Serdar ATAMERT; Mehmet KUTUKCU; Chris D'HULST; Jan MESTDAGH
- Web page: https://patentgrep.com/patent/US20240313520A1

## CPC

- H02G 15/18: protected by sleeves, e.g. for communication cable (two-part covers H02G15/10 {; preforms having internal stresses B29C61/00})
- H01R 4/68: Connections to or between superconductive connectors
- H02G 1/14: for joining or terminating cables
- H10N 60/0856: {of devices comprising metal borides, e.g. MgB2}
- H10N 60/80: Constructional details
- Y02E 40/60: Superconducting electric elements or equipment; Power systems integrating superconducting elements or equipment
- H02G: INSTALLATION OF ELECTRIC CABLES OR LINES, OR OF COMBINED OPTICAL AND ELECTRIC CABLES OR LINES
- H01R: ELECTRICALLY-CONDUCTIVE CONNECTIONS; STRUCTURAL ASSOCIATIONS OF A PLURALITY OF MUTUALLY-INSULATED ELECTRICAL CONNECTING ELEMENTS; COUPLING DEVICES; CURRENT COLLECTORS
- H10N: ELECTRIC SOLID-STATE DEVICES NOT OTHERWISE PROVIDED FOR
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A joint of superconducting wires having at least two superconducting wires, each with a sheath and with a core of reacted superconducting MgB2. At least one first superconducting wire has a first flattened end and at least one second superconducting wire has a second flattened end. The joint further has a tubular metal connector having a centre filled with MgB2 material. The first flattened end of the first superconducting wire is inserted at one side of the connector until it is in contact with the MgB2 material, the second flattened end of the second superconducting wire is inserted at the other side of the connector until it is in contact with the MgB2 material, the connector is pressed at both sides to fix the superconducting wires, and the centre of the connector is pressed to compact the MgB2 material.

## Claims

### Claim 1

A joint of superconducting wires,
said joint comprising at least two superconducting wires each with a sheath and with a core of reacted superconducting MgB2,
at least one first superconducting wire having a first flattened end and at least one second superconducting wire having a second flattened end,
said joint further comprising a tubular metal connector,
said connector having a centre being filled with magnesium or boron or MgB2 material,
said first flattened end of said at least one first superconducting wire being inserted at one side of said connector until it is in contact with said magnesium or boron or MgB2 material,
said second flattened end of said at least one second superconducting wire being inserted at the other side of said connector until it is in contact with said magnesium or boron or MgB2 material,
said connector being pressed at both sides to fix said at least one first superconducting wire and said at least one second superconducting wire,
said centre of said connector being pressed to compact said magnesium or boron or MgB2 material.

### Claim 2 (depends on 1)

The joint according to claim 1,
wherein said first flattened end and said second flattened end have a width to thickness ratio ranging from 1.1 to 10, preferably from 1.1 to 5.0.

### Claim 3 (depends on 1)

The joint according to claim 1,
wherein said tubular metal connector comprises low carbon steel.

### Claim 4 (depends on 1)

The joint according to claim 1,
wherein said tubular metal connector comprises titanium.

### Claim 5

(canceled)

### Claim 6

A method of joining at least two superconducting wires having a superconducting core of reacted MgB2, said method comprising the following steps:
a. providing at least one first superconducting wire and at least one second superconducting wire,
said at least one first superconducting wire having a first end and
said at least one second superconducting wire having a second end;
b. flattening said first end of said first superconducting wire and flattening said second end of said second superconducting wire;
c. providing a tubular metal connector having a length Ltot and having a centre;
d. filling said centre of said connector with unreacted Mg powder and B powder;
e. flattening said connector in case said connector has an original circular cross-section;
f. inserting said first end of said least one first superconductor at one side in said connector over a length L1 until contact with said Mg powder and B powder;
g. inserting said second end of said at least one second superconductor at the other side in said connector over a length L2 until contact with said Mg powder and B powder;
h. pressing said connector at both sides to fix said at least one first superconductor wire and said at least one second superconductor wire in said connector;
i. pressing said centre of said connector over a length Lcenter to compact said Mg and B powder, wherein said lengths Ltot, L1, L2 and Lcenter matching following equation:
Ltot
=
L
⁢
1
+
L
⁢
2
+
2
×
Lcr
+
Lcenter
where Lcr is a critical distance between, on the one hand, the first flattened end and the second flattened end, and, on the other hand, the pressed length Lcenter of the centre of said connector needed to avoid that the superconducting wires are pressed together with the pressing of said centre.

### Claim 7 (depends on 6)

The method according to claim 6,
wherein said method comprises the following step:
subjecting said connector and said first flattened end and second flattened end to a heat treatment to create superconductivity in the centre and to restore superconductivity in said first flattened end and second flattened end.

### Claim 8 (depends on 7)

The method according to claim 7,
wherein said heat treatment comprises a first phase of heating in a range of 800° C. to 1000° C. during 20 minutes to 40 minutes and a second phase of heating in a range of 550° C. to 750° C. during 45 minutes to 75 minutes.

### Claim 9 (depends on 6)

The method according to claim 6,
wherein flattening said first end of said at least one first superconducting wire and flattening said second end of said at least one second superconducting wire are done to a degree where the width to thickness ratio of said first end and of said second end range from 1.25 to 2.5, preferably from 1.50 to 2.0.

### Claim 10 (depends on 6)

The method according to claim 6,
wherein said critical distance Lcr ranges from 0.6 mm to 5.0 mm.

### Claim 11 (depends on 1)

The joint according to claim 1,
wherein said tubular metal connector comprises low carbon steel, and
wherein said tubular metal connector comprises titanium.

### Claim 12 (depends on 11)

The joint according to claim 11,
wherein said tubular metal connector has a titanium barrier inside and a low carbon steel around said titanium barrier.