# US 2024/0309210 A1 · Method and device for producing products by using lignocellulose-containing particles

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0309210 A1
- Document ID: US20240309210A1
- Status: Published application
- Kind: A1
- Application number: 18/670,534
- Filed: 2024-05-21
- Published: 2024-09-19
- Earliest claimed: 2018-09-18
- Assignees: Polymertrend LLC.
- Applicants: Polymertrend LLC.
- Inventors: Max ZAHER; Wolfgang SCHWARZ; Volker THOLE
- Web page: https://patentgrep.com/patent/US20240309210A1

## CPC

- B27N 1/00: Pretreatment of moulding material
- C08L 97/02: Lignocellulosic material, e.g. wood, straw or bagasse {(manufacture of articles made from lignocellulosic material by dry processes B27N)}
- B27K 5/0035: {Electron beam-radiation}
- B27N 1/02: Mixing the material with binding agent (mixing in general B01F)
- B27N 3/02: from particles
- B27K 2200/10: Articles made of particles or fibres consisting of wood or other lignocellulosic material
- B27K 2200/15: Pretreated particles or fibres
- C08L 2205/03: containing three or more polymers in a blend
- C08L 2205/14: containing polymeric additives characterised by shape
- B27N: MANUFACTURE BY DRY PROCESSES OF ARTICLES, WITH OR WITHOUT ORGANIC BINDING AGENTS, MADE FROM PARTICLES OR FIBRES CONSISTING OF WOOD OR OTHER LIGNOCELLULOSIC OR LIKE ORGANIC MATERIAL (containing cementitious material B28B; shaping of substances in a plastic state B29C; fibreboards made from fibrous suspensions D21J; drying F26B17/00)
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- B27K: PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR (applying liquids or other fluent materials to surfaces in general B05; coating wood or similar material B44D); CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS

## Abstract

The invention relates to a method and devices for producing products (65) by using cellulose-containing particles, with which the following steps are carried out: a) irradiating the particles with electrons in the energy range >1 MeV: b) mixing the irradiated particles with electron-beam-reactive powder of a synthetic polymer, in particular a thermoplastic, having powder particle sizes <2000 micrometres and/or with a liquid electron-beam-reactive synthetic or bio-based polymer; c) forming the mixture created in a way corresponding to the form of the product to be produced, in particular forming it into a nonwoven (56): d) heating the formed mixture to 100-180° C.; e) pressing the formed mixture without heating; and f) irradiating the pressed mixture with electrons in the energy range of 1 MeV to 10 Me V and also with appropriately chosen dosages and dosing rates.

## Claims

### Claim 1

Method for producing a formed part containing lignocellulose, the method having the following steps:
a) irradiation of lignocellulose-containing particles in the energy range between 1 MeV and 10 MeV, preferably >3 MeV<8 MeV;
b) mixing the irradiated lignocellulose-containing particles with an electron-beam-reactive polymer in powder form, in particular a thermoplastic, with powder particle sizes <2000 micrometres (μm), and/or with a liquid containing electron-beam-reactive polymer;
c) forming of the mixture produced in a way corresponding to the form of the formed part to be produced, in particular forming it into a nonwoven;
d) conveying the formed mixture to a preheating device;
e) heating the formed mixture to 100-180° C.;
f) pressing the formed mixture without significant heating; and
g) irradiating the pressed mixture with electrons in the energy range from 1 MeV to 10 MeV.

### Claim 2 (depends on 1)

Method according to claim 1, characterised in that in step a) irradiation takes place with a dosage between 50 and 150 kGy, in particular with a dosage input of 100 kGy plus/minus 20 kGy.

### Claim 3 (depends on 1)

Method according to claim 1, characterised in that in step f) irradiation takes place according to the specified mixture recipe and selected product aim with a dosage from 50 to 250 kGy, in particular 100 kGy plus/minus 20 kGy.

### Claim 4 (depends on 1)

Method according to claim 1, characterised in that in step e) a nonwoven is pressed to form a board.

### Claim 5 (depends on 1)

Method according to claim 1, characterised in that in step b) the particle sizes are in the range from 1000 to 1500 micrometres (μm).

### Claim 6 (depends on 1)

Method according to claim 1, characterised in that in step b) to produce a wood material, 5% to <30% proportions by mass of a polymer are added.

### Claim 7 (depends on 1)

Method according to claim 1, characterised in that in step b) to produce a WPC 30% to 60% proportions by mass of a polymer are added.

### Claim 8 (depends on 1)

Method according to claim 1, characterised in that in step a) the energy range is between 5 and 10 MeV.

### Claim 9 (depends on 1)

Method according to claim 1, characterised in that in step b) the lignocellulose-containing particles are heated before or during the addition of the thermoplastic powder to a temperature from 60° C. to 160° C., preferably to 80° C. to 120° C.

### Claim 10 (depends on 1)

Method according to claim 1, characterised in that before or in step b) the lignocellulose-containing particles are acted upon by an adhesive agent before the addition of the thermoplastic powder.

### Claim 11 (depends on 10)

Method according to claim 10, characterised in that adhesives and/or paraffins, starches and/or albuminous substances are used as adhesive agents.

### Claim 12

Device for producing a composite containing lignocellulose-containing particles, said device comprising:
a) an first electron beam accelerator designed to irradiate the particles with electrons in the energy range >1 MeV;
aa) a screening repository designed to split the particles into three size-dependent fractions via screens into a coarse fraction, a medium fraction, and a fine fraction;
ab) a bottom layer spreader and a top layer spreader designed to form a bottom layer and a top layer from the particles of said fraction;
ac) a middle layer spreader designed to form a middle layer from the particles of said coarse fraction and said medium fraction;
b) at least one mixer designed to mix the irradiated particles with electron-beam-reactive powder of a synthetic polymer, with powder particle sizes <2000 micrometres (μm), and/or with a fluid containing electron-beam-reactive synthetic polymer;
c) a device designed to form the mixture produced in b) in a way corresponding to the form of the composite to be produced;
d) a conveyor for conveying the formed mixture to a preheating device;
wherein said the preheating device is a high frequency heater (HF), an infared heater (IR) or a microwave heater (MW) designed to heat the formed mixture to 100° C. to 180° C.;
e) a press designed to press said formed mixture without significant heating; and
f) a high-energy electron beam accelerator in the energy range from 1 MeV to 10 MeV in an outwardly radiation-protected process chamber to irradiate the pressed and formed mixture carried past by a transport device.

### Claim 13 (depends on 2)

Method according to claim 2, characterised in that in step f) irradiation takes place according to the specified mixture recipe and selected product aim with a dosage from 50 to 250 kGy.

### Claim 14 (depends on 2)

Method according to claim 2, characterised in that in step e) a nonwoven is pressed to form a board.

### Claim 15 (depends on 3)

Method according to claim 3, characterised in that in step e) a nonwoven is pressed to form a board.

### Claim 16 (depends on 2)

Method according to claim 2, characterised in that in step b) the particle sizes are in the range from 1000 to 1500 micrometres (μm).

### Claim 17 (depends on 3)

Method according to claim 3, characterised in that in step b) the particle sizes are in the range from 1000 to 1500 micrometres (μm).