# US 2024/0309125 A1 · Polyethylene for use in the production of crosslinked polyethylene (pex)

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0309125 A1
- Document ID: US20240309125A1
- Status: Published application
- Kind: A1
- Application number: 18/575,941
- Filed: 2022-07-07
- Published: 2024-09-19
- Earliest claimed: 2021-07-08
- Applicants: Borealis AG
- Inventors: Sara Cascone; Elena Pomakhina
- Web page: https://patentgrep.com/patent/US20240309125A1

## CPC

- C08F 10/02: Ethene
- C08L 23/04: Homopolymers or copolymers of ethene
- C08F 4/24: Oxides
- C08F 110/02: Ethene
- C08F 210/16: Copolymers of ethene with alpha-alkenes, e.g. EP rubbers
- C08J 3/247: {Heating methods}
- C08J 7/02: with solvents, e.g. swelling agents
- C08J 2323/04: Homopolymers or copolymers of ethene
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
- C08L: COMPOSITIONS OF MACROMOLECULAR COMPOUNDS (compositions based on polymerisable monomers C08F, C08G; artificial filaments or fibres D01F; textile treating compositions D06)
- C08J: WORKING-UP; GENERAL PROCESSES OF COMPOUNDING; AFTER-TREATMENT NOT COVERED BY SUBCLASSES C08B, C08C, C08F, C08G or C08H (working, e.g. shaping, of plastics B29)

## Abstract

A polyethylene (PE) for the production of crosslinked polyethylene (PEX), having a beneficial balance of unsaturation properties and processability properties, processes for producing crosslinked polyethylene (PEX) from said polyethylene (PE), and the crosslinked polyethylene (PEX) thus produced.

## Claims

### Claim at position 1

1: A polyethylene (PE) for the production of crosslinked polyethylene (PEX), wherein the polyethylene (PE) fulfils inequation (I):
1.4
≤
UI
×
PI
<
20
(
I
)
wherein the unsaturation index (UI) is defined in Formula (i),
UI
=
(
10
^
7
)
/
(
Mw
×
[
vinyl
]
)
(
i
)
wherein
Mw is the weight average molecular mass of the polyethylene (PE), measured according to gel permeation chromatography, as expressed in units of g/mol;
[vinyl] is the concentration of vinyl groups per 1000 CHn carbons of the polyethylene (PE), as measured by 1H-NMR spectroscopy;
and the processability index (PI) is defined in Formula (ii):
PI
=
MFR
21
/
F
120
(
ii
)
wherein
MFR21 is the melt flow rate of the polyethylene (PE), measured according to ISO 1333 at 190° C. at a load of 21.6 kg, as expressed in units of g/10 min;
F120 is the melt strength of the polyethylene (PE), measured according to ISO 16790:2021 at a die pressure of 120 bar, as expressed in units of cN.

### Claim at position 2 (depends on 1)

2: The polyethylene (PE) according to claim 1, having an unsaturation index (UI), as defined in Formula (i), in the range from 70 to 103.

### Claim at position 3 (depends on 1)

3: The polyethylene (PE) according to claim 1, having a processability index (PI), as defined in Formula (ii), in the range from 0.02 to 0.20.

### Claim at position 4 (depends on 1)

4: The polyethylene (PE) according to claim 1, having a melt flow rate MFR21, measured according to ISO 1333 at 190° C. at a load of 21.6 kg, in the range from 2.5 to 30.0 g/10 min.

### Claim at position 5 (depends on 1)

5: The polyethylene (PE) according to claim 1, having an F120 melt strength, measured according to ISO 16790:2021 at a die pressure of 120 bar, in the range from 40 to 120 cN.

### Claim at position 6 (depends on 1)

6: The polyethylene (PE) according to claim 1, having a weight average molecular mass Mw, measured according to gel permeation chromatography, in the range from 150,000 to 300,000 g/mol.

### Claim at position 7 (depends on 1)

7: The polyethylene (PE) according to claim 1, having a vinyl concentration [vinyl], measured by 1H-NMR spectroscopy, in the range from 0.10 to 2.00 vinyl units per 1000 CHn carbons.

### Claim at position 8 (depends on 1)

8: The polyethylene (PE) according to claim 1, having a molecular weight distribution (Mw/Mn), measured according via gel permeation chromatography, in the range from 3 to 20.

### Claim at position 9 (depends on 1)

9: The polyethylene (PE) according to claim 1, having a density, measured according to ISO 1183, in the range from 935 to 965 kg/m3.

### Claim at position 10 (depends on 1)

10: A process for the production of crosslinked polyethylene (PEX), comprising the steps of:
a) soaking polyethylene (PE) according to claim 1, in reactor powder form, in liquid peroxide or a peroxide solution,
b) extruding the soaked polyethylene powder in an extruder, thereby obtaining crosslinked polyethylene (PEX).

### Claim at position 11 (depends on 1)

11: A process for the production of crosslinked polyethylene (PEX), wherein the crosslinking is achieved through the application of radiation to a composition (C) comprising the polyethylene (PE) according to any one of claim 1 in a molten state.

### Claim at position 12 (depends on 11)

12: The process for the production of crosslinked polyethylene (PEX) according to claim 11, wherein the composition (C) further comprises a photoinitiator and the radiation applied to the molten composition is UV radiation.

### Claim at position 13 (depends on 10)

13: The crosslinked polyethylene (PEX) obtainable via the process of claim 10.

### Claim at position 14 (depends on 10, 13)

14: A crosslinked polyethylene pipe, comprising at least 90 wt.-% of the crosslinked polyethylene (PEX) according to claim 13, wherein the pipe is produced either according to claim 10 wherein extrusion step b) is a pipe extrusion step.

### Claim 15

(canceled)

### Claim at position 16 (depends on 11, 13)

16: A crosslinked polyethylene pipe, comprising at least 90 wt. % of the crosslinked polyethylene (PEX) according to claim 13, wherein the pipe is produced according to claim 11 wherein a pipe extrusion step is carried out prior to the crosslinking step.