# US 2024/0308904 A1 · Compositions and methods relating to increased carbon dioxide uptake in mixing and curing of concrete

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0308904 A1
- Document ID: US20240308904A1
- Status: Published application
- Kind: A1
- Application number: 18/184,314
- Filed: 2023-03-15
- Published: 2024-09-19
- Earliest claimed: 2023-03-15
- Assignees: Saudi Arabian Oil Company
- Applicants: Saudi Arabian Oil Company
- Inventors: Mohammed AL MEHTHEL; Sami A. AL ABDULJABBAR; Waseem Rahim KHATRI
- Web page: https://patentgrep.com/patent/US20240308904A1

## CPC

- C04B 7/34: Hydraulic lime cements; Roman cements {; natural cements}
- C04B 28/04: Portland cements
- C04B 28/10: Lime cements or magnesium oxide cements
- C04B 28/12: Hydraulic lime
- C04B 38/103: {the foaming being obtained by the introduction of a gas other than untreated air, e.g. nitrogen}
- C04B 40/0032: {Controlling the process of mixing, e.g. adding ingredients in a quantity depending on a measured or desired value (B28C7/00 takes precedence)}
- C04B 40/0071: {making use of a rise in pressure}
- C04B 40/0231: {Carbon dioxide hardening}
- C09K 8/473: Density reducing additives, e.g. for obtaining foamed cement compositions
- C04B 2103/20: Retarders
- C04B 2103/302: {Water reducers}
- C04B 2103/48: Foam stabilisers
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE

## Abstract

Cementitious compositions comprising lime, which may be foamed or non-foamed compositions, may increase carbon dioxide uptake of the cementitious compositions. Said cementitious compositions may be used in various cementing methods including pre-casting methods, cast-in-place methods, and primary or secondary cementing operations in a wellbore. The carbon dioxide may be added to the cementitious compositions during mixing, during pre-conditioning, during curing, or any combination thereof. Further, the carbon dioxide may be delivered as a gas (e.g., a gas that includes 1 vol % to 100 vol % carbon dioxide) or as a gas-entrained admixture that includes the gas, water, and a foaming agent.

## Claims

### Claim 1

A method comprising:
mixing a cementitious composition comprising:
a cement binder at 0 kg/m3 to 500 kg/m3 based on a dry weight of the cementitious composition;
optionally, a secondary cementitious material at 0.1 kg/m3 to 350 kg/m3 based on the dry weight of the cementitious composition;
lime at 0.1 kg/m3 to 500 kg/m3 based on the dry weight of the cementitious composition;
fine aggregates at 300 kg/m3 to 1500 kg/m3 based on the dry weight of the cementitious composition;
coarse aggregates at 300 kg/m3 to 1200 kg/m3 based on the dry weight of the cementitious composition;
water in a weight ratio to the cement binder, the secondary cementitious material, and the lime cumulatively of 0.2:1 to 0.8:1; and
a foaming agent at 0.01 wt % to 1 wt % based on a weight of the water; and
wherein the cementitious composition has a maximum dry weight of 2000 kg/m3;
injecting a gas into the cementitious composition, the gas comprising carbon dioxide;
placing the cementitious composition having the gas therein in a desired location; and
allowing the cementitious composition having the gas therein to cure to a concrete composition.

### Claim 2 (depends on 1)

The method of claim 1 further comprising:
mixing of the cementitious composition having the gas therein for 1 minute to 30 minutes.

### Claim 3 (depends on 1)

The method of claim 1, wherein the gas is a first gas, and wherein the method further comprises:
exposing the cementitious composition after being placed in the desired location to a second gas that comprises carbon dioxide.

### Claim 4 (depends on 1)

The method of claim 1, wherein the carbon dioxide is present in the gas at 1 vol % to 100 vol %.

### Claim 5 (depends on 1)

The method of claim 1, wherein the cementitious composition further comprises one or more additives at 0.1 wt % to 1 wt % based on a total weight of cementitious components in the cementitious composition.

### Claim 6 (depends on 1)

The method of claim 1, wherein the cementitious composition further comprises 0.1 wt % to 2 wt % of an admixture of a water reducer additive and a retarder additive based on the weight of the cement binder .

### Claim 7

A method comprising:
mixing a cementitious composition comprising:
a cement binder at 0 kg/m3 to 500 kg/m3 based on a dry weight of the cementitious composition;
optionally, a secondary cementitious material at 0.1 kg/m3 to 350 kg/m3 based on the dry weight of the cementitious composition;
lime at 0.1 kg/m3 to 500 kg/m3 based on the dry weight of the cementitious composition;
fine aggregates at 300 kg/m3 to 1500 kg/m3 based on the dry weight of the cementitious composition; and
coarse aggregates at 300 kg/m3 to 1200 kg/m3 based on the dry weight of the cementitious composition; and
wherein the cementitious composition has a maximum dry weight of 2000 kg/m3;
injecting a gas-entrained admixture into the cementitious composition, the gas-entrained mixture comprising carbon dioxide, water in a weight ratio to the cement binder, the secondary cementitious material, and the lime cumulatively of 0.2:1 to 0.8:1, and a foaming agent at 0.01 wt % to 1 wt % based on a weight of the water;
mixing the cementitious composition;
placing the cementitious composition in a desired location; and
allowing the cementitious composition to cure to a concrete composition.

### Claim 8 (depends on 7)

The method of claim 7, wherein the mixing of the cementitious composition is for 1 minute to 30 minutes.

### Claim 9 (depends on 7)

The method of claim 7 further comprising:
exposing the cementitious composition after being placed in the desired location to a second gas that comprises carbon dioxide.

### Claim 10 (depends on 7)

The method of claim 7, wherein the carbon dioxide is present in the gas at 1 vol % to 100 vol %.

### Claim 11 (depends on 7)

The method of claim 7, wherein the cementitious composition further comprises one or more additives at 0.1 wt % to 1 wt % based on a total weight of cementitious components in the cementitious composition.

### Claim 12 (depends on 7)

The method of claim 7, wherein the cementitious composition further comprises 0.1 wt % to 2 wt % of an admixture of a water reducer additive and a retarder additive based on the weight of the cement binder.

### Claim 13

A method comprising:
placing a cementitious composition in a mold, the cementitious composition comprising:
a cement at 0 kg/m3 to 500 kg/m3 based on a dry weight of the cementitious composition;
optionally, a secondary cementitious material at 0.1 kg/m3 to 350 kg/m3 based on the dry weight of the cementitious composition;
lime at 0.1 kg/m3 to 500 kg/m3 based on the dry weight of the cementitious composition;
fine aggregates at 300 kg/m3 to 1500 kg/m3 based on the dry weight of the cementitious composition;
coarse aggregates at 300 kg/m3 to 1200 kg/m3 based on the dry weight of the cementitious composition; and
wherein the cementitious composition has a dry weight of 2000 kg/m3 to 4000 kg/m3;
exposing the cementitious composition in the mold to air for a pre-conditioning period to produce a pre-conditioned member;
placing the pre-conditioned member in an enclosure; and
curing the pre-conditioned member by exposing the pre-conditioned member to a gas comprising carbon dioxide to produce a concrete member.

### Claim 14 (depends on 13)

The method of claim 13, wherein the exposing of the pre-conditioned member to the gas is for 2 hours to 8 hours.

### Claim 15 (depends on 13)

The method of claim 13 further comprising:
exposing the pre-conditioned member to water.

### Claim 16 (depends on 13)

The method of claim 13, wherein an environment inside the enclosure is at 0° C. to 90° C. during the curing.

### Claim 17 (depends on 13)

The method of claim 13, wherein an environment inside the enclosure is at atmospheric pressure to 50 psi above atmospheric pressure during the curing.

### Claim 18 (depends on 13)

The method of claim 13, wherein an environment inside the enclosure is at a relative humidity of 10% to 95% during the curing.

### Claim 19 (depends on 13)

The method of claim 13, wherein the enclosure comprises an adjustable cover.

### Claim 20 (depends on 13)

The method of claim 13, wherein the enclosure is a curing chamber.