# US 2024/0301106 A1 · Catalytic, Sulfur-Free Chain Transfer Agent for Modulation of Network Topology in Crosslinked Photopolymers

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0301106 A1
- Document ID: US20240301106A1
- Status: Published application
- Kind: A1
- Application number: 18/587,704
- Filed: 2024-02-26
- Published: 2024-09-12
- Earliest claimed: 2022-10-31
- Assignees: University of Denver
- Applicants: University of Denver
- Inventors: Brady Worrell; Brian Donovan; Nicholas Bagnall; Meredith Jones
- Web page: https://patentgrep.com/patent/US20240301106A1

## CPC

- C08F 4/46: selected from alkali metals
- C08F 220/14: Methyl esters {, e.g. methyl (meth)acrylate}
- C08F 2/38: Polymerisation using regulators, e.g. chain terminating agents {, e.g. telomerisation}
- C08F 2/48: by ultraviolet or visible light
- C08F 2/50: with sensitising agents
- C08F 4/7096: {Cobalt or compounds thereof}
- C08F 120/14: Methyl esters {, e.g. methyl (meth)acrylate}
- C08F 222/102: {of dialcohols, e.g. ethylene glycol di(meth)acrylate or 1,4-butanediol dimethacrylate}
- C08F: MACROMOLECULAR COMPOUNDS OBTAINED BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS

## Abstract

A method for tailoring mechanical properties of a photopolymer includes providing an active monomer feedstock, adding a sulfur-free chain transfer agent (CTA) to the active monomer feedstock to form a mixture, and curing the mixture under predetermined conditions. The sulfur-free CTA includes a Cobalt(II) complex or a Cobalt(III) complex, the mechanical properties include glass transition temperature, crosslinking density, and/or conversion rate, and a concentration of the sulfur-free CTA is less than 30% of the mixture. The predetermined conditions include intensity, wavelength, and application time of energy from a light source, a cure temperature, and/or the concentration of the sulfur-free CTA in the mixture. The method may further include adding a diluent to the mixture to modify a viscosity of the active monomer feedstock. The diluent may include one of a reactive diluent and a non-reactive diluent, such as methyl methacrylate (MMA) and methacrylate (MA).

## Claims

### Claim 1

A method for tailoring mechanical properties of a photopolymer, the method comprising:
providing an active monomer feedstock;
adding a sulfur-free chain transfer agent (CTA) to the active monomer feedstock to form a mixture; and
curing the mixture under predetermined conditions;
wherein the sulfur-free CTA includes at least one of a Cobalt(II) complex and a Cobalt(III) complex,
wherein mechanical properties include at least one of glass transition temperature, crosslinking density, and conversion rate, and
wherein a concentration of the sulfur-free CTA is less than 30% of the mixture.

### Claim 2 (depends on 1)

The method of claim 1, wherein the predetermined conditions include intensity, wavelength, and application time of energy from a light source, a cure temperature, the concentration of the sulfur-free CTA in the mixture, and diffusion of the sulfur-free CTA within the mixture.

### Claim 3 (depends on 1)

The method of claim 1, further comprising adding a diluent to the mixture to modify a viscosity of the active monomer feedstock.

### Claim 4 (depends on 3)

The method of claim 3, wherein the diluent includes at least one of a reactive diluent and a non-reactive diluent.

### Claim 5 (depends on 3)

The method of claim 3, wherein the diluent includes at least one of methyl methacrylate (MMA) and methacrylate (MA).

### Claim 6 (depends on 1)

The method of claim 1, wherein adding the sulfur-free CTA includes adding CoBF-iPr as the sulfur-free CTA.