# US 2024/0293855 A1 · A Low Roughness Lithium Metal Anode Produced Via Multiple Compressions

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0293855 A1
- Document ID: US20240293855A1
- Status: Published application
- Kind: A1
- Application number: 18/578,374
- Filed: 2023-03-07
- Published: 2024-09-05
- Earliest claimed: 2022-03-07
- Applicants: Soelect Inc.
- Inventors: Sungjin Cho
- Web page: https://patentgrep.com/patent/US20240293855A1

## CPC

- B21B 3/00: Rolling materials of special alloys so far as the composition of the alloy requires or permits special rolling methods or sequences {; Rolling of aluminium, copper, zinc or other non-ferrous metals}(altering special metallurgical properties of alloys, other than structure consolidation or mechanical properties resulting therefrom C21D, C22F)
- B21B 1/22: for rolling {plates, strips,} bands or sheets of indefinite length (B21B1/42 takes precedence)
- B21B 1/222: {in a rolling-drawing process; in a multi-pass mill}
- B21B 1/227: {Surface roughening or texturing}
- B21B 1/24: in a continuous {or semi-continuous} process {(B21B1/224 takes precedence)}
- B21B 13/00: Metal-rolling stands, i.e. an assembly composed of a stand frame, rolls, and accessories (B21B17/00 - B21B23/00 take precedence)
- B21B 13/02: with axes of rolls arranged horizontally
- H01M 4/043: {involving compressing or compaction}
- H01M 4/0435: {Rolling or calendering}
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 12/04: composed of a half-cell of the fuel-cell type and of a half-cell of the primary-cell type
- H01M 12/08: composed of a half-cell of a fuel-cell type and a half-cell of the secondary-cell type
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- B21B: ROLLING OF METAL (auxiliary operations used in connection with metal-working operations covered in B21, see B21C; bending by rolling B21D; manufacture of particular objects, e.g. screws, wheels, rings, barrels, balls, by rolling B21H; pressure welding by means of a rolling mill B23K20/04)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A process that includes compressing a lithium metal material having an initial material thickness and initial material surface roughness into a compressed lithium metal material having a first compressed material thickness is disclosed. The method further includes compressing the compressed lithium metal material one or more additional times into a further compressed lithium metal material having a final compressed material thickness and a final material surface roughness, wherein the final compressed material thickness having a value at or between 5 micrometers and 200 micrometers and is less than the initial compressed material thickness and wherein the final material surface roughness is smoother than the initial material surface roughness and is characterized by Ra value of less than or equal to 1.0 micrometers and a Rz value of less than or equal to 5.0 micrometers.

## Claims

### Claim 1

A method for producing a low roughness lithium metal material anode via multiple compressions comprising:
compressing, by a first rolling mill unit, a lithium metal material having an initial material thickness and initial material surface roughness into a compressed lithium metal material having a first compressed material thickness, wherein the first compressed material thickness is less than the initial material thickness; and
compressing, by the first rolling mill unit or at least a second rolling mill unit, the compressed lithium metal material one or more additional times into a further compressed lithium metal material having a final compressed material thickness and a final material surface roughness, wherein the final compressed material thickness having a value at or between 5 micrometers and 200 micrometers and is less than the initial compressed material thickness and wherein the final material surface roughness is smoother than the initial material surface roughness and is characterized by an average roughness (Ra) value of less than or equal to 1.0 micrometers and a maximum roughness (Rz) value of less than or equal to 5.0 micrometers.

### Claim 2 (depends on 1)

The method of claim 1 wherein the lithium metal material is repeatedly introduced to the first rolling mill unit in a one-way mechanical direction via multiple passes.

### Claim 3 (depends on 1)

The method of claim 1 wherein the lithium metal material is introduced to the first rolling mill unit and the at least second rolling mill unit of the rolling mill system in a single mechanical direction via a single pass.

### Claim 4 (depends on 3)

The method of claim 3 wherein the lithium metal material is introduced to the rolling mill system without folding the lithium metal material and/or without introducing the lithium material in a bi-directional manner.

### Claim 5 (depends on 1)

The method of claim 1 wherein the average roughness value and maximum roughness value exhibited by the further compressed lithium metal material are both reduced by each compression performed by the first rolling mill unit and/or the second rolling mill unit.

### Claim 6 (depends on 1)

The method of claim 1 wherein the first rolling mill unit and/or the second rolling mill unit is a tandem rolling mill device.

### Claim 7 (depends on 1)

The method of claim 1 wherein the lithium metal material is a lithium metal workpiece and/or at least a portion of lithium metal foil.

### Claim 8 (depends on 1)

The method of claim 1 wherein the further compressed lithium metal material exhibits a reduction in the number of grains, as compared to the lithium metal material and compressed lithium metal material, after being compressed by one or more of the first rolling mill unit and the second rolling mill unit.

### Claim 9 (depends on 1)

The method of claim 1 wherein the first rolling mill unit and the second rolling mill unit are positioned in series and configured with incrementally decreasing rolling gap sizes such that the lithium metal material is incrementally compressed by the rolling mill system.

### Claim 10 (depends on 9)

The method of claim 9 wherein the compression rate applied to the lithium metal material is controlled by incrementally decreasing the rolling gap spaces associated with working roller components of the first rolling mill unit and/or the second rolling mill unit.

### Claim 11 (depends on 10)

The method of claim 10 wherein a rolling gap space formed by the positioning of an upper roller component and a lower working roller component of the first rolling mill unit and/or the at least second rolling mill unit is adjusted to incrementally control the compression rate applied to the lithium metal material.

### Claim 12 (depends on 1)

The method of claim 1 wherein the further compressed lithium metal material is used to manufacture a lithium metal anode.

### Claim 13 (depends on 12)

The method of claim 12 wherein the lithium metal anode is compatible with a lithium-ion battery, a lithium sulfur battery, a lithium air battery, or a solid-state battery.

### Claim 14

A method for controlling the compression rate of lithium metal material comprising:
introducing a lithium metal material having an initial material thickness and initial material surface roughness into a first rolling mill unit of a rolling mill system;
compressing, by the first rolling mill unit, the lithium metal material into a compressed lithium metal material having a first compressed material thickness and first compressed material surface roughness;
introducing the compressed lithium metal material into either i) the first rolling mill again or ii) at least a second rolling mill unit of the rolling mill system that is positioned in series with the first rolling mill unit; and
compressing, by the first rolling mill unit or the at least second rolling mill unit, the compressed lithium metal material one or more additional times into a further compressed lithium metal material having a final compressed material thickness and a final material surface roughness, wherein the final compressed material thickness having a value at or between 5 micrometers and 200 micrometers and is less than the initial compressed material thickness and wherein the final material surface roughness is smoother than the initial material surface roughness and is characterized by an average roughness (Ra) value of less than or equal to 1.0 micrometers and a maximum roughness (Rz) value of less than or equal to 5.0 micrometers.