# US 2024/0287669 A1 · Method for coating stainless steel press plates and coated press plates produced thereby

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0287669 A1
- Document ID: US20240287669A1
- Status: Published application
- Kind: A1
- Application number: 18/652,130
- Filed: 2024-05-01
- Published: 2024-08-29
- Earliest claimed: 2016-02-09
- Assignees: Wilsonart LLC
- Applicants: Wilsonart LLC
- Inventors: Muyuan M. Ma
- Web page: https://patentgrep.com/patent/US20240287669A1

## CPC

- C23C 14/0688: {Cermets, e.g. mixtures of metal and one or more of carbides, nitrides, oxides or borides}
- B30B 15/062: {Press plates}
- B32B 15/00: Layered products comprising {a layer of} metal
- B32B 15/01: all layers being exclusively metallic {(making layered metal workpieces by pressure cladding B23K20/22; making coatings with a metallic material characterised by its composition C23C30/00)}
- B32B 15/012: {one layer being formed of an iron alloy or steel, another layer being formed of aluminium or an aluminium alloy}
- B32B 37/0046: {characterised by constructional aspects of the apparatus}
- C23C 14/025: {Metallic sublayers}
- C23C 14/067: {Borides}
- C23C 14/352: {using more than one target (C23C14/56 takes precedence)}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- B30B: PRESSES IN GENERAL (producing ultra-high pressure or ultra-high pressure and high temperature to effect modifications of a substance, e.g. for making artificial diamonds B01J3/00 ){(compressing means for refuse receptacles B65F1/1405)}
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM

## Abstract

A method for coating stainless steel press plates includes preparing the stainless steel press plate for coating and coating the stainless steel press plate with a diboride doped with 1%-5% by weight aluminum to produce a diboride-aluminum coating. The step of coating includes applying the diboride-aluminum coating to a stainless steel press plate using a magnetron sputter coating system.

## Claims

### Claim 1

A method for coating stainless steel press plates, comprising:
preparing the stainless steel press plate for coating;
coating the stainless steel press plate with a diboride doped with 1%-5% by weight aluminum to produce a diboride-aluminum coating, wherein the step of coating includes applying the diboride-aluminum coating to a stainless steel press plate using a magnetron sputter coating system.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the diboride is titanium diboride.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the stainless steel press plate is a 410 stainless steel high gloss press plates.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the stainless steel press plate is a 300 stainless steel press plate, a 410 stainless steel press plate, a 420 stainless steel press plate, a 630 stainless steel press plate, or a 633 stainless steel press plate.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the diboride-aluminum coating has a Vickers hardness of at least 35 GPa.

### Claim 6 (depends on 5)

The method according to claim 5, wherein the diboride-aluminum coating has a Vickers hardness of 46 GPa.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the diboride-aluminum coating has a thickness of about 3 microns.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the step of coating includes doping the diboride with 2% by weight aluminum.

### Claim 9 (depends on 8)

The method according to claim 8, wherein the step of coating includes applying the diboride-aluminum coating at a substrate bias of 60-90 V and at temperature of 200° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the diboride-aluminum coating has a minimum bond strength of 1.6 kilogram force.

### Claim 11 (depends on 10)

The method according to claim 10, wherein the diboride-aluminum coating has a minimum bond strength of 1.8 kilogram force.

### Claim 12 (depends on 1)

The method according to claim 1, wherein the step of preparing the stainless steel press plate includes cleaning a pressing side of the stainless steel press plate.

### Claim 13 (depends on 12)

The method according to claim 12, wherein the step of preparing the stainless steel press plate includes etching the pressing side of the stainless steel press plate.

### Claim 14 (depends on 12)

The method according to claim 12, wherein the step of preparing the stainless steel press plate includes applying a layer of titanium directly onto the pressing side of the stainless steel press plate

### Claim 15 (depends on 1)

The method according to claim 1, wherein the step of coating includes applying multiple layers of the diboride-aluminum coating.

### Claim 16 (depends on 1)

The method according to claim 1, wherein the diboride-aluminum coating is applied in a two-stage process composed of a gradient based diboride-aluminum coating layer and a top titanium diboride-aluminum coating layer.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the gradient based diboride-Al coating layer is 600 nm in thickness.

### Claim 18 (depends on 17)

The method according to claim 17, wherein the top diboride-aluminum coating layer is 1,240 nm in thickness.

### Claim 19

A coated stainless steel press plate manufactured in according with the method comprising:
preparing the stainless steel press plate for coating;
coating the stainless steel press plate with a diboride doped with 1%-5% by weight aluminum to produce a diboride-aluminum coating, wherein the step of coating includes applying the diboride-aluminum coating to a stainless steel press plate using a magnetron sputter coating system.