A method (200, 400, 500, 600) for drawing a bare optical fiber (118) from a cylindrical glass preform (102) in a furnace chamber (104), the method (200, 400, 500, 600) comprising:
- melting the cylindrical glass preform (102) in presence of a first inert gas and a second inert gas inside the furnace chamber (104) to draw the bare optical fiber (118) such that the first inert gas and the second inert gas are in a predefined ratio,
- and
- cooling the bare optical fiber (118), wherein a short-term Bare Fiber Diameter (BFD) variation of the bare optical fiber (118) is less than 0.1 micrometers (μm) from a mean diameter of the bare optical fiber (118)
- wherein the first inert gas is defined by a first atomic number and the second inert gas is defined by a second atomic number, wherein the second atomic number is at least 5 times the first atomic number.