# US 2024/0278213 A1 · Photocatalytic layer arrangement and method for producing such a layer arrangement

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0278213 A1
- Document ID: US20240278213A1
- Status: Published application
- Kind: A1
- Application number: 18/693,297
- Filed: 2022-07-29
- Published: 2024-08-22
- Earliest claimed: 2021-09-24
- Assignees: Dr. Johannes Heidenhain GmbH
- Applicants: DR. JOHANNES HEIDENHAIN GmbH
- Inventors: Peter SPECKBACHER; Wolfgang SEDLMEIER; Martina DOWY; Réka CSIKI; Bernhard WUNDERLICH
- Web page: https://patentgrep.com/patent/US20240278213A1

## CPC

- B01J 21/063: {Titanium; Oxides or hydroxides thereof}
- B01J 23/26: Chromium
- B01J 35/19: {Catalysts containing parts with different compositions}
- B01J 35/39: Photocatalytic properties
- B01J 35/393: {Metal or metal oxide crystallite size}
- B01J 35/40: characterised by dimensions, e.g. grain size (in a colloidal state B01J35/23; crystallite size B01J35/77)
- B01J 37/0228: {in several steps}
- B01J 37/0244: {Coatings comprising several layers}
- B01J 37/347: {Ionic or cathodic spraying; Electric discharge}
- C03C 17/3605: {Coatings of the type glass/metal/inorganic compound}
- C03C 17/3649: {made of metals other than silver}
- C23C 14/0057: {using reactive gases other than O2, H2O, N2, NH3 or CH4}
- C23C 14/083: {of refractory metals or yttrium}
- C03C 2218/155: by reactive sputtering
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)

## Abstract

A photocatalytic layer arrangement includes a carrier substrate on which a chromium layer with a defined nitrogen content is deposited. A titanium oxide layer having the formula TiOx (x=2-4) is grown on the chromium layer, and the anatase phase of the titanium oxide layer with respect to the rutile phase of the titanium oxide layer has a percentage in the range of 30%-90%.

## Claims

### Claim at position 1

1-15. (canceled)

### Claim 16

A photocatalytic layer arrangement, comprising:
a carrier substrate;
a chromium layer having a defined nitrogen content arranged on the carrier substrate; and
a titanium oxide layer having the formula TiOx(x=2-4) arranged on the chromium layer;
wherein an anatase phase of the titanium oxide layer with respect to a rutile phase of the titanium oxide layer has a percentage between 30% and 90%.

### Claim 17 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the chromium layer is arranged as a deposited layer on the carrier substrate.

### Claim 18 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the titanium oxide layer is arranged as a grown layer on the chromium layer.

### Claim 19 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the anatase phase of the titanium oxide layer with respect to the rutile phase of the titanium oxide layer has a percentage between 50% and 80%.

### Claim 20 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein a layer thickness of the titanium oxide layer is between 30 nm and 300 nm.

### Claim 21 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the titanium oxide layer has a granular surface structure with anatase crystallites in a size between 20 nm and 120 nm.

### Claim 22 (depends on 21)

The photocatalytic layer arrangement according to claim 21, wherein the anatase crystallites in the titanium oxide layer have a substructure.

### Claim 23 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein a layer thickness of the chromium layer is between 30 nm and 150 nm.

### Claim 24 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the nitrogen contents of the chromium layer is between 15 at % and 25 at %.

### Claim 25 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the nitrogen content of the chromium layer is between 15 at % and 25 at % at least to a depth of 10 nm.

### Claim 26 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the carrier substrate includes glass.

### Claim 27 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the photocatalytic layer arrangement is arranged in an optical sensor adapted to examine samples that include biological molecules.

### Claim 28 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the carrier substrate includes borosilicate glass and/or quartz glass.

### Claim 29 (depends on 16)

The photocatalytic layer arrangement according to claim 16, wherein the carrier substrate includes a glass ceramic, zinc selenide, and/or potassium bromide.

### Claim 30

A method for producing a photocatalytic layer arrangement, comprising:
applying a chromium layer having a defined nitrogen content to a carrier substrate using a reactive sputtering method; and
depositing a titanium oxide layer having the formula TiOx (x=2-4) on the chromium layer using a low-temperature sputtering method;
wherein a titanium oxide layer grows during the deposition, an anatase phase of the titanium oxide layer respect to an rutile phase of the titanium oxide layer has a percentage between 30% and 90%.

### Claim 31 (depends on 30)

The method according to claim 30, wherein the nitrogen content of the chromium layer is between 15 at % and 25 at %, and the nitrogen is contained near a surface of the chromium layer at least to a depth of 10 nm.

### Claim 32 (depends on 30)

The method according to claim 30, wherein the chromium layer is applied using the reactive sputtering method with an argon-nitrogen flow ratio that satisfies the following condition:Ar (sccm)/N2 (sccm)=1.0 to 2.0.

### Claim 33 (depends on 30)

The method according to claim 30, wherein a layer thickness of the chromium layer is between 30 nm and 150 nm.

### Claim 34 (depends on 30)

The method according to claim 30, wherein a layer thickness of the titanium oxide layer is between 30 nm and 300 nm.

### Claim 35 (depends on 30)

The method according to claim 30, wherein a granular surface structure of the titanium oxide layer includes anatase crystallites having a size between 20 nm and 120 nm.