# US 2024/0274913 A1 · Method for recovering waste lithium cobalt oxide battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0274913 A1
- Document ID: US20240274913A1
- Status: Published application
- Kind: A1
- Application number: 18/559,058
- Filed: 2022-08-24
- Published: 2024-08-15
- Earliest claimed: 2021-11-30
- Assignees: Guangdong Brunp Recycling Technology Co., Ltd.; Hunan Brunp Recycling Technology Co., Ltd.; Yichang Brunp Contemporary Amperex Co., Ltd.
- Applicants: Guangdong Brunp Recycling Technology Co., Ltd.; Hunan Brunp Recycling Technology Co., Ltd.; Yichang Brunp Contemporary Amperex Co., Ltd.
- Inventors: Yingsheng ZHONG; Haijun YU; Yinghao XIE; Aixia LI; Bo LI; Changdong LI
- Web page: https://patentgrep.com/patent/US20240274913A1

## CPC

- C01B 32/215: Purification; Recovery or purification of graphite formed in iron making, e.g. kish graphite
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- C01F 7/428: by oxidation in an aqueous solution
- C22B 1/248: of metal scrap or alloys
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/165: {with organic acids}
- C22B 3/22: by physical processes, e.g. by filtration, by magnetic means {, or by thermal decomposition} (treatment or purification of solutions by liquid-liquid extraction C22B3/26)
- C22B 3/3842: {Phosphinic acid, e.g. H2P(O)(OH)}
- C22B 3/3844: {Phosphonic acid, e.g. H2P(O)(OH)2}
- C22B 3/408: {using a mixture of phosphorus-based acid derivatives of different types}
- C22B 7/005: {Separation by a physical processing technique only, e.g. by mechanical breaking}
- C22B 7/007: {by acid leaching}
- C22B 15/0004: {without modification of the copper constituent}
- C22B 15/0071: {containing sulfur}
- C22B 15/0089: {by chemical methods}
- C22B 21/0007: {Preliminary treatment of ores or scrap or any other metal source (Bayer processes C01F)}
- C22B 21/0023: {from waste materials}
- C22B 23/0415: {with acids or salt solutions except ammonium salts solutions}
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0453: {Treatment or purification of solutions, e.g. obtained by leaching (C22B23/0407 takes precedence)}
- C22B 23/0461: {by chemical methods}
- C22B 26/12: Obtaining lithium
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01F: COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM, CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THE RARE-EARTH METALS (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts of peroxyacids C01B15/00; sulfides or polysulfides of magnesium, calcium, strontium, or barium C01B17/42; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds other than ammonia or cyanogen containing nitrogen and non-metals and optionally metals C01B21/082; amides or imides of silicon C01B21/087}; metal {imides or} amides C01B21/092, {C01B21/0923}; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanic acid C01C3/14; salts of cyanamide C01C3/16; thiocyanates C01C3/20; {double sulfates of magnesium with sodium or potassium C01D5/12; with other alkali metals C01D15/00, C01D17/00})
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

Disclosed is a method for recovering a waste lithium cobalt oxide battery, the method comprising: feeding a lithium cobalt oxide battery black powder in a column-shaped container, adding a first acid to the column-shaped container for heat leaching until solids in the column-shaped container are not reduced any more so as to obtain a first leachate and leaching residues, wherein the first acid is a weak acid, and a filtering structure is arranged at the bottom of the column-shaped container; and adding a second acid to the column-shaped container containing the leaching residues for heat leaching until solids in the column-shaped container are not reduced any more so as to obtain a second leachate and graphite, wherein the second acid is a strong acid. According to the present invention, consumption of an inorganic strong acid can be reduced, emission of strong acid gas is reduced, and green and low-carbon heat leaching of the black powder is achieved.

## Claims

### Claim 1

A method for recycling a spent lithium cobalt oxide battery, comprising the following steps:
S1: putting black powders from a lithium cobalt oxide battery into a column-shaped container, adding a first acid to the column-shaped container for hot leaching until solids in the column-shaped container no longer decrease, to obtain a first leachate and a leaching residue, wherein the first acid is selected from the group consisting of methanoic acid, acetic acid, benzoic acid and a mixture thereof, and the concentration of the first acid is 0.1-35 wt %; the bottom of the column-shaped container is provided with a filter structure; the first acid has a temperature of 35-80° C., and the first acid further contains sodium thiosulfate in an amount of 0.1-12 wt %; and
S2: adding a second acid to the column-shaped container containing the leaching residue for hot leaching until solids in the column-shaped container no longer decrease, to obtain a second leachate and graphite, wherein the second acid is a strong acid.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in S1, the black powders from a lithium cobalt oxide battery is obtained by: disassembling the spent lithium cobalt oxide battery to obtain cells, measuring the voltage of the cells to classify the cells into low-voltage cells and high-voltage cells, discharging, pyrolyzing and crushing the low-voltage cells, and removing copper-aluminum foils and separators to obtain the black powders from a lithium cobalt oxide battery.

### Claim 3 (depends on 2)

The method according to claim 2, wherein the high-voltage cells are assembled into a battery pack to provide power for heating.

### Claim 4 (depends on 1)

The method according to claim 1, further comprising a step of producing cobalt oxalate from the first leachate by
adding alkali to the first leachate to adjust pH and separating aluminium hydroxide precipitations;
adding the second acid to adjust pH to 3.0-4.5, adding a synergistic extractant for extraction and separating a cobalt-containing phase;
adding the second acid to the cobalt-containing phase for back-extraction and separating an aqueous phase by back-extraction; and
adding a compound containing oxalate to the aqueous phase from the back-extraction and obtaining a cobalt oxalate by solid-liquid separation.

### Claim 5 (depends on 1)

The method according to claim 1, wherein in S2, to the second leachate, adding aluminum powders to separate out copper sponge, and adding alkali to adjust pH to 4.0-6.5, and separating out aluminium hydroxide.

### Claim 6

(canceled)

### Claim 7

(canceled)

### Claim 8 (depends on 1)

The method according to claim 1, wherein in S2, the second acid is selected from the group consisting of hydrochloric acid, phosphoric acid, sulfuric acid, nitric acid and a mixture thereof; the concentration of the second acid is 0.01-0.2 mol/L; and the second acid has a temperature of 35-80° C.

### Claim 9 (depends on 4)

The method according to claim 4, wherein the synergistic extractant consists of extractant and cyclohexane at a mass ratio of (15-50):(30-85), wherein the extractant consists of dialkyl hypophosphorous acid and mono-2-ethylhexyl (2-ethylhexyl)phosphonate at a volume ratio of (1-4):(1-10).

### Claim 10 (depends on 4)

The method according to claim 4, wherein the compound containing oxalate is selected from the group consisting of oxalic acid, ammonium oxalate, sodium oxalate and a mixture thereof.