# US 2024/0274906 A1 · Method for Regenerated Raw Materials from Waste Cadmium Nickel Battery Based on Solvent Extraction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0274906 A1
- Document ID: US20240274906A1
- Status: Published application
- Kind: A1
- Application number: 18/022,543
- Filed: 2022-06-10
- Published: 2024-08-15
- Earliest claimed: 2022-04-27
- Assignees: South China University of Technology; Sichuan Changhong Battery Co., Ltd
- Applicants: South China University of Technology; Sichuan Changhong Battery Co., Ltd
- Inventors: Yongqing ZHANG; Lei ZHOU; Mingzhang LIU; Juncong FU; Jiang CHEN; Jihong YI
- Web page: https://patentgrep.com/patent/US20240274906A1

## CPC

- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- C01G 11/00: Compounds of cadmium
- C01G 11/003: {Preparation involving a liquid-liquid extraction, an adsorption or an ion-exchange}
- C01G 51/01: Preparation or separation involving a liquid-liquid extraction, an adsorption or an ion-exchange
- C01G 51/80: Compounds containing cobalt, with or without oxygen or hydrogen, and containing one or more other elements (C01G51/02, C01G51/06 - C01G51/40 take precedence)
- C01G 53/01: Preparation or separation involving a liquid-liquid extraction, an adsorption or an ion-exchange
- C01G 53/80: Compounds containing nickel, with or without oxygen or hydrogen, and containing one or more other elements (C01G53/02, C01G53/06 - C01G53/40 take precedence)
- C07C 51/412: {by conversion of the acids, their salts, esters or anhydrides with the same carboxylic acid part}
- C22B 3/08: Sulfuric acid {, other sulfurated acids or salts thereof}
- C22B 3/3842: {Phosphinic acid, e.g. H2P(O)(OH)}
- C22B 3/3846: {Phosphoric acid, e.g. (O)P(OH)3}
- C22B 3/44: by chemical processes (treatment or purification of solutions by liquid-liquid extraction C22B3/26, by ion-exchange extraction C22B3/42)
- C22B 7/005: {Separation by a physical processing technique only, e.g. by mechanical breaking}
- C22B 7/007: {by acid leaching}
- C22B 17/04: {by wet processes}
- C22B 23/043: {Sulfurated acids or salts thereof}
- C22B 23/0484: {in acidic type solutions}
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

A method for regenerating raw materials of waste Nickel-Cadmium batteries based on solvent extraction is disclosed. The method is used for disassembling, rinsing and shredding industrial waste from Nickel-Cadmium batteries. The solvent extraction technology is easy for large-scale and continuous production, and valuable metals such as cadmium, cobalt and nickel are extracted from the waste Nickel-Cadmium batteries to prepare products such as cadmium nitrate, cobalt nitrate, nickel nitrate which are directly used for producing raw materials for Nickel-Cadmium batteries. No new waste salt and waste residues are generated in the process. High-efficiency separation and purification of all valuable metals during the regeneration of waste Nickel-Cadmium batteries and the full-life cycle regeneration cycle of Nickel-Cadmium batteries are achieved.

## Claims

### Claim 1

A method for regenerating a raw materials of waste Nickel-Cadmium batteries based on a solvent extraction comprising the following steps:
1) disassembling, rinsing, and shredding an industrial waste cadmium-nickel battery to obtain a material;
2) leaching the material with a sulfuric acid solution to obtain a leachate;
3) taking the leachate obtained in step 2, adding a first oxidizing agent to the leachate to oxidize Fe2+ in the leachate to Fe3+-, adjusting a pH to 0.8-1.8, adding a first extractant, and extracting to obtain a first raffinate and a first organic phase; washing the first organic phase with dilute sulfuric acid, and stripping with an oxalic acid solution to obtain an iron oxalate solution;
4) adjusting a pH of the first raffinate to 2.0-3.0, adding the first extractant to the first raffinate for a first extraction to obtain a second raffinate and a second organic phase; washing the second organic phase with a cadmium sulfate solution, and stripping with a dilute nitric acid solution to obtain a cadmium nitrate solution;
5) adjusting a pH of the second raffinate to 4.5-5.5, and adding a second extractant for a second extraction to obtain a third raffinate and a third organic phase; washing the third organic phase with a cobalt sulfate solution, and stripping with the dilute nitric acid solution to obtain an cobalt nitrate solution;
6) adjusting a pH of the third raffinate to 5.0-6.0, and adding the first extractant to the third raddinate for a third extraction to obtain a sodium sulfate solution and a fourth organic phase; washing the fourth organic phase with a nickel nitrate solution, and stripping with the dilute nitric acid solution to obtain a resulting nickel nitrate solution; wherein the first extractant is formed by mixing P204 and a solvent oil, and the second extractant is formed by mixing DZ272 and the solvent oil; and the first extractant and the second extractant are saponified when used.

### Claim 2 (depends on 1)

The method according to claim 1, wherein in step 1, a content of K, Li and Ca elements in a waste electrode plate obtained from the step of disassembling, rinsing, and shredding the industrial waste cadmium-nickel battery is less than 0.01 wt %, wherein the waste electrode plate is treated with a two-stage wet shredding, a maximum particle size of a shredded industrial waste cadmium-nickel battery is 10×100 mm, and a moisture content of the shredded industrial waste cadmium-nickel battery is less than 10%.

### Claim 3 (depends on 1)

The method according to claim 1, wherein in step 2, a mixing ratio of the material to the sulfuric acid solution is 1:5-1:12, a concentration of the sulfuric acid solution is 1.5-3.0 mol/l, a temperature of an acid leaching process system is 343-368K, an acid leaching time is 6-24 h, wherein leaching further comprises stirring during the leaching at a stirring speed of 150-300 rpm.

### Claim 4 (depends on 1)

The method according to claim 1, where in in step 2, the step of leaching the material further comprises adding a second oxidizing agent to facilitate a dissolution of the material, wherein the second oxidizing agent is a hydrogen peroxide solution, and a concentration of the hydrogen peroxide solution is 30-40%, and an addition amount of the hydrogen peroxide solution is 6-12% of a volume of the leachate in step 2.

### Claim 5 (depends on 1)

The method according to claim 1, wherein in step 3, the first oxidizing agent is hydrogen peroxide, and an adding amount of the first oxidizing agent added is 1.2-2 times a molar amount of ferrous ions in a leaching solution; wherein extracting is performed 3-7 times, the washing stages are 1-3, and stripping is performed 3-7 times; and each stripping is performed at 308-323K; extracting and washing operations are performed at 288-298K; an amount of oxalic acid in the oxalic acid solution is 1.5-2 times a molar amount of the Fe3+ in the first organic phase.

### Claim 6 (depends on 1)

The method according to claim 1, wherein in step 4, the first extraction is performed 3-7 times, the washing is performed 3-5 times, and the stripping is performed 3-5 times; wherein an amount of nitric acid in the dilute nitric acid solution is 2-2.5 times a molar amount of Cd2+ in the second organic phase; and the cadmium nitrate solution obtained by stripping is evaporated and concentrated to obtain the cadmium nitrate solution or a cadmium nitric crystal meeting a quality standard for the raw materials of the Nickel-Cadmium batteries.

### Claim 7 (depends on 1)

The method according to claim 1, wherein in step 5), the second extraction is performed 3-7 times, the washing is performed 2-6 times, and the stripping is performed 2-6 times; wherein the second extraction is performed at 308-323K, and the stripping and the washing are performed at 288-298K; a nitric acid in the dilute nitric acid solution is 2-2.5 times a molar amount of Co2+ in the third organic phase; and wherein the cobalt nitrate solution obtained by stripping is evaporated and concentrated to obtain the cobalt nitrate solution or a cobalt nitric crystal meeting a quality standard of the raw materials of the Nickel-Cadmium batteries.

### Claim 8 (depends on 1)

The method according to claim 1, wherein in step 6), the third extraction is performed 6-10 times; the washing is performed 2-6 times; and the stripping is performed 2-6 times; wherein the third extraction is performed at 308-323K, the stripping and the washing are performed at 288-298K; and wherein a nitric acid in the dilute nitric acid solution is 2-2.5 times a molar amount of Ni2+ in the fourth organic phase, and the resulting nickel nitrate solution obtained by stripping is evaporated and concentrated to obtain the resulting nickel nitrate solution or a nickel nitric crystal conforming to a quality standards of the raw materials of the Nickel-Cadmium batteries. raw material.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the first extractant or the second extractant is saponifed with a sodium hydroxide solution having a mass fraction of 25-35%; a concentration of the P204 in the first extractant is 0.5-1.2 mol/L; and a concentration of the DZ272 in the second extractant is 0.05-0.15 mol/L.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the solvent oil is a 230 # solvent oil or a 260 #solvent oil (sulfonated kerosene); the sodium sulfate solution is kept at a temperature of 308-323K, and an industrial grade sodium sulfate is obtained after an evaporation and a concentration of the sodium sulfate solution.

### Claim 11 (depends on 2)

The method according to claim 2, wherein the solvent oil is a 230 #solvent oil or a 260 #solvent oil (sulfonated kerosene); the sodium sulfate solution is kept at a temperature of 308-323K, and an industrial grade sodium sulfate is obtained after an evaporation and a concentration of the sodium sulfate solution.

### Claim 12 (depends on 3)

The method according to claim 3, wherein the solvent oil is a 230 #solvent oil or a 260 #solvent oil (sulfonated kerosene); the sodium sulfate solution is kept at a temperature of 308-323K, and an industrial grade sodium sulfate is obtained after an evaporation and a concentration of the sodium sulfate solution.

### Claim 13 (depends on 4)

The method according to claim 4, wherein the solvent oil is a 230 #solvent oil or a 260 #solvent oil (sulfonated kerosene); the sodium sulfate solution is kept at a temperature of 308-323K, and an industrial grade sodium sulfate is obtained after an evaporation and a concentration of the sodium sulfate solution.

### Claim 14 (depends on 5)

The method according to claim 5, wherein the solvent oil is a 230 #solvent oil or a 260 #solvent oil (sulfonated kerosene); the sodium sulfate solution is kept at a temperature of 308-323K, and an industrial grade sodium sulfate is obtained after an evaporation and a concentration of the sodium sulfate solution.

### Claim 15 (depends on 6)

The method according to claim 6, wherein the solvent oil is a 230 #solvent oil or a 260 #solvent oil (sulfonated kerosene); the sodium sulfate solution is kept at a temperature of 308-323K, and an industrial grade sodium sulfate is obtained after an evaporation and a concentration of the sodium sulfate solution.

### Claim 16 (depends on 7)

The method according to claim 7, wherein the solvent oil is a 230 #solvent oil or a 260 #solvent oil (sulfonated kerosene); the sodium sulfate solution is kept at a temperature of 308-323K, and an industrial grade sodium sulfate is obtained after an evaporation and a concentration of the sodium sulfate solution.

### Claim 17 (depends on 8)

The method according to claim 8, wherein the solvent oil is a 230 #solvent oil or a 260 #solvent oil (sulfonated kerosene); the sodium sulfate solution is kept at a temperature of 308-323K, and an industrial grade sodium sulfate is obtained after an evaporation and a concentration of the sodium sulfate solution.

### Claim 18 (depends on 9)

The method according to claim 9, wherein the solvent oil is a 230 #solvent oil or a 260 #solvent oil (sulfonated kerosene); the sodium sulfate solution is kept at a temperature of 308-323K, and an industrial grade sodium sulfate is obtained after an evaporation and a concentration of the sodium sulfate solution.