# US 2024/0266575 A1 · Fe-cr redox flow battery systems and methods for preparation of chromium-containing electrolyte therefor

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0266575 A1
- Document ID: US20240266575A1
- Status: Published application
- Kind: A1
- Application number: 18/638,415
- Filed: 2024-04-17
- Published: 2024-08-08
- Earliest claimed: 2020-11-16
- Assignees: Cougar Creek Technologies, LLC
- Applicants: Cougar Creek Technologies, LLC
- Inventors: Liyu Li; Qingtao Luo
- Web page: https://patentgrep.com/patent/US20240266575A1

## CPC

- H01M 8/188: {by recharging of redox couples containing fluids; Redox flow type batteries}
- C22C 1/00: Making non-ferrous alloys (by electrothermic methods C22B4/00; by electrolysis C25C1/24, C25C3/36)
- C22C 27/06: Alloys based on chromium
- H01M 4/38: of elements or alloys
- H01M 8/04186: of liquid-charged or electrolyte-charged reactants
- H01M 8/04201: {Reactant storage and supply, e.g. means for feeding, pipes}
- H01M 8/04276: Arrangements for managing the electrolyte stream, e.g. heat exchange
- H01M 8/04544: {Voltage}
- H01M 8/04611: {of the individual fuel cell}
- H01M 8/04932: {of the individual fuel cell}
- H01M 8/08: Fuel cells with aqueous electrolytes
- H01M 16/003: {of fuel cells with other electrochemical devices, e.g. capacitors, electrolysers}
- H01M 8/0693: {Treatment of the electrolyte residue, e.g. reconcentrating}
- H01M 2004/8694: {Bipolar electrodes}
- H01M 2300/0002: Aqueous electrolytes
- H01M 2300/0005: Acid electrolytes
- Y02E 60/10: Energy storage using batteries
- Y02E 60/50: Fuel cells
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C22C: ALLOYS (treatment of alloys C21D, C22F)
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A method for preparation of electrolyte for a redox flow battery includes reducing chromium ore using a carbon source to convert the chromium ore to an iron/chromium alloy with carbon particles; dissolving the iron/chromium alloy with carbon particles in sulfuric acid to form a first solution; adding calcium chloride or barium chloride to the first solution to produce a second solution including FeCl3 and CrCl3; and adding an acid to the second solution to form the electrolyte. Other methods can be used for preparing an electrolyte from chromium waste material.

## Claims

### Claim 1

A method for preparation of electrolyte for a redox flow battery, the method comprising:
dissolving chromium waste material in HCl or H2SO4 to generate an electrolyte comprising CrCl3 or Cr2(SO4)3 and at least one metal impurity, respectively;
reducing the at least one metal impurity in the electrolyte using an electrode of the redox flow battery to form particles of the at least one metal impurity;
collecting the particles of the at least one metal impurity; and
removing the collected particles using a cleaning solution.

### Claim 2 (depends on 1)

The method of claim 1, wherein collecting the particles comprises collecting at least a portion of the particles on an electrode of the redox flow battery system.

### Claim 3 (depends on 2)

The method of claim 2, wherein the electrode comprises interdigitated openings or indentations for collection of the particles.

### Claim 4 (depends on 1)

The method of claim 1, wherein the at least one metal impurity comprises at least one of nickel, antimony, bismuth, zinc, platinum, palladium, gold, or copper.

### Claim 5 (depends on 1)

The method of claim 1, wherein the cleaning solution comprises ferric ions.

### Claim 6 (depends on 1)

The method of claim 1, wherein the cleaning solution is at least a portion of a catholyte of the redox flow battery system.

### Claim 7 (depends on 1)

The method of claim 1, wherein the cleaning solution comprises hydrogen peroxide or ferric chloride.

### Claim 8 (depends on 1)

The method of claim 1, further comprising adding FeCl2, Fe+FeCl3, Fe(OH)2, or Fe+Fe(OH)3 to obtain a preselected ratio of FeCl3/CrCl3 in the electrolyte.

### Claim 9 (depends on 1)

The method of claim 1, wherein the chromium waste comprises Cr(OH)3.

### Claim 10

A method for hydrogen gas production, the method comprising:
providing a redox flow battery, comprising an anolyte comprising chromium ions in solution, a catholyte comprising iron ions in solution, a first half-cell comprising a first electrode in contact with the anolyte, a second half-cell comprising a second electrode in contact with the catholyte, and a first separator separating the first half-cell from the second half-cell;
coupling an electrolysis cell to the redox flow battery, the electrolysis cell comprising third and fourth electrodes and water;
discharging the redox flow battery into the electrolysis cell to produce hydrogen gas by electrolysis of the water in the electrolysis cell;
removing the hydrogen gas from the electrolysis cell; and
storing the hydrogen gas in a container.

### Claim 11 (depends on 10)

The method of claim 10, wherein at least a portion of the chromium ions form a chromium complex with at least one of the following: NH3, NH4+, CO(NH2)2, SCN−, or CS(NH2)2.

### Claim 12 (depends on 11)

The method of claim 11, wherein the chromium complex comprises a compound or ion having the formula [Cr3+(J)x(M)y(H2O)z]
wherein x, y, and z are non-negative integers with x+y+z=6 and x is at least 1,
J is selected from the group consisting of NH3, NH4+, CO(NH2)2, SCN−, or CS(NH2)2, and
each M is different from J and independently selected from the group consisting of Cl−, F−, Br−, I−, NH4+, NH3, ethylenediaminetetraacetic acid (EDTA), CN−, SCN−, S2−, O—NO2−, OH−, NO2−, CH3CN, C5H5N, NC5H4—C5H4N, C12H8N2, CO(NH2)2, CS(NH2)2, P(C6H5)3, —CO, CH3—CO—CH2—CO—CH3, NH2—CH2—CH2—NH2, NH2CH2COO−, O—SO22−, or P(o-tolyl)3.

### Claim 13 (depends on 12)

The method of claim 12, wherein J is NH3 or NH4+ and at least one M is CO(NH2)2.

### Claim 14 (depends on 12)

The method of claim 12, wherein the chromium complex further comprises at least one counterion selected from the ground consisting of ammonium, chloride, bromide, iodide, fluoride, sulfate, or nitrate.

### Claim 15 (depends on 10)

The method of claim 10, wherein the redox flow battery comprises a base having a first surface and a second surface opposite the first surface, the first electrode disposed on the first surface of the base, the second electrode disposed on the second surface of the base, and conductive elements that extend through the base, wherein the base resists flow of anolyte and catholyte through the base and each of the conductive elements comprises a first end portion exposed at the first surface of the base and a second end portion exposed at the second surface of the base, wherein the first electrode comprises the first end portions of the conductive elements and the second electrode comprises the second end portions of the conductive elements.

### Claim 16 (depends on 10)

The method of claim 10, wherein the redox flow battery further comprises a balance arrangement comprising
a balance electrolyte comprising vanadium ions in solution,
a third half-cell comprising a third electrode in contact with the anolyte or the catholyte,
a fourth half-cell comprising a fourth electrode in contact with the balance electrolyte, and
a reductant in the balance electrolyte or introducible to the balance electrolyte for reducing dioxovanadium ions.

### Claim 17 (depends on 16)

The method of claim 16, wherein the reductant is NH3, NH4+, CO(NH2)2, or CS(NH2)2.

### Claim 18 (depends on 16)

The method of claim 16, wherein the reductant is an organic compound.

### Claim 19 (depends on 10)

The method of claim 10, the method comprising:
intermittently, periodically, or continuously making a measurement of a value indicative of a state of charge of the anolyte or the catholyte before entering or after leaving the first half-cell or the second half-cell, respectively; and
generating a temporal energy profile of the anolyte or the catholyte, respectively, using the measurements.

### Claim 20 (depends on 19)

The method of claim 19, wherein the redox flow battery system further comprises an anolyte pump configured for pumping anolyte into and out of the first half-cell and a catholyte pump configured for pumping catholyte into or out of the second half-cell;
the method further comprising using the temporal energy profile to vary pumping speed of the anolyte pump and the catholyte pump.