# US 2024/0266494 A1 · Transfer laminate, method for manufacturing anode for lithium secondary battery, anode for lithium secondary battery, and lithium secondary battery comprising anode

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0266494 A1
- Document ID: US20240266494A1
- Status: Published application
- Kind: A1
- Application number: 18/294,415
- Filed: 2023-02-02
- Published: 2024-08-08
- Earliest claimed: 2022-02-09
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Mun Kyu JOO; ILHA LEE; Sarah KIM; Seoyoung JEON; Yohan KWON; Jonghyun CHAE
- Web page: https://patentgrep.com/patent/US20240266494A1

## CPC

- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/043: {involving compressing or compaction}
- B32B 37/025: {Transfer laminating}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/382: {Lithium (H01M4/405 takes precedence)}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- B32B 2307/538: Roughness
- B32B 2307/7376: Thickness
- B32B 2307/748: Releasability
- B32B 2309/02: Temperature
- B32B 2309/105: Thickness
- B32B 2309/12: Pressure
- B32B 2311/00: Metals, their alloys or their compounds
- B32B 2367/00: Polyesters, e.g. PET, i.e. polyethylene terephthalate
- B32B 2457/10: Batteries
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- B32B: LAYERED PRODUCTS, i.e. PRODUCTS BUILT-UP OF STRATA OF FLAT OR NON-FLAT, e.g. CELLULAR OR HONEYCOMB, FORM
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The present application relates to a transfer laminate, a negative electrode for a lithium secondary battery, a method for manufacturing a lithium secondary battery, and a lithium secondary battery.

## Claims

### Claim 1

A transfer laminate comprising:
a base layer;
a release layer on one or both surfaces of the base layer; and
a lithium metal layer on a surface of the release layer opposite to a surface of the release layer in contact with the base layer,
wherein a thickness of the release layer is 0.1 μm or greater and 10 μm less, and
wherein an average surface roughness (Sa) of the base layer is 50 nm or greater.

### Claim 2 (depends on 1)

The transfer laminate of claim 1, wherein the average surface roughness (Sa) of the base layer is smaller than the thickness of the release layer.

### Claim 3 (depends on 1)

The transfer laminate of claim 1, wherein a releasing force of a surface of the release layer in contact with the base layer is 100 gf/inch or less, and wherein a cross-cut test value of the surface of the release layer in contact with the base layer is 0 B to 1 B according to ASTM3359.

### Claim 4 (depends on 1)

The transfer laminate of claim 1, wherein a thickness of the lithium metal layer is 1 μm or greater and 10 μm or less.

### Claim 5 (depends on 1)

The transfer laminate of claim 1, wherein a thickness of the base layer is 1 μm or greater and 300 μm or less.

### Claim 6 (depends on 1)

The transfer laminate of claim 1, wherein the base layer is comprises one or more selected from the group consisting of polyethylene terephthalate (PET), polyethylenenaphtalate (PEN), polyimide (PI), poly(methylmethacrylate)(PMMA), polypropylene, polyethylene and polycarbonate.

### Claim 7 (depends on 1)

A manufacturing method of a negative electrode for a lithium secondary battery, the manufacturing method comprising:
providing a negative electrode for the lithium secondary battery comprising a negative electrode current collector layer and a negative electrode active material layer on one surface or both surfaces of the negative electrode current collector layer;
transferring a lithium metal layer by laminating the transfer laminate of claim 1 onto a surface of the negative electrode active material layer opposite to a surface in contact with the negative electrode current collector layer; and
pre-lithiating the negative electrode active material layer.

### Claim 8 (depends on 7)

The manufacturing method of claim 7, wherein the transferring of the lithium metal layer by laminating the transfer laminate onto the surface of the negative electrode active material layer opposite to the surface in contact with the negative electrode current collector layer comprises laminating the transfer laminate such that a surface of the lithium metal layer opposite to a surface in contact with the release layer comes into contact with the surface of the negative electrode active material layer opposite to the surface in contact with the negative electrode current collector layer, and removing the base layer.

### Claim 9 (depends on 7)

The manufacturing method of claim 7, wherein the laminating is performed under a pressurization condition of 20 kgf/cm to 60 kgf/cm at a temperature condition of 20° C. to 80° C.

### Claim 10 (depends on 7)

The manufacturing method of claim 7, wherein in the pre-lithiating of the negative electrode active material layer, the negative electrode active material layer is pre-lithiated within 30 minutes to 48 hours after transferring the lithium metal layer.

### Claim 11 (depends on 7)

A negative electrode for a lithium secondary battery manufactured by the manufacturing method of a negative electrode for a lithium secondary battery of claim 7.

### Claim 12 (depends on 11)

A lithium secondary battery comprising:
a positive electrode;
the negative electrode for a lithium secondary battery of claim 11;
a separator between the positive electrode and the negative electrode; and
an electrolyte.

### Claim 13 (depends on 2)

The transfer laminate of claim 2, wherein the average surface roughness (Sa) of the base layer is 50 nm or greater and 0.1 μm or less.

### Claim 14 (depends on 2)

The transfer laminate of claim 2, wherein the average surface roughness (Sa) of the base layer is 55 nm or greater and 90 nm or less.

### Claim 15 (depends on 1)

The transfer laminate of claim 1, wherein the release layer comprises one or more selected from the group consisting of silicon-modified polyester in which a silicon chain is graft-linked to a polyester main chain; an acryl resin; Si; melamine; and fluorine.

### Claim 16 (depends on 1)

The transfer laminate of claim 1, wherein a releasing force of the surface of the release layer in contact with the base layer satisfies a range of 10 gf/inch or greater and 30 gf/inch or less.