# US 2024/0263339 A1 · Method for Manufacturing a Component by Means of Layered Construction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0263339 A1
- Document ID: US20240263339A1
- Status: Published application
- Kind: A1
- Application number: 18/567,198
- Filed: 2022-06-02
- Published: 2024-08-08
- Earliest claimed: 2021-06-07
- Assignees: Friedrich-Alexander-Universität Erlangen-Nürnberg
- Applicants: Friedrich-Alexander-Universität Erlangen-Nürnberg
- Inventors: Carolin Körner; Julian Pistor
- Web page: https://patentgrep.com/patent/US20240263339A1

## CPC

- C30B 13/06: the molten zone not extending over the whole cross-section
- B22F 10/25: Direct deposition of metal particles, e.g. direct metal deposition [DMD] or laser engineered net shaping [LENS]
- B22F 10/28: Powder bed fusion, e.g. selective laser melting [SLM] or electron beam melting [EBM]
- B22F 10/36: of energy beam parameters
- B22F 10/364: for post-heating, e.g. remelting
- B22F 10/38: to achieve specific product aspects, e.g. surface smoothness, density, porosity or hollow structures
- B22F 12/13: to preheat the material
- B22F 12/44: characterised by the configuration of the radiation means
- B22F 12/45: Two or more
- B23K 26/0006: {taking account of the properties of the material involved (B23K26/32, B23K26/40 take precedence)}
- B23K 26/0732: {into a rectangular shape}
- B23K 26/0738: {into a linear shape}
- B23K 26/342: Build-up welding
- B23P 6/007: {using only additive methods, e.g. build-up welding}
- B33Y 10/00: Processes of additive manufacturing
- B33Y 80/00: Products made by additive manufacturing
- C30B 11/003: {Heating or cooling of the melt or the crystallised material}
- C30B 11/005: {by irradiation or electric discharge}
- C30B 13/22: by irradiation or electric discharge
- C30B 13/24: using electromagnetic waves
- C30B 29/52: Alloys
- B22F 2998/10: Processes characterised by the sequence of their steps
- B22F 2999/00: Aspects linked to processes or compositions used in powder metallurgy
- B23K 2103/12: Copper or alloys thereof
- B23K 2103/26: {Alloys of Nickel and Cobalt and Chromium}
- C22C 2200/00: Crystalline structure
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR
- B22F: WORKING METALLIC POWDER; MANUFACTURE OF ARTICLES FROM METALLIC POWDER; MAKING METALLIC POWDER (making alloys by powder metallurgy C22C); APPARATUS OR DEVICES SPECIALLY ADAPTED FOR METALLIC POWDER
- B23K: SOLDERING OR UNSOLDERING; WELDING; CLADDING OR PLATING BY SOLDERING OR WELDING; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING; WORKING BY LASER BEAM
- B23P: METAL-WORKING NOT OTHERWISE PROVIDED FOR; COMBINED OPERATIONS; UNIVERSAL MACHINE TOOLS (arrangements for copying or controlling B23Q)
- B33Y: ADDITIVE MANUFACTURING, i.e. MANUFACTURING OF THREE-DIMENSIONAL [3D] OBJECTS BY ADDITIVE DEPOSITION, ADDITIVE AGGLOMERATION OR ADDITIVE LAYERING, e.g. BY 3D PRINTING, STEREOLITHOGRAPHY OR SELECTIVE LASER SINTERING
- C22C: ALLOYS (treatment of alloys C21D, C22F)

## Abstract

The invention relates to a method for producing a component by means of layered construction, by combining a plurality of crystallites of a metallic material to form a single crystal. The single crystal is formed by thermomechanically activated successive anisotropic plastic deformation. The metallic material is heated during the construction of a new layer, with the result that the metallic material is melted in a linear region. The linear region is moved in order to construct the new layer.

## Claims

### Claim 1

A method for producing a component (1) by means of layered construction, comprising combining a plurality of crystallites of a metallic material to form a single crystal, wherein the single crystal is formed by thermomechanically activated successive anisotropic plastic deformation, wherein the metallic material is heated during the construction of a new layer, with the result that the metallic material is melted in a linear region,
wherein mechanical stresses occur during melting and subsequent cooling, in particular solidification, of the metallic material, wherein the plastic deformation of the metallic material is caused by these mechanical stresses,
wherein the mechanical stresses have a preferred direction because of the linear design of the melted linear region, whereby the anisotropic plastic deformation results, and
wherein the new layer is gradually constructed by being traversed by the melted linear region, wherein the component is constructed layer by layer in a construction direction,
wherein the linear region has a length (L) along its extension direction and a width (B) and a depth (D) which are both perpendicular to the extension direction of the linear region, wherein the ratio of length (L) and width (B) is at least 5:1, wherein the ratio of width (B) and depth (D) lies in a range of from 1:2 to 10:1, wherein the linear region is moved in order to construct the new layer, and
wherein the linear region is subjected to a lateral movement perpendicular to its extension direction with a lateral speed vlat while maintaining its extension direction.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the ratio of length (L) and width (B) is at least 20:1.

### Claim 3 (depends on 1)

The method according to claim 1, wherein the ratio of width (B) and depth (D) lies in a range of from 2:1 to 4:1.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the depth (D) of the linear region is in the range from 50 μm to 1000 μm.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the component is produced layer by layer by at least one of local melting of a powder layer of the metallic material or local application of the metallic material.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the metallic material in the linear region is melted by at least one of a laser or an electron beam.

### Claim 7 (depends on 1)

The method according to claim 1, wherein the component or an installation space containing the component is additionally heated.

### Claim 8 (depends on 1)

The method according to claim 1, wherein at least one of the metallic material, the component or the installation space is heated to a temperature (T) in the range of from 300° ° C. to 1200° C.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the layered construction is effected along a construction direction (4) and layers with thicknesses in the range of between 10 μm and 500 μm are generated.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the metallic material is formed of at least one of a nickel-based alloy, a nickel-titanium alloy or a copper alloy.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the lateral speed vlat is between 0.1 mm/s and 100 mm/s.

### Claim 12 (depends on 11)

The method according to claim 11, wherein a crystal orientation of the single crystal is adjusted in a defined manner by adjustment of extension direction and lateral movement of the linear region in successive layers.

### Claim 13 (depends on 1)

The method according to claim 1, wherein the extension direction of the linear region in successive layers is the same or is rotated by an angle corresponding to a rotational symmetry of the crystal lattice.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the direction of the lateral movement of the linear region in successive layers is the same or is rotated by an angle corresponding to a rotational symmetry of the crystal lattice.

### Claim 15 (depends on 1)

The method according to claim 1, wherein the extension direction and the direction of the lateral movement of the linear region in successive layers, or in each case after a particular number of layers, are rotated by an equal angle value.

### Claim 16 (depends on 1)

The method according to claim 1, further comprising at least one of the following:
varying the extension direction of the linear region during the construction of the new layer,
varying the lateral movement of the linear region during the construction of the new layer,
varying
the extension direction of the linear region in the construction direction, or
varying the lateral movement of the linear region in the construction direction.

### Claim 17 (depends on 1)

The method according to claim 1, wherein a linear region is melted only in subregions of the component.

### Claim 18 (depends on 1)

The method according to claim 1, wherein monocrystalline and polycrystalline regions are produced in the component.

### Claim 19 (depends on 1)

The method according to claim 1, wherein a continuous change in the crystal orientation is produced in the component.

### Claim 20

A component comprising a single crystal with exactly adjusted primary and secondary crystal orientation, produced by a means of layered construction, comprising combining a plurality of crystallites of a metallic material to form a single crystal, wherein the single crystal is formed by thermomechanically activated successive anisotropic plastic deformation, wherein the metallic material is heated during the construction of a new layer, with the result that the metallic material is melted in a linear region,
wherein mechanical stresses occur during melting and subsequent cooling, in particular solidification, of the metallic material, wherein the plastic deformation of the metallic material is caused by these mechanical stresses,
wherein the mechanical stresses have a preferred direction because of the linear design of the melted linear region, whereby the anisotropic plastic deformation results, and
wherein the new layer is gradually constructed by being traversed by the melted linear region, wherein the component is constructed layer by layer in a construction direction,
wherein the linear region has a length (L) along its extension direction and a width (B) and a depth (D) which are both perpendicular to the extension direction of the linear region, wherein the ratio of length (L) and width (B) is at least 5:1, wherein the ratio of width (B) and depth (D) lies in a range of from 1:2 to 10:1, wherein the linear region is moved in order to construct the new layer, and wherein the linear region is subjected to a lateral movement perpendicular to its extension direction with a lateral speed vlat while maintaining its extension direction.