# US 2024/0258597 A1 · Energy-efficient pyrometallurgical process for treating li-ion batteries

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0258597 A1
- Document ID: US20240258597A1
- Status: Published application
- Kind: A1
- Application number: 18/561,016
- Filed: 2022-05-24
- Published: 2024-08-01
- Earliest claimed: 2021-05-26
- Assignees: Umicore AG & Co. KG
- Applicants: Umicore
- Inventors: Lennart SCHEUNIS
- Web page: https://patentgrep.com/patent/US20240258597A1

## CPC

- C22B 23/02: by dry processes
- C21C 7/076: Use of slags or fluxes as treating agents (C21C7/06, C21C7/064, C21C7/068 take precedence)
- C22B 1/005: {Preliminary treatment of scrap (C22B1/02 - C22B1/26 take precedence)}
- C22B 7/001: {Dry processes}
- C22B 7/004: {separating two or more metals by melting out (liquation), i.e. heating above the temperature of the lower melting metal component(s); by fractional crystallisation (controlled freezing)}
- C22B 7/04: Working-up slag
- C22B 23/021: {by reduction in solid state, e.g. by segregation processes}
- C22B 23/026: {from spent catalysts}
- C22B 23/028: {separation of nickel from cobalt}
- C22B 23/06: Refining
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 10/54: Reclaiming serviceable parts of waste accumulators
- Y02P 10/20: Recycling
- Y02W 30/84: Recycling of batteries or fuel cells
- C22B: PRODUCTION AND REFINING OF METALS (electrolytic C25); PRETREATMENT OF RAW MATERIALS
- C21C: PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OF WROUGHT-IRON OR STEEL; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present disclosure concerns a 2-step smelting process, for recovering of Ni and Co from batteries and other sources. The process comprises the steps of: defining an oxidizing level Ox, and a battery-bearing metallurgical charge; oxidizing smelting of the metallurgical charge by injecting an O2-bearing gas into the melt to reach the defined oxidizing level Ox; and, reducing smelting of the obtained slag using a heat source and a reducing agent. The process is more energy-efficient than a single-step reducing smelting process and provides for a higher purity alloy and for a cleaner final slag.

## Claims

### Claim at position 1

1-12. (canceled)

### Claim 13

Process for the recovery of valuable metals from a metallurgical charge comprising slag formers, and Li-ion batteries or their derived products containing Co, Ni, metallic Al, and C, comprising the steps of:
providing a metallurgical smelting furnace equipped with means for the submerged injection of an O2-bearing gas;
defining an oxidizing level Ox characterizing oxidizing smelting conditions according to the formula:
Ox
=
p
⁢
CO
2
/
(
p
⁢
CO
+
p
⁢
CO
2
)
,
wherein 0.1<Ox<1, pCO and pCO2 are the partial pressures of CO and CO2 in contact with the melt;
preparing the metallurgical charge comprising a weight fraction Bf of Li-ion batteries or their derived products, according to the formula:
1
>
Bf
>
0
,
3
/
(
(
1
+
3.5
*
Ox
)
*
C
)
+
2.5
*
Al
)
,
wherein Ox is the oxidizing level, and Al and C are the weight fractions of respectively metallic Al and C in said batteries or their derived products;
oxidizing smelting the metallurgical charge by injecting an O2-bearing gas into the melt to reach the defined oxidizing level Ox, thereby obtaining a first alloy with a major part of Ni, and a first slag containing residual Ni and Co;
liquid/liquid separation of the first alloy from the first slag; and
reducing smelting of the first slag using a heat source and a reducing agent, maintaining a reduction potential ensuring the reduction of Co and Ni, thereby producing a second alloy, and a second slag containing less than 1% by weight of Ni.

### Claim 14

Process for the recovery of valuable metals from a metallurgical charge comprising slag formers, and Li-ion batteries or their derived products containing Co, Ni, metallic Al, and C, comprising the steps of:
providing a metallurgical smelting furnace equipped with means for the submerged injection of an O2-bearing gas;
preparing the metallurgical charge using a weight fraction Bf of Li-ion batteries or their derived products in the metallurgical charge;
defining an oxidizing level Ox characterizing oxidizing smelting conditions according to the formula:
Ox
=
p
⁢
CO
2
/
(
p
⁢
CO
+
p
⁢
CO
2
)
>
(
(
(
0.3
/
Bf
-
2.5
*
Al
)
/
C
)
-
1
)
/
3
.
5
,
wherein 0.1<Ox<1, pCO and pCO2 are the partial pressures of CO and CO2 in contact with the melt, and Al and C are the weight fractions of respectively metallic Al and C in said batteries or their derived products;
oxidizing smelting the metallurgical charge by injecting an O2-bearing gas into the melt to reach the defined oxidizing level Ox, thereby obtaining a first alloy with a major part of Ni, and a first slag containing residual Ni and Co;
liquid/liquid separation of the first alloy from the first slag; and,
reducing smelting of the first slag using a heat source and a reducing agent, maintaining a reduction potential ensuring the reduction of Co and Ni, thereby producing a second alloy, and a second slag containing less than 1% by weight of Ni.

### Claim 15 (depends on 13)

Process according to claim 13, wherein the step of oxidizing smelting is autogenous.

### Claim 16 (depends on 13)

Process according to claim 13, wherein the first slag is maintained in the liquid state between the steps of liquid/liquid separation and the step of reducing smelting.

### Claim 17 (depends on 13)

Process according to claim 13, wherein the O2-bearing gas is enriched air or pure O2.

### Claim 18 (depends on 13)

Process according to claim 13, wherein Ox<0.98.

### Claim 19 (depends on 13)

Process according to claim 13, wherein said slag formers comprise, by weight, up to 50% CaO, up to 55% Al2O3, and up to 65% SiO2.

### Claim 20 (depends on 13)

Process according to claim 13, further comprising a step of transferring the separated first slag to a second furnace suitable for performing a step of reducing smelting, thereby obtaining a second Ni and Co-bearing alloy, and a depleted second slag.

### Claim 21 (depends on 20)

Process according to claim 20, wherein said second furnace is an electric furnace.

### Claim 22 (depends on 13)

Process according to claim 13, further comprising a step of liquid/liquid separation of the second alloy from the second slag.

### Claim 23 (depends on 22)

Process according to claim 22, further comprising a step of recirculating the separated second alloy to the step of autogenous smelting.

### Claim 24 (depends on 13)

Process according to claim 13, further comprising the steps of:
atomizing the first alloy; and,
dissolving the atomized alloy in acidic conditions, thereby obtaining a metal-bearing solution suitable for further hydrometallurgical refining.