# US 2024/0258512 A1 · Anode for lithium secondary battery, method for manufacturing lithium secondary battery, and lithium secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0258512 A1
- Document ID: US20240258512A1
- Status: Published application
- Kind: A1
- Application number: 18/561,099
- Filed: 2022-11-22
- Published: 2024-08-01
- Earliest claimed: 2021-11-29
- Assignees: LG Energy Solution, Ltd.
- Applicants: LG Energy Solution, Ltd.
- Inventors: Seoyoung JEON; Sarah KIM; ILHA LEE; Mun Kyu JOO; Yohan KWON; Jonghyun CHAE
- Web page: https://patentgrep.com/patent/US20240258512A1

## CPC

- H01M 4/131: Electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/386: {Silicon or alloys based on silicon}
- H01M 4/0404: {by coating on electrode collectors}
- H01M 4/044: {Activating, forming or electrochemical attack of the supporting material}
- H01M 4/134: Electrodes based on metals, Si or alloys
- H01M 4/1391: of electrodes based on mixed oxides or hydroxides, or on mixtures of oxides or hydroxides, e.g. LiCoOx
- H01M 4/1395: of electrodes based on metals, Si or alloys
- H01M 4/366: {as layered products}
- H01M 4/48: of inorganic oxides or hydroxides
- H01M 10/049: {Processes for forming or storing electrodes in the battery container}
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- H01M 50/609: Arrangements or processes for filling with liquid, e.g. electrolytes
- H01M 10/0569: characterised by the solvents
- H01M 50/105: Pouches or flexible bags
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- Y02P 70/50: Manufacturing or production processes characterised by the final manufactured product
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A negative electrode for a lithium secondary battery, a method for manufacturing a lithium secondary battery, and a lithium secondary battery are disclosed. The negative electrode includes a negative electrode current collector; a negative electrode active material layer on one surface or both surfaces of the current collector; and an electrolyte solution dissolution layer on a surface of the negative electrode active material layer opposite to a surface of the negative electrode active material layer facing the negative electrode current collector layer. The electrolyte solution dissolution layer has a thickness of 0.1 μm or more and 5 μm or less. The electrolyte solution dissolution layer comprises a binder copolymer comprising a monomer unit comprising a fluoro group, and the monomer unit is present in an amount of 5 parts by weight or more and 20 parts by weight or less based on 100 parts by weight of the binder copolymer.

## Claims

### Claim 1

A negative electrode for a lithium secondary battery, comprising:
a negative electrode current collector layer;
a negative electrode active material layer on one surface or both surfaces of the negative electrode current collector layer; and
an electrolyte solution dissolution layer on a surface of the negative electrode active material layer opposite to a surface of the negative electrode active material layer brought into contact with facing the negative electrode current collector layer,
wherein the electrolyte solution dissolution layer has a thickness of 0.1 μm or more and 5 μm or less, and
wherein the electrolyte solution dissolution layer comprises a binder copolymer comprising a monomer unit comprising a fluoro group, and wherein the monomer unit is present in an amount of 5 parts by weight or more and 20 parts by weight or less based on 100 parts by weight of the binder copolymer.

### Claim 2 (depends on 1)

The negative electrode of claim 1, wherein the monomer unit comprises a perfluoro olefin.

### Claim 3 (depends on 1)

The negative electrode of claim 1, wherein the electrolyte solution dissolution layer further comprises an acrylic polymer, and wherein the binder copolymer is present in an amount of 1 part by weight or more and 20 parts by weight or less based on 100 parts by weight of the electrolyte solution dissolution layer.

### Claim 4 (depends on 1)

The negative electrode of claim 1, wherein the negative electrode active material layer comprises: a silicon-containing active material; a negative electrode conductive material; and a negative electrode binder, and
wherein the silicon-containing active material comprises one or more selected from the group consisting of SiOx, wherein x=0, SiOx, wherein 0<x<2, SiC, a metal impurity, and a Si alloy.

### Claim 5 (depends on 4)

The negative electrode of claim 4, wherein the silicon-based silicon-containing active material comprises one or more selected from the group consisting of SiOx, wherein x=0, and SiOx, wherein 0<x<2, and comprises 70 parts by weight or more of the SiOx, wherein x=0, based on 100 parts by weight of the silicon based silicon-containing active material.

### Claim 6 (depends on 1)

The negative electrode of claim 1, wherein the negative electrode current collector layer has a thickness of 1 μm or more and 100 μm or less, and
wherein the negative electrode active material layer has a thickness of 20 μm or more and 500 μm or less.

### Claim 7

A method for manufacturing a lithium secondary battery, the method comprising:
forming a negative electrode current collector layer and a negative electrode active material layer on one surface or both surfaces of the negative electrode current collector layer;
forming an electrolyte solution dissolution layer by coating a surface of the negative electrode active material layer opposite to a surface of the negative electrode active material layer facing the negative electrode current collector layer with an electrolyte solution dissolution layer composition to form a negative electrode for the lithium secondary battery;
transferring lithium metal to a surface of the electrolyte solution dissolution layer opposite to a surface of the electrolyte solution dissolution layer facing the negative electrode active material layer;
forming a positive electrode current collector layer and a positive electrode active material layer on one surface or both surfaces of the positive electrode current collector layer to form a positive electrode for a lithium secondary battery;
laminating a separator between the negative electrode and the positive electrode and placing the resulting laminate in a battery pouch; and
pre-lithiating the negative electrode by introducing an electrolyte solution into the battery pouch.

### Claim 8 (depends on 7)

The method of claim 7, wherein the pre-lithiating of the negative electrode by introducing the electrolyte solution into the battery pouch is performed under a pressurized condition of 5 kgf/cm2 to 20 kgf/cm2 under a temperature condition of 60° C. to 80° C.

### Claim 9 (depends on 7)

The method of claim 7, wherein a time of completing the pre-lithiation in the pre-lithiating of the negative electrode by introducing the electrolyte solution into the battery pouch is 6 hours and more and 24 hours or less.

### Claim 10 (depends on 7)

The method of claim 7, wherein the transferring of the lithium metal to the surface of the electrolyte solution dissolution layer opposite to the surface of the electrolyte solution dissolution layer facing the negative electrode active material layer comprises preparing a transfer laminate comprising a substrate layer and lithium metal provided on the substrate layer;
laminating the transfer laminate on the electrolyte solution dissolution layer wherein a surface opposite to a surface of the lithium metal facing the substrate layer faces a surface opposite to a surface of the electrolyte solution dissolution layer facing the negative electrode active material layer; and
removing the substrate layer.

### Claim 11 (depends on 10)

The method of claim 10, wherein a release layer is formed on the surface of the transfer laminate with which the substrate layer and the lithium metal are brought into contact.

### Claim 12 (depends on 7)

The method of claim 7, wherein the lithium metal has a thickness of 1 μm or more and 10 μm or less.

### Claim 13 (depends on 7)

A lithium secondary battery manufactured by the method according to claim 7.