# US 2024/0258452 A1 · Systems and Methods for Epitaxy-Free Thin-Film Solar Cells

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0258452 A1
- Document ID: US20240258452A1
- Status: Published application
- Kind: A1
- Application number: 18/424,598
- Filed: 2024-01-26
- Published: 2024-08-01
- Earliest claimed: 2023-01-27
- Assignees: California Institute of Technology
- Applicants: California Institute of Technology
- Inventors: Phillip R. Jahelka; Andrew W. Nyholm; Harry A. Atwater
- Web page: https://patentgrep.com/patent/US20240258452A1

## CPC

- H10F 71/139: {using temporary substrates}
- H10F 71/1395: {for thin-film devices}
- H10F 10/144: comprising only Group III-V materials, e.g. GaAs,AlGaAs, or InP photovoltaic cells
- H10F 77/169: Thin semiconductor films on metallic or insulating substrates
- H10F 71/127: {The active layers comprising only Group III-V materials, e.g. GaAs or InP}
- H10F 77/1243: {characterised by the dopants}
- H10F 77/211: {for photovoltaic cells}
- Y02E 10/544: Solar cells from Group III-V materials
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Systems and methods for epitaxy-free thin-film solar cells are described. The thin-film solar cells can be fabricated with low cost epitaxy-free processes. The solar cells have high efficiency and are lightweight. These properties make the solar cells desired for space based solar cell applications.

## Claims

### Claim 1

A method for fabricating a semiconductor device comprising:
forming a semiconductor layer on a semiconductor substrate via a diffusion doping process, wherein the semiconductor layer and the semiconductor substrate forms a p-n junction;
depositing a stress film on the semiconductor layer;
exfoliating a thin film by applying a pulling force to the stress film, wherein the thin film comprises the semiconductor layer and at least a portion of the semiconductor substrate;
depositing at least one electrode on the thin film to form an ohmic contact; and
etching a portion of the exfoliated thin film while preserving the stress film and the at least one electrode to form a semiconductor device.

### Claim 2 (depends on 1)

The method of claim 1, wherein the semiconductor substrate comprises a material selected from the group consisting of: silicon, germanium, a III-V semiconductor, GaAs, GaP, InP, AlGaAs, GaInP, and GaAsP.

### Claim 3 (depends on 1)

The method of claim 1, wherein the semiconductor substrate has a (110) orientation.

### Claim 4 (depends on 1)

The method of claim 1, wherein the semiconductor substrate comprises an n-type semiconductor, and the semiconductor layer comprises a p-type semiconductor.

### Claim 5 (depends on 1)

The method of claim 1, wherein the semiconductor substrate comprises a p-type semiconductor, and the semiconductor layer comprises an n-type semiconductor.

### Claim 6 (depends on 1)

The method of claim 1, wherein the stress film comprises a metallic material selected from the group consisting of: nickel, chromium, and germanium.

### Claim 7 (depends on 1)

The method of claim 1, wherein the thin film has a thickness less than or equal to 5 μm.

### Claim 8 (depends on 1)

The method of claim 1, further comprising applying an adhesive tape to the stress film and pulling the adhesive tape to exfoliate the thin film.

### Claim 9 (depends on 8)

The method of claim 8, wherein the adhesive tape comprises an acrylic glue or a silicone glue.

### Claim 10 (depends on 1)

The method of claim 1, wherein the semiconductor substrate has a doping concentration less than or equal to 5×1017 cm−3; wherein the semiconductor layer has a doping concentration less than or equal to 5×1017 cm−3.

### Claim 11 (depends on 1)

The method of claim 1, wherein the at least one electrode comprises a plurality of metal layers.

### Claim 12 (depends on 11)

The method of claim 11, wherein the at least one electrode comprises at least one of: palladium, germanium, silver, indium, copper, tin, and gold.

### Claim 13 (depends on 1)

The method of claim 1, wherein the diffusion doping process uses a sealed container with an inert gas; wherein the container comprises a refractory material.

### Claim 14 (depends on 1)

The method of claim 1, further comprising annealing the at least one electrode to a temperature less than or equal to 200° C. to form the ohmic contact.

### Claim 15 (depends on 1)

The method of claim 1, wherein the semiconductor substrate comprises n-GaAs, and the semiconductor layer comprises p-GaAs; wherein the diffusion doping processes uses a material comprising Zn as a dopant; wherein the stress film comprises nickel; wherein the at least one electrode comprises palladium, germanium, and gold.

### Claim 16 (depends on 15)

The method of claim 15, wherein the etching step uses an etch solution comprising hydrogen peroxide and alkali hydroxide.

### Claim 17 (depends on 15)

The method of claim 15, wherein the semiconductor device has an open circuit potential of at least 850 mV.

### Claim 18 (depends on 8)

The method of claim 8, further comprising applying a second adhesive tape to the at least one electrode; removing the adhesive tape; and removing the stress film; and depositing a second set of electrodes onto the thin film.

### Claim 19

A solar cell comprising:
an n-gallium arsenide (GaAs) substrate with a (110) orientation;
a p-GaAs layer forming a junction with the n-GaAs substrate, wherein a thickness of the n-GaAs substrate and the p-GaAs layer is less than or equal to 5 μm;
a plurality of electrodes deposited on the n-GaAs substrate, wherein each of the plurality of electrodes comprises a plurality of metal layers; and
at least one electrode deposited on the p-GaAs layer.

### Claim 20 (depends on 19)

The solar cell of claim 19, wherein the n-GaAs substrate has a doping concentration less than or equal to 5×1017 cm−3, and the p-GaAs layer has a doping concentration less than or equal to 5×1017 cm−3; wherein the plurality of electrodes comprises at least one of: palladium, germanium, silver, indium, copper, tin, and gold; wherein the at least one electrode comprises at least one of: nickel, germanium, and chromium.

### Claim 21

A solar cell comprising:
an n-gallium arsenide (GaAs) substrate with a (110) orientation;
a p-GaAs layer forming a junction with the n-GaAs substrate, wherein a thickness of the n-GaAs substrate and the p-GaAs layer is less than or equal to 5 μm;
a first set of electrodes deposited on the n-GaAs substrate, wherein each of the first set of electrodes comprises a plurality of metal layers; and
a second electrode deposited on the p-GaAs layer.

### Claim 22 (depends on 21)

The solar cell of claim 21, wherein the n-GaAs substrate has a doping concentration less than or equal to 5×1017 cm−3, and the p-GaAs layer has a doping concentration less than or equal to 5×1017 cm−3; wherein the first set of electrodes comprises at least one of: palladium, germanium, silver, indium, copper, tin, and gold; wherein the second electrode comprises at least one of: gold, indium, and silver.