# US 2024/0254392 A1 · Greenhouse gas emission reduction method for heavy metal contaminated soil

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0254392 A1
- Document ID: US20240254392A1
- Status: Published application
- Kind: A1
- Application number: 18/632,384
- Filed: 2024-04-11
- Published: 2024-08-01
- Earliest claimed: 2021-10-14
- Assignees: Jiangxi Agricultural University
- Applicants: Jiangxi Agricultural University
- Inventors: Ling Zhang; Yu Gao; Baihui Wang; Jian Bai; Aixin Li; Laicong Luo; Xiaoqin Lai
- Web page: https://patentgrep.com/patent/US20240254392A1

## CPC

- C09K 17/06: Calcium compounds, e.g. lime
- B01J 20/048: {containing phosphorus, e.g. phosphates, apatites, hydroxyapatites}
- B09C 1/08: chemically
- C01B 25/32: Phosphates of magnesium, calcium, strontium, or barium
- Y02C 20/10: of nitrous oxide (N2O)
- C09K: MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FOR ELSEWHERE
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- B09C: RECLAMATION OF CONTAMINATED SOIL (gatherers for removing stone or the like from the soil A01B43/00; sterilising soil by steam A01G11/00; removing undesirable matter, e.g. rubbish, from the land E01H15/00)
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- Y02C: CAPTURE, STORAGE, SEQUESTRATION OR DISPOSAL OF GREENHOUSE GASES [GHG]

## Abstract

The present disclosure provides a greenhouse gas emission reduction method for a heavy metal contaminated soil, falling within the technical field of emission reduction of greenhouse gas nitrous oxide. Specifically, hydroxyapatite (HAP) is added to a soil to effectively reduce the emission of nitrous oxide in the soil, and at the same time, the treatment of heavy metal contamination is realized, which is very suitable for the promotion and use of nitrous oxide emission reduction in the contaminated soil.

## Claims

### Claim 1

A greenhouse gas emission reduction method for a soil, hydroxyapatite (HAP) being used to reduce the emission of a nitrogen-containing gas in a soil, the nitrogen-containing gas being nitrous oxide, and an amount of HAP being 1-5% of a mass of a dry soil.

### Claim 2 (depends on 1)

The greenhouse gas emission reduction method for a soil according to claim 1, wherein the soil is a heavy metal contaminated soil.

### Claim 3 (depends on 1)

The greenhouse gas emission reduction method for a soil according to claim 1, wherein HAP is prepared by a sol-gel method using calcium nitrate and phosphoric acid as raw materials.

### Claim 4 (depends on 3)

The greenhouse gas emission reduction method for a soil according to claim 3, wherein a preparation method for HAP comprises the steps of: mixing a calcium nitrate solution with a phosphoric acid solution, adding aqueous ammonia at 40-50° C. to adjust a pH to 9-11, and continuing to react 30-50 min, followed by ageing to obtain a colloid; washing the colloid with water, followed by performing suction filtering to obtain a filter cake; and drying the filter cake, calcining the dried filter cake, and continuing to grind and sieve the calcined filter cake to prepare HAP.