# US 2024/0254038 A1 · Glass substrate, manufacturing method therefor, and electronic device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0254038 A1
- Document ID: US20240254038A1
- Status: Published application
- Kind: A1
- Application number: 18/633,479
- Filed: 2024-04-11
- Published: 2024-08-01
- Earliest claimed: 2021-10-12
- Assignees: BYD Company Limited
- Applicants: BYD Company Limited
- Inventors: Jingna CUI; Jiaxin ZHANG; Yulei PEI; Shuang WU; Qiying GAI
- Web page: https://patentgrep.com/patent/US20240254038A1

## CPC

- C03C 21/002: {to perform ion-exchange between alkali ions (C03C21/005 takes precedence)}
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

A glass substrate and a method for preparing the same, and an electronic device are provided. Two opposite sides of the glass substrate respectively have a first surface compressive stress layer and a second surface compressive stress layer. A surface compressive stress of the first surface compressive stress layer is greater than a surface compressive stress of the second surface compressive stress layer, and a depth of the first surface compressive stress layer is less than a depth of the second surface compressive stress layer.

## Claims

### Claim 1

A glass substrate, comprising:
a first surface compressive stress layer and a second surface compressive stress layer respectively disposed on two opposite sides of the glass substrate, a surface compressive stress of the first surface compressive stress layer being greater than a surface compressive stress of the second surface compressive stress layer; and a depth of the first surface compressive stress layer being less than a depth of the second surface compressive stress layer.

### Claim 2 (depends on 1)

The glass substrate according to claim 1, wherein a ratio of an absolute value of a difference between a compressive stress integral of the first surface compressive stress layer and a compressive stress integral of the second surface compressive stress layer to the compressive stress integral of any surface compressive stress layer is less than or equal to 5%.

### Claim 3 (depends on 2)

The glass substrate according to claim 2, wherein:
when the compressive stress integral of the first surface compressive stress layer obtained is equal to the compressive stress integral of the second surface compressive stress layer, the ratio of the absolute value of the difference between the compressive stress integral of the first surface compressive stress layer and the compressive stress integral of the second surface compressive stress layer to the compressive stress integral of the first surface compressive stress layer or the compressive stress integral of the second surface compressive stress layer is less than or equal to 5%;
when the compressive stress integral of the first surface compressive stress layer obtained is greater than the compressive stress integral of the second surface compressive stress layer, the ratio of the absolute value of the difference between the compressive stress integral of the first surface compressive stress layer and the compressive stress integral of the second surface compressive stress layer to the compressive stress integral of the second surface compressive stress layer is less than or equal to 5%; and
when the compressive stress integral of the first surface compressive stress layer obtained is less than the compressive stress integral of the second surface compressive stress layer, the ratio of the absolute value of the difference between the compressive stress integral of the first surface compressive stress layer and the compressive stress integral of the second surface compressive stress layer to the compressive stress integral of the first surface compressive stress layer is less than or equal to 5%.

### Claim 4 (depends on 1)

The glass substrate according to claim 1, wherein a surface compressive stress of the first surface compressive stress layer is 700 MPa to 1200 MPa; and a surface compressive stress of the second surface compressive stress layer is 300 MPa to 850 MPa.

### Claim 5 (depends on 1)

The glass substrate according to claim 1, wherein a ratio of the surface compressive stress of the first surface compressive stress layer to the surface compressive stress of the second surface compressive stress layer is greater than or equal to 1.2.

### Claim 6 (depends on 1)

The glass substrate according to claim 1, wherein when a thickness of the glass substrate is t, a depth of the first surface compressive stress layer is greater than or equal to 0.004 mm and is less than or equal to 0.1t; and the depth of the second surface compressive stress layer is greater than or equal to 0.085 mm and less than or equal to 0.6t.

### Claim 7 (depends on 1)

The glass substrate according to claim 1, wherein the thickness t of the glass substrate is 0.1 mm to 5 mm.

### Claim 8 (depends on 1)

The glass substrate according to claim 1, wherein a material of the glass substrate comprises one or more of lithium aluminum silicate glass, sodium calcium silicate glass, and soda-lime glass.

### Claim 9 (depends on 1)

The glass substrate according to claim 1, wherein the first surface compressive stress layer and/or the second surface compressive stress layer are obtained by performing chemical strengthening or physical tempering on a glass substrate.

### Claim 10 (depends on 1)

The glass substrate according to claim 1, wherein a bending strength of the glass substrate is 1000 MPa to 2100 MPa.

### Claim 11

A method for preparing a glass substrate, wherein two opposite sides of the glass substrate respectively have a first surface compressive stress layer and a second surface compressive stress layer; a surface compressive stress of the first surface compressive stress layer is greater than a surface compressive stress of the second surface compressive stress layer; and a depth of the first surface compressive stress layer is less than a depth of the second surface compressive stress layer, the method comprising:
providing a glass substrate precursor, the glass substrate precursor comprising two opposite side surfaces, and a first protective layer being arranged on one side surface to obtain the glass substrate precursor with the first protective layer;
placing the glass substrate precursor with the first protective layer in molten salt for primary strengthening to form a compressive stress layer on one side of the glass substrate precursor without the first protective layer arranged;
removing the first protective layer, and arranging a second protective layer on one side surface of the glass substrate precursor with the compressive stress layer arranged; and
placing the glass substrate precursor with the second protective layer in the molten salt for secondary strengthening to form a compressive stress layer on one side of the glass substrate precursor without the second protective layer arranged, and removing the second protective layer to obtain the glass substrate.

### Claim 12 (depends on 11)

The method according to claim 11, wherein the molten salt is sodium salt and potassium salt.

### Claim 13 (depends on 11)

The method according to claim 11, wherein the molten salt comprises one or more of potassium nitrate and sodium nitrate.

### Claim 14 (depends on 11)

The method according to claim 11, wherein a temperature of the molten salt is 360° C. to 450° ° C.

### Claim 15 (depends on 11)

The method according to claim 11, wherein time of the primary strengthening and/or the secondary strengthening is 60 min to 200 min.

### Claim 16 (depends on 11)

The method according to claim 11, wherein the primary strengthening and/or the secondary strengthening are carried out step by step using various kinds of molten salt.

### Claim 17 (depends on 11)

The method according to claim 11, wherein the first protective layer and the second protective layer are heat-resistant protective coatings.

### Claim 18 (depends on 1)

An electronic device, comprising an electronic component and a glass cover plate covering the electronic component, the glass cover plate comprising the glass substrate according to claim 1.

### Claim 19 (depends on 18)

The electronic device according to claim 18, wherein in the glass substrate, the second surface compressive stress layer is close to the electronic component, and the first surface compressive stress layer is far away from the electronic component.

### Claim 20 (depends on 18)

The electronic device according to claim 18, wherein the glass cover plate is a screen cover plate and/or a back cover plate of the electronic device.