# US 2024/0254035 A1 · Hollow glass microspheres coated from reactive graphene

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0254035 A1
- Document ID: US20240254035A1
- Status: Published application
- Kind: A1
- Application number: 18/424,068
- Filed: 2024-01-26
- Published: 2024-08-01
- Earliest claimed: 2023-01-30
- Assignees: HydroGraph Clean Power Inc.
- Applicants: HydroGraph Clean Power Inc.
- Inventors: Ranjith Divigalpitiya; Jun Wang
- Web page: https://patentgrep.com/patent/US20240254035A1

## CPC

- C03C 17/22: with other inorganic material (C03C17/34, C03C17/44 take precedence)
- C03C 11/002: {Hollow glass particles}
- C03C 17/009: {Mixtures of organic and inorganic materials, e.g. ormosils and ormocers}
- C03C 2218/111: by dipping, immersion
- C03C: CHEMICAL COMPOSITION OF GLASSES, GLAZES OR VITREOUS ENAMELS; SURFACE TREATMENT OF GLASS; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS, MINERALS OR SLAGS; JOINING GLASS TO GLASS OR OTHER MATERIALS

## Abstract

Graphene coated hollow glass microspheres may be easily prepared by mixing Pristine Reactive Graphene Particles with hollow glass microspheres under conditions to associate the Pristine Reactive Graphene Particles on the external surface of the hollow glass microspheres by chemical coupling with a silane coupling agent to form graphene coated hollow glass microspheres. Graphene coated hollow glass microspheres prepared by the methods as described herein are also provided. In an embodiment, graphene coated hollow glass microspheres comprise a graphene coating formed from Pristine Reactive Graphene Particles associated on the external surface of the hollow glass microspheres by chemical coupling with a silane coupling agent.

## Claims

### Claim 1

A method of making graphene coated hollow glass microspheres comprising:
providing Pristine Reactive Graphene Particles having an average particle size of from about 10 to about 500 nm and having an oxygen content of from about 0.5% to about 15% oxygen;
providing hollow glass microspheres having an average diameter of from about 10 μm to 150 μm and a wall thickness of from about 0.5 μm to about 2 μm and having an external surface;
Reacting either the hollow glass microspheres or the Pristine Reactive Graphene Particles with a silane coupling agent to provide reactive hollow glass microspheres or glass-reactive Pristine Reactive Graphene Particles; and
mixing the Pristine Reactive Graphene Particles with the reactive hollow glass microspheres under conditions to associate the Pristine Reactive Graphene Particles on the external surface of the reactive hollow glass microspheres by chemical coupling with the silane coupling agent, or
mixing the glass-reactive Pristine Reactive Graphene Particles with the hollow glass microspheres under conditions to associate the glass-reactive Pristine Reactive Graphene Particles on the external surface of the hollow glass microspheres by chemical coupling with the silane coupling agent to provide graphene coated hollow glass microspheres.

### Claim 2 (depends on 1)

The method of claim 1, wherein the graphene coated hollow glass microspheres are prepared by
reacting the hollow glass microspheres with a silane coupling agent to provide reactive hollow glass microspheres and
mixing the Pristine Reactive Graphene Particles are mixed with the reactive hollow glass microspheres under conditions to associate the Pristine Reactive Graphene Particles on the external surface of the reactive hollow glass microspheres by chemical coupling with the silane coupling agent.

### Claim 3 (depends on 1)

The method of claim 1, wherein the graphene coated hollow glass microspheres are prepared by
reacting the Pristine Reactive Graphene Particles with a silane coupling agent to provide glass-reactive Pristine Reactive Graphene Particles; and
mixing the glass-reactive Pristine Reactive Graphene Particles with the hollow glass microspheres under conditions to associate the glass-reactive Pristine Reactive Graphene Particles on the external surface of the hollow glass microspheres by chemical coupling with the silane coupling agent to provide graphene coated hollow glass microspheres.

### Claim 4 (depends on 1)

The method of claim 1, wherein the hollow glass microspheres are treated by hydroxylation prior to reaction with the silane coupling agent.

### Claim 5 (depends on 1)

The method of claim 1, wherein the hollow glass microspheres are treated in a solution comprising a base selected from the group consisting of KOH, NaOH, NH4OH, and combinations thereof prior to reaction with the silane coupling agent.

### Claim 6 (depends on 1)

The method of claim 1, wherein the Pristine Graphene Particles are treated with a surfactant.

### Claim 7 (depends on 1)

The method of claim 1, wherein the Pristine Graphene Particles are treated with a surfactant prior to mixing of the Pristine Graphene Particles with the hollow glass microspheres.

### Claim 8 (depends on 1)

The method of claim 1, wherein the Pristine Graphene Particles are treated with a surfactant at the time of mixing of the Pristine Graphene Particles with the hollow glass microspheres.

### Claim 9 (depends on 6)

The method of claim 6, wherein the surfactant is selected from the group consisting of sodium cholate, and hexadecyltrimethylammonium bromide.

### Claim 10 (depends on 1)

The method of claim 1, wherein the hollow glass microspheres have an average diameter of from about 20 μm to 140 μm, or wherein the hollow glass microspheres have an average diameter of from about 20 μm to 140 μm, or wherein the hollow glass microspheres have an average diameter of from about 30 μm to about 115, or wherein the hollow glass microspheres have an average diameter of from 30 μm to 90 μm, or wherein the hollow glass microspheres have an average diameter of from about 15 μm to about 70 μm, or wherein the hollow glass microspheres have an average diameter of from about 10 μm to 50 μm.

### Claim 11 (depends on 1)

The method of claim 1, wherein the hollow glass microspheres have a wall thickness of from about 0.7 μm to about 1.2 μm.

### Claim 12 (depends on 1)

The method of claim 1, wherein the Pristine Reactive Graphene Particles have an average particle size of from about 35 nm to about 250 nm; or wherein the Pristine Reactive Graphene Particles have an average particle size of from about 50 nm to about 200 nm; or wherein the Pristine Reactive Graphene Particles used in preparation of the graphene coated hollow glass microspheres have an average particle size of from about 75 nm to about 150.

### Claim 13 (depends on 1)

The method of claim 1, wherein the Pristine Reactive Graphene Particles have an oxygen content of from about 0.5% to about 10% oxygen, or wherein the Pristine Reactive Graphene Particles have an oxygen content of from about 1% to about 8% oxygen, or wherein the Pristine Reactive Graphene Particles have an oxygen content of from about 1.5% to about 6% oxygen, or wherein the Pristine Reactive Graphene Particles have an oxygen content of from about 1.5% to about 5% oxygen, or wherein the Pristine Reactive Graphene Particles have an oxygen content of from about 1.5% to about 4% oxygen.

### Claim 14 (depends on 1)

The method of claim 1, wherein the graphene coated hollow glass microspheres have an average graphene coating coverage of at least about 60% of the external surface area of the hollow glass microspheres when evaluated by FESEM at 250× magnification.

### Claim 15 (depends on 1)

The method of claim 1, wherein the Pristine Graphene Particles are mixed with the hollow glass microspheres under gentle stirring conditions such that less than 30% of the hollow glass microspheres are broken during the preparation of the graphene coated hollow glass microspheres; or wherein the Pristine Graphene Particles are mixed with the hollow glass microspheres under gentle stirring conditions such that less than 20% of the hollow glass microspheres are broken during the preparation of the graphene coated hollow glass microspheres; or wherein the Pristine Graphene Particles are mixed with the hollow glass microspheres under gentle stirring conditions such that less than 10% of the hollow glass microspheres are broken during the preparation of the graphene coated hollow glass microspheres.

### Claim 16 (depends on 1)

The method of claim 1, wherein the Pristine Reactive Graphene Particles are present on the hollow glass microspheres in an amount effective to provide graphene coated hollow glass microspheres having an L*a*b*color value of L*=about 15 to 17; a*=about −1 to 0; and b*=about −0.5 to −1.5; or wherein the Pristine Reactive Graphene Particles are present on the hollow glass microspheres in an amount effective to provide graphene coated hollow glass microspheres having an L*a*b*color value of about L*=16.6; a*=−0.43 & b*=−0.98.

### Claim 17 (depends on 1)

The method of claim 1, wherein the Pristine Reactive Graphene Particles are present on the hollow glass microspheres in an amount effective to provide graphene coated hollow glass microspheres having an electrical conductivity of from about 0.4 S/m to about 0.6 S/m.

### Claim 18 (depends on 1)

The method of claim 1, wherein the amino silane coupling agent is selected from gamma-aminopropyl-triethoxy-silane (KH550 or A1100), N-(ρ-aminoethyl)-γ-aminopropyltrimethoxysilane (KH792 or A1120) or (γ-trimethoxy-silylpropyl) amine (A1170).

### Claim 19 (depends on 1)

The method of claim 1, further comprising the step of reacting residual oxide surface groups on the Pristine Reactive Graphene Particles of the graphene coated hollow glass microspheres with reactants to provide functionalized graphene coated hollow glass microspheres.

### Claim 20 (depends on 19)

The method of claim 19, wherein the functionalized graphene coated hollow glass microspheres comprises functionalities selected from the group consisting of methyl esters, primary amines, amides, alcohol esters, hydroxides, carboxylic acids, or combinations thereof.

### Claim 21 (depends on 19)

The method of claim 19, wherein the functionalized graphene coated hollow glass microspheres comprises at least one functionality that is a targeting moiety selected from the group consisting of aptamers, peptides, antibodies, receptor proteins, and combinations thereof.

### Claim 22 (depends on 1)

Graphene coated hollow glass microspheres prepared by the method of claim 1.

### Claim 23

Graphene coated hollow glass microspheres comprising
hollow glass microspheres having an average diameter of from about 10 μm to 150 μm and a wall thickness of from about 0.5 μm to about 2 μm,
and Pristine Reactive Graphene Particles having an average particle size of from about 10 to about 500 nm and having an oxygen content of from about 0.5% to about 15% oxygen;
wherein the Pristine Reactive Graphene Particles are associated on the surface of the hollow glass microspheres by chemical coupling with a silane coupling agent.