# US 2024/0254030 A1 · Manufacturing method for high-quality quartz crucible

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0254030 A1
- Document ID: US20240254030A1
- Status: Published application
- Kind: A1
- Application number: 18/631,507
- Filed: 2024-04-10
- Published: 2024-08-01
- Earliest claimed: 2022-03-25
- Assignees: Jinzhou Youxin Quartz Technology Co., Ltd
- Applicants: Jinzhou Youxin Quartz Technology Co., Ltd
- Inventors: Man CHEN; Zonghui LI; Jian ZHU; Ye WANG; Zhen WANG; Zhiqiang ZHANG
- Web page: https://patentgrep.com/patent/US20240254030A1

## CPC

- C03B 19/066: {for the production of quartz or fused silica articles (other processes specially adapted for the production of quartz or fused silica articles C03B20/00)}
- C03B 19/095: {by centrifuging, e.g. arc discharge in rotating mould (crucibles for crystal pulling in general C30B15/10, C30B35/002)}
- C30B 35/002: {Crucibles or containers}
- C30B 15/10: Crucibles or containers for supporting the melt
- C30B 29/06: Silicon
- C03B: MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
- C30B: SINGLE-CRYSTAL GROWTH (by using ultra-high pressure, e.g. for the formation of diamonds, B01J3/06); UNIDIRECTIONAL SOLIDIFICATION OF EUTECTIC MATERIAL OR UNIDIRECTIONAL DEMIXING OF EUTECTOID MATERIAL; REFINING BY ZONE-MELTING OF MATERIAL (zone-refining of metals or alloys C22B); PRODUCTION OF A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (casting of metals, casting of other substances by the same processes or devices B22D; working of plastics B29; modifying the physical structure of metals or alloys C21D, C22F); SINGLE CRYSTALS OR HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE; AFTER-TREATMENT OF SINGLE CRYSTALS OR A HOMOGENEOUS POLYCRYSTALLINE MATERIAL WITH DEFINED STRUCTURE (for producing semiconductor devices or parts thereof H10); APPARATUS THEREFOR

## Abstract

A manufacturing method for high-quality quartz crucible uses a vacuum arc method to melt, the positioning of the graphite electrode and dwell time at each position meet following requirements in which: taking a position of an upper end surface of a mold opening as a zero point, an end of the graphite electrode is marked as + when above the zero point, marked as − when below the zero point; a starting position of the graphite electrode is +0.10˜0.30 times an outer diameter of the crucible, dwell time ≥2 minutes, then the position is descended sequentially in accordance with a stepwise positioning method, staying for a period of time every time descending to a position, the graphite electrode continuously releases a high-temperature arc to melt crucible blank during a corresponding period of time at a corresponding position, and reaches a bottom polishing position after moving at least 3 times.

## Claims

### Claim 1

A manufacturing method for high-quality quartz crucible, the manufacturing method using vacuum arc method and comprising following steps:
pouring high-purity quartz sand raw material into a crucible mold, using a forming device to evenly mold the quartz sand raw material on an inner surface of a mold to form a crucible blank, moving the crucible mold as a whole into an arc melting furnace, melting the quartz sand by releasing high-temperature arc through a graphite electrode, and finally, rapidly cooling to form a quartz crucible blank; wherein in process of using the graphite electrode to release high-temperature arc, control positioning of the graphite electrode in a height direction and dwell time at each position to meet following requirements in which:
taking a position of an upper end surface of a mold opening as a zero point, an end of the graphite electrode is marked as + when above the zero point, marked as − when below the zero point; during melting process, a starting position of the graphite electrode is +0.10˜0.30 times an outer diameter of the crucible, dwell time ≥2 minutes, then the position is descended sequentially in accordance with a stepwise positioning method, staying for a period of time every time descending to a position, the graphite electrode continuously releases a high-temperature arc to melt the crucible blank during a corresponding period of time at a corresponding position, and reaches a bottom polishing position after moving at least 3 times; the bottom polishing position is a lowest position that the graphite electrode reaches and enters an interior of the crucible blank, 300-550 mm away from a bottom of the crucible; at the bottom polishing position, the graphite electrode stays for a predetermined time to perform high-temperature polishing and volatile impurity removal to the bottom of the crucible;
after leaving from the bottom polishing position, the graphite electrode ascends again to a finishing position, the finishing position is +0.05-0.07 times the outer diameter of the crucible, at this position, high-temperature polishing and volatile impurity removal are conducted to an upper part of an inner wall of the quartz crucible.

### Claim 2 (depends on 1)

The manufacturing method according to claim 1, wherein, during the entire melting process, the positioning of the graphite electrode comprises the starting position, a second position, a third position, a fourth position, a fifth position, the bottom polishing position and the finishing position, wherein from the starting position to the bottom polishing position is stepwise descending and staying for a period of time at each position.

### Claim 3 (depends on 2)

The manufacturing method according to claim 2, wherein, the dwell time allocation for the graphite electrode at each position is as follows: a sum of the dwell time at the starting position, the second position, and the third position is 0.4-0.5 t, the dwell time at the fourth position is 0.1-0.2 t, the dwell time at the fifth position is 0.1 t, the dwell time at the bottom polishing position is 0.2-0.3 t, and the dwell time at the finishing position is 0.1 t; t is a total melting time of a target quartz crucible.

### Claim 4 (depends on 3)

The manufacturing method according to claim 3, wherein, according to quartz crucibles with different specifications, the dwell time allocation for the graphite electrode at each position is as follows:
a quartz crucible with an outer diameter of 24 inches: the sum of the dwell time at the starting position, the second position and the third position is 0.4 t, the dwell time at the fourth position is 0.2 t, the dwell time at the fifth position is 0.1 t, the dwell time at the bottom polishing position is 0.2 t; the dwell time at the finishing position is 0.1 t; and the total melting time is 14-16 minutes;
a quartz crucible with an outer diameter of 26 inches: the sum of the dwell time at the starting position, the second position and the third position is 0.45 t, the dwell time at the fourth position is 0.15 t, the dwell time at the fifth position is 0.1 t, the dwell time at the bottom polishing position is 0.2 t; the dwell time at the finishing position is 0.1 t; and the total melting time is 17-19 minutes;
a quartz crucible with an outer diameter of 28 inches: the sum of the dwell time at the starting position, the second position and the third position is 0.45 t, the dwell time at the fourth position is 0.1 t, the dwell time at the fifth position is 0.1 t, the dwell time at the bottom polishing position is 0.25 t; the dwell time at the finishing position is 0.1 t; and the total melting time is 22-26 minutes;
a quartz crucible with an outer diameter of 32 inches: the sum of the dwell time at the starting position, the second position and the third position is 0.4 t, the dwell time at the fourth position is 0.1 t, the dwell time at the fifth position is 0.1 t, the dwell time at the bottom polishing position is 0.3 t; the dwell time at the finishing position is 0.1 t; and the total melting time is 28-32 minutes.

### Claim 5 (depends on 1)

The manufacturing method according to claim 1, wherein, during graphite electrode positioning process, positioning accuracy of the graphite electrode at each position is ±5 mm.

### Claim 6 (depends on 1)

The manufacturing method according to claim 1, wherein, during the entire melting process, vacuum pressure is controlled at −0.093 MPa˜−0.1 MPa; power of the graphite electrode is 500-2000 kW.

### Claim 7 (depends on 6)

The manufacturing method according to claim 6, wherein, when melting a quartz crucible with an outer diameter of 24 inches, the power of the graphite electrode is 750-850 kW; when melting a quartz crucible with an outer diameter of 26 inches, the power of the graphite electrode is 850-950 kW; when melting a quartz crucible with an outer diameter of 28 inches, the power of the graphite electrode is 1000-1100 kW; when melting a quartz crucible with an outer diameter of 32 inches, the power of the graphite electrode is 1300-1400 kW.

### Claim 8 (depends on 1)

The manufacturing method according to claim 1, wherein, during graphite electrode positioning process, at the end of melting at each position, the graphite electrode is subjected to air blowing for dust removal, and volatile matter deposited on a surface of the graphite electrode is blown away.

### Claim 9 (depends on 2)

The manufacturing method according to claim 2, wherein, a height difference between the bottom polishing position and the fifth position is more than 100 mm.

### Claim 10 (depends on 1)

A high-quality quartz crucible, wherein, the crucible is produced using the manufacturing method according to claim 1.