# US 2024/0251797 A1 · Method for producing molded article for water purification

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0251797 A1
- Document ID: US20240251797A1
- Status: Published application
- Kind: A1
- Application number: 18/629,962
- Filed: 2024-04-09
- Published: 2024-08-01
- Earliest claimed: 2022-04-28
- Assignees: Sang Won BAEK
- Inventors: Sang Won BAEK; Yong Jin BAEK
- Web page: https://patentgrep.com/patent/US20240251797A1

## CPC

- A01N 59/00: Biocides, pest repellants or attractants, or plant growth regulators containing elements or inorganic compounds
- A01N 25/34: Shaped forms, e.g. sheets, not provided for in any other sub-group of this main group
- A01N 59/06: Aluminium; Calcium; Magnesium; Compounds thereof
- A01N 59/14: Boron; Compounds thereof
- A01N 59/16: Heavy metals; Compounds thereof
- A01P 1/00: Disinfectants; Antimicrobial compounds or mixtures thereof
- A01P 3/00: Fungicides
- A01P 13/00: Herbicides; Algicides
- Y02W 10/37: using solar energy
- A01N: PRESERVATION OF BODIES OF HUMANS OR ANIMALS OR PLANTS OR PARTS THEREOF (preservation of food or foodstuff A23); BIOCIDES, e.g. AS DISINFECTANTS, AS PESTICIDES OR AS HERBICIDES (preparations for medical, dental or toiletry purposes which kill or prevent the growth or proliferation of unwanted organisms A61K); PEST REPELLANTS OR ATTRACTANTS; PLANT GROWTH REGULATORS
- A01P: BIOCIDAL, PEST REPELLANT, PEST ATTRACTANT OR PLANT GROWTH REGULATORY ACTIVITY OF CHEMICAL COMPOUNDS OR PREPARATIONS
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present disclosure relates to a method for producing a molded article for water purification, including: preparing a natural mineral extract in an environmentally friendly manner; preparing a natural mineral-photocatalyst aqueous solution containing photocatalytic titanium dioxide (TiO2) nanopowder dispersed in the natural mineral extract; and impregnating a plastic material with the natural mineral-photocatalyst aqueous solution under high-temperature and high-pressure conditions. The produced molded article may be installed on the surface of water or under water in lakes, reservoirs, ponds, rivers, aquariums, fish farms, swimming pools, water purification plants, and the like to adsorb and degrade organic substances, block the growth of bacteria and mold, and effectively reduce algal bloom.

## Claims

### Claim 1

A method for producing a deodorizer, comprising the following sequential steps:
(1) preparing natural mineral powder by pulverizing a natural mineral mixture, which contains 5 to 15 wt % of red clay, 5 to 15 wt % of volcanic ash, 25 to 35 wt % of barley stone, 25 to 35 wt % of granophyre, and 15 to 25 wt % of tourmaline, to a size of 325 mesh or less;
(2) preparing a natural mineral extract by adding the natural mineral powder, prepared in step (1), to a 2- to 5-fold weight of purified water to obtain a natural mineral powder aqueous solution, grinding the natural mineral powder by a ball mill for 24 to 48 hours, and then precipitating a solid from the natural mineral powder aqueous solution, followed by separating a colloidal transparent supernatant, containing natural minerals dissolved in purified water, from the solid;
(3) preparing a natural mineral-photocatalyst aqueous solution by dispersing 1 to 10 parts by weight of titanium dioxide (TiO2) nanopowder having a particle size of 1 to 100 nm in 100 parts by weight of the natural mineral extract prepared in step (2);
(4) impregnating a plastic material having a particle size of 1 to 10 mm with the natural mineral-photocatalyst aqueous solution, prepared in step (3), by spraying the natural mineral-photocatalyst aqueous solution in a high-temperature and high-pressure closed container charged with the plastic material; and
(5) producing a molded article having a predetermined shape from the plastic material impregnated with the natural mineral-photocatalyst aqueous solution in step (4).

### Claim 2 (depends on 1)

The method of claim 1, wherein step (4) comprises spraying the natural mineral-photocatalyst aqueous solution in the closed container at a temperature of 80 to 120° C. and a pressure of 3 to 6 bar, followed by cooling at room temperature (15 to 25° C.).

### Claim 3 (depends on 1)

The method of claim 1, wherein the plastic molded article produced in step (5) is in the form of a plate or hollow sphere having a specific gravity in the range of 0.9 to 1.5.

### Claim 4 (depends on 3)

The method of claim 3, wherein the plastic molded article in the form of the hollow sphere has 2 to 6 water-circulation holes formed therethrough.

### Claim 5 (depends on 1)

A deodorizer produced according to the method of claim 1.