# US 2024/0247379 A1 · Formation of metallic films on electroless metal plating of surfaces

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0247379 A1
- Document ID: US20240247379A1
- Status: Published application
- Kind: A1
- Application number: 18/099,846
- Filed: 2023-01-20
- Published: 2024-07-25
- Earliest claimed: 2023-01-20
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Chao Liu; David John Jorgensen; Marc Shull; Christopher Laurent Beaudry; Joseph Frederick Behnke
- Web page: https://patentgrep.com/patent/US20240247379A1

## CPC

- C23C 28/323: {with at least one amorphous metallic material layer}
- C23C 28/34: {including at least one inorganic non-metallic material layer, e.g. metal carbide, nitride, boride, silicide layer and their mixtures, enamels, phosphates and sulphates}
- H01J 37/32467: {Material}
- H01J 37/32477: {characterised by the means for protecting vessels or internal parts, e.g. coatings}
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

Embodiments of the disclosure relate to articles, coated chamber components, and techniques of coating chamber components and systems. In particular, disclosed is a chamber component and methods of forming the chamber component that includes a substrate and a first layer disposed on the substrate, the first layer including a metal with a first atomic concentration. The chamber component further includes a second layer disposed on the first layer, the second layer including the metal with a second atomic concentration that is at least 5 percent higher than the first atomic concentration.

## Claims

### Claim 1

A chamber component for a processing chamber, comprising:
a substrate;
a first layer disposed on the substrate, the first layer comprising a metal with a first atomic concentration; and
a second layer disposed on the first layer, the second layer comprising the metal with a second atomic concentration that is at least 5 percent higher than the first atomic concentration.

### Claim 2 (depends on 1)

The chamber component of claim 1, wherein the metal comprises nickel.

### Claim 3 (depends on 1)

The chamber component of claim 1, wherein the first layer comprises an amorphous layer of electroless nickel plated layer.

### Claim 4 (depends on 1)

The chamber component of claim 1, wherein the second layer comprises a crystalline layer of nickel.

### Claim 5 (depends on 1)

The chamber component of claim 1, further comprising:
a third layer disposed on the second layer, wherein the third layer comprises a nickel fluoride layer.

### Claim 6 (depends on 5)

The chamber component of claim 5, wherein the first layer comprises phosphorus with a atomic concentration at or above 10 percent, and wherein the second layer is free of phosphorus or comprises phosphorus with atomic concentration at or below 5 percent.

### Claim 7 (depends on 1)

The chamber component of claim 1, wherein the substrate comprises at least one of aluminum alloy, aluminum nitride (AlN), alumina (Al2O3), nickel (Ni), stainless steel, nickel-chromium alloy, austenitic nickel-chromium-based superalloy, pure nickel, quartz, iron, cobalt, titanium, magnesium, copper, zinc, or chromium.

### Claim 8 (depends on 1)

The chamber component of claim 1, wherein the second atomic concentration is at or above 95 percent.

### Claim 9 (depends on 8)

The chamber component of claim 8, wherein the second atomic concentration is at or above 99 percent.

### Claim 10 (depends on 1)

The chamber component of claim 1, wherein the substrate comprises a surface of a tool of a semiconductor processing chamber, and wherein the tool comprises at least one of a heater, an electrostatic chuck, a faceplate, a showerhead, a liner, a blocker plate, a gas box, an edge ring, or a bellows.

### Claim 11

A method comprising:
maintaining a plasma environment at a temperature that exceeds 250 degrees Celsius, wherein the plasma environment comprises fluorine radicals; and
exposing a layered structure to the plasma environment, wherein the layered structure comprises:
a substrate, and
a first layer disposed on the substrate, the first layer comprising a metal with a first atomic concentration below 90 percent.

### Claim 12 (depends on 11)

The method of claim 11, wherein maintaining the plasma environment comprises:
receiving, by a remote plasma source (RPS), a source gas, wherein the source gas comprises a fluorine-rich gas, wherein the fluorine-rich gas comprises at least one of:
nitrogen trifluoride,
molecular fluorine,
chlorine trifluoride, or
hydrogen fluoride,
causing dissociation of at least a part of the source gas into one or more products, wherein the one or more products comprise the fluorine radicals; and
providing the fluorine radicals to the plasma environment.

### Claim 13 (depends on 12)

The method of claim 12, wherein the source gas further comprises an inert gas, wherein a mass fraction of the inert gas in the source gas is between 50 percent and 80 percent, and a mass fraction of the fluorine-rich gas in the source gas is between 20 percent and 50 percent.

### Claim 14 (depends on 13)

The method of claim 13, wherein the temperature exceeds 290 degrees Celsius.

### Claim 15 (depends on 14)

The method of claim 14, wherein the temperature exceeds 340 degrees Celsius.

### Claim 16 (depends on 11)

The method of claim 11, further comprising:
maintaining the plasma environment at a pressure at or below 10 Torr.

### Claim 17 (depends on 11)

The method of claim 11, wherein exposing the layered structure to the plasma environment occurs for a predetermined time, associated with formation of a second layer of a target thickness, wherein the second layer is formed from the first layer and comprises nickel with a second atomic concentration that is at least 5 percent higher than the first concentration.

### Claim 18 (depends on 17)

The method of claim 17, wherein the predetermined time is longer than one hour.

### Claim 19 (depends on 17)

The method of claim 17, further comprising:
coating the second layer with a third layer, wherein the third layer comprises nickel fluoride.

### Claim 20 (depends on 11)

The method of claim 11, wherein the first layer comprises electroless nickel plated layer.

### Claim 21

A processing chamber, comprising:
a chamber component, comprising:
a substrate; and
a first layer disposed on the substrate, the first layer comprising a metal with a first atomic concentration; and
a second layer disposed on the first layer, the second layer comprising the metal with a second atomic concentration that is at least 5 percent higher than the first atomic concentration.