# US 2024/0246870 A1 · All-solid waste-based carbonated unburned lightweight aggregate and preparation method thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0246870 A1
- Document ID: US20240246870A1
- Status: Published application
- Kind: A1
- Application number: 18/018,855
- Filed: 2022-04-13
- Published: 2024-07-25
- Earliest claimed: 2021-11-29
- Assignees: Zhejiang University
- Applicants: Zhejiang University
- Inventors: TAO WANG; MENGXIANG FANG; WENKANG WANG; XIANG GAO; ZHONGYANG LUO; KEFA CEN
- Web page: https://patentgrep.com/patent/US20240246870A1

## CPC

- C04B 18/027: {Lightweight materials}
- C04B 18/08: Flue dust {, i.e. fly ash}
- C04B 18/142: {Steelmaking slags, converter slags}
- C04B 18/144: {Slags from the production of specific metals other than iron or of specific alloys, e.g. ferrochrome slags}
- C04B 20/026: {Comminuting, e.g. by grinding or breaking; Defibrillating fibres other than asbestos}
- C04B 40/0231: {Carbon dioxide hardening}
- C04B 40/0259: {Hardening promoted by a rise in pressure (C04B40/024 takes precedence)}
- C04B 40/0263: {Hardening promoted by a rise in temperature (C04B40/024 takes precedence)}
- C04B 2111/40: Porous or lightweight materials
- Y02W 30/91: Use of waste materials as fillers for mortars or concrete
- C04B: LIME, MAGNESIA; SLAG; CEMENTS; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDING MATERIALS; ARTIFICIAL STONE {(roofing granules E04D7/005)}; CERAMICS (devitrified glass-ceramics C03C10/00); REFRACTORIES; TREATMENT OF NATURAL STONE
- Y02W: CLIMATE CHANGE MITIGATION TECHNOLOGIES RELATED TO WASTEWATER TREATMENT OR WASTE MANAGEMENT

## Abstract

The present invention is proposed to disclose a method for preparing an all-solid waste-based carbonated unburned lightweight aggregate. The method includes the following steps: (1) subjecting an active component type solid waste, a lightweight filling type solid waste, and an alkali activation type solid waste to grinding and mixing to obtain a mixed solid waste powder; and (2) subjecting the mixed solid waste powder and water to granulation to obtain particles, and subjecting the particles to precuring and mineralization curing with CO2 to obtain the all-solid waste-based carbonated unburned lightweight aggregate. The active component type solid waste includes blast furnace slag, steel slag, or furnace slag. The lightweight filling type solid waste includes fly ash, river silt, or red mud. The alkali activation type solid waste includes carbide slag. In the present invention, all raw materials are selected from solid wastes, the alkali activation type solid waste is used as an alkali activator to replace traditional quicklime, sodium hydroxide, and sodium silicate, and a CO2 mineralization strengthening technology is used, so that the carbon fixation potential of the solid wastes is fully exerted, natural resources are saved, and the all-solid waste-based carbonated unburned lightweight aggregate prepared has excellent compressive strength.

## Claims

### Claim 1

A method for preparing an all-solid waste-based carbonated unburned lightweight aggregate, comprising the following steps:
(1) subjecting an active component type solid waste, a lightweight filling type solid waste, and an alkali activation type solid waste to grinding and mixing to obtain a mixed solid waste powder; and
(2) subjecting the mixed solid waste powder and water to granulation to obtain particles, and subjecting the particles to precuring and mineralization curing with CO2 to obtain the all-solid waste-based carbonated unburned lightweight aggregate;
wherein the active component type solid waste comprises blast furnace slag, steel slag, or furnace slag; the lightweight filling type solid waste comprises fly ash, river silt, or red mud; and the alkali activation type solid waste comprises carbide slag.

### Claim 2 (depends on 1)

The method for preparing an all-solid waste-based carbonated unburned lightweight aggregate according to claim 1, wherein after the mineralization curing with CO2, the particles are subjected to natural curing under the condition of water supplement to obtain the all-solid waste-based carbonated unburned lightweight aggregate.

### Claim 3 (depends on 1)

The method for preparing an all-solid waste-based carbonated unburned lightweight aggregate according to claim 1, wherein the active component type solid waste is the blast furnace slag or the steel slag, the lightweight filling type solid waste is the fly ash, and the alkali activation type solid waste is the carbide slag.

### Claim 4 (depends on 1)

The method for preparing an all-solid waste-based carbonated unburned lightweight aggregate according to claim 1, wherein the mixed solid waste powder has a particle size of less than 100 μm.

### Claim 5 (depends on 1)

The method for preparing an all-solid waste-based carbonated unburned lightweight aggregate according to claim 1, wherein in the mixed solid waste powder, a weight ratio of the active component type solid waste to the lightweight filling type solid waste to the alkali activation type solid waste is (1-9):1:(0.02-1).

### Claim 6 (depends on 1)

The method for preparing an all-solid waste-based carbonated unburned lightweight aggregate according to claim 1, wherein in step (2), the granulation process comprises the following steps:
(1) taking the mixed solid waste powder and the water at a mass ratio of 1:(0.2-0.3), dividing the mixed solid waste powder into a first part and a second part at a mass ratio of equal to or greater than 2, and subjecting the first part of the mixed solid waste powder and the water to granulation; and
(2) taking another spare water as a spray supplement to the granulation until a slurry mixture is formed by the first part of the mixed solid waste powder and the water, and then adding the second part of the mixed solid waste powder to obtain spherical particles.

### Claim 7 (depends on 1)

The method for preparing an all-solid waste-based carbonated unburned lightweight aggregate according to claim 1, wherein in step (2), the precuring is conducted under ambient pressure at a humidity of 70%-90% RH and a temperature of 15-25° C. for 24-72 hours.

### Claim 8 (depends on 1)

The method for preparing an all-solid waste-based carbonated unburned lightweight aggregate according to claim 1, wherein in step (2), a water-solid ratio of the particles after the precuring is controlled at 0.15-0.25.

### Claim 9 (depends on 1)

The method for preparing an all-solid waste-based carbonated unburned lightweight aggregate according to claim 1, wherein in step (2), the mineralization curing with CO2 is conducted under a CO2 pressure of 0.1-1 MPa at a temperature of 40-140° C. for 2-4 hours.

### Claim 10 (depends on 1)

An all-solid waste-based carbonated unburned lightweight aggregate prepared by the method for preparing an all-solid waste-based carbonated unburned lightweight aggregate according to claim 1.