# US 2024/0239004 A1 · Wood materials having anisotropic elasticity, and methods for fabrication and use thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0239004 A1
- Document ID: US20240239004A1
- Status: Published application
- Kind: A1
- Application number: 18/563,562
- Filed: 2022-05-27
- Published: 2024-07-18
- Earliest claimed: 2021-05-28
- Assignees: University of Maryland, College Park
- Applicants: University of Maryland, College Park
- Inventors: Liangbing HU; Xinpeng ZHAO; Yu LIU
- Web page: https://patentgrep.com/patent/US20240239004A1

## CPC

- B27K 5/06: Softening or hardening of wood
- D21B 1/021: {by chemical means}
- A43B 1/06: made of wood, cork, card-board, paper or like fibrous material
- B05D 3/104: {Pretreatment of other substrates}
- B05D 7/06: to wood
- B27K 3/0221: {Pore opening (B27K3/0214 takes precedence)}
- B27K 3/0278: {involving an additional treatment during or after impregnation}
- B27K 3/34: Organic impregnating agents {(polymers B27K3/15)}
- B27K 3/52: Impregnating agents containing mixtures of inorganic and organic compounds
- B27K 5/02: Staining or dyeing wood {(wood staining compositions C09D15/00)}; Bleaching wood (bleaching wood pulp D21C9/10)
- B05D 1/18: performed by dipping
- B27K 2240/10: Extraction of components naturally occurring in wood, cork, straw, cane or reed
- B27K: PROCESSES, APPARATUS OR SELECTION OF SUBSTANCES FOR IMPREGNATING, STAINING, DYEING, BLEACHING OF WOOD OR SIMILAR MATERIALS, OR TREATING OF WOOD OR SIMILAR MATERIALS WITH PERMEANT LIQUIDS, NOT OTHERWISE PROVIDED FOR (applying liquids or other fluent materials to surfaces in general B05; coating wood or similar material B44D); CHEMICAL OR PHYSICAL TREATMENT OF CORK, CANE, REED, STRAW OR SIMILAR MATERIALS
- D21B: FIBROUS RAW MATERIALS OR THEIR MECHANICAL TREATMENT
- A43B: CHARACTERISTIC FEATURES OF FOOTWEAR; PARTS OF FOOTWEAR
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)

## Abstract

A piece of natural wood can be immersed in a first solution at a first temperature less than 100° C. and then immersed in a second solution at a second temperature greater than 100° C. so as to form a piece of partially-delignified wood. In some embodiments, the first and second solutions can be the same solution, and the immersion at the second temperature can be heating the solution from the first temperature to the second temperature. The immersion in the first and second solutions can be effective to remove 45-90% of lignin from the piece of natural wood and to destroy a structure of the ray cells in the piece of natural wood while retaining cell walls of the other cells. The partially-delignified wood can then be dried. After drying, the partially-delignified wood can be clastic along its tangential direction but inelastic along its radial and longitudinal directions.

## Claims

### Claim 1

A method comprising:
(a) providing a piece of natural wood having a longitudinal direction, a radial direction, and a tangential direction, the natural wood having a microstructure with lumina formed by cell walls of (i) vessels and wood fiber cells or (ii) tracheids, each of the lumina having an axis that extends along the longitudinal direction, the natural wood further having ray cells, each ray cell having an axis that extends along the radial direction, the tangential direction being perpendicular to the longitudinal and radial directions;
(b) immersing at least part of the piece of natural wood in a first solution at a first temperature for a first time, the first temperature being less than 100° C.;
(c) after the immersing of (b), immersing the at least part of the piece of natural wood in a second solution at a second temperature for a second time so as to form a piece of partially-delignified wood, the second temperature being greater than 100° C., wherein the immersing of (b) and the immersing of (c) are effective to remove between 45% and 90%, inclusive, of lignin from the piece of natural wood and destroy a structure of the ray cells in the piece of natural wood while retaining the lumina formed by the cell walls; and
(d) after (c), drying the piece of partially-delignified wood such that the lumina remain open,
wherein, after (d), the piece of partially-delignified wood is substantially elastic along the tangential direction and substantially inelastic along the radial and longitudinal directions.

### Claim at position 2

2-4. (canceled)

### Claim 5 (depends on 1)

The method of claim 1, wherein, after (d), a moisture content of the piece of partially-delignified wood is less than or equal to 15 wt %.

### Claim 6

(canceled)

### Claim 7 (depends on 1)

The method of claim 1, wherein the first time is greater than or equal to 8 hours, and the second time is less than or equal to 10 hours.

### Claim at position 6

8-9. (canceled)

### Claim 10 (depends on 1)

The method of claim 1, wherein the first temperature is 5-95° C.,
inclusive, and/or the second temperature is 120-180° C., inclusive.

### Claim 11 (depends on 1)

The method of claim 1, wherein the first solution, the second solution, or both the first and second solutions comprise sodium hydroxide (NaOH), lithium hydroxide (LiOH), potassium hydroxide (KOH), sodium sulfite (Na2SO3), sodium sulfate (Na2SO4), sodium sulfide (Na2S), NanS wherein n is an integer, urea (CH4N2O), sodium bisulfite (NaHSO3), sulfur dioxide (SO2), anthraquinone (C14H8O2), methanol (CH3OH), ethanol (C2H5OH), butanol (C4H9OH), formic acid (CH2O2), hydrogen peroxide (H2O2), acetic acid (CH3COOH), butyric acid (C4H8O2), peroxyformic acid (CH2O3), peroxyacetic acid (C2H4O3), ammonia (NH3), tosylic acid (p-TsOH), sodium hypochlorite (NaClO), sodium chlorite (NaClO2), chlorine dioxide (ClO2), chlorine (Cl2), or any combination of the above.

### Claim at position 9

12-14. (canceled)

### Claim 15 (depends on 1)

The method of claim 1, further comprising, subjecting the piece of partially-delignified wood to one or more surface treatments.

### Claim 16 (depends on 15)

The method of claim 15, wherein the one or more surface treatments comprises applying a coating to external surfaces, internal surfaces, or both external and internal surfaces of the piece of partially-delignified wood, and the coating has a thickness of 10 nm to 10 μm, inclusive.

### Claim at position 12

17-23. (canceled)

### Claim 24 (depends on 15)

The method of claim 15, wherein, after the one or more surface treatments, the piece of partially-delignified wood has a porosity of at least 50%.

### Claim 25 (depends on 1)

The method of claim 1, further comprising, filling the open lumina of the piece of partially-delignified wood with a natural or synthetic polymer, wherein, after the filling, the piece of partially-delignified wood has a porosity of less than or equal to 10%.

### Claim 26

(canceled)

### Claim 27 (depends on 1)

The method of claim 1, wherein, after (d), a modulus of elasticity of the piece of partially-delignified wood along the tangential direction is at least an order of magnitude less than that along the radial direction or that along the longitudinal direction.

### Claim 28

(canceled)

### Claim 29 (depends on 1)

The method of claim 1, further comprising, after (d), arranging the piece of partially-delignified wood in or as part of a structure such that a force applied to the structure is directed substantially along the tangential direction.

### Claim at position 19

30-31. (canceled)

### Claim 32

A wood structure comprising:
a piece of partially-delignified wood that retains lumina formed by cell walls of (i) vessels and wood fiber cells or (ii) tracheids from an original natural wood but lacks ray cells from the original natural wood, each of the lumina having an axis that extends along a longitudinal direction of the natural wood, each ray cell having an axis that extends along a radial direction of the natural wood,
wherein a tangential direction of the natural wood is perpendicular to the longitudinal and radial directions, and
the piece of partially-delignified wood is substantially elastic along the tangential direction and substantially inelastic along the radial and longitudinal directions.

### Claim at position 21

33-34. (canceled)

### Claim 35 (depends on 32)

The wood structure of claim 32, wherein:
the natural wood is a hardwood, and a lignin content of the piece of partially-delignified wood is 2-16.5 wt %, inclusive; or
the natural wood is a softwood, and a lignin content of the piece of partially-delignified wood is 2.5-19.2 wt %, inclusive.

### Claim 36

(canceled)

### Claim 37 (depends on 32)

The wood structure of claim 32, wherein a moisture content of the piece of partially-delignified wood is less than or equal to 15 wt %.

### Claim 38

(canceled)

### Claim 39 (depends on 32)

The wood structure of claim 32, wherein the piece of partially-delignified wood has a compressive strength of 0.1-1.5 MPa, inclusive, at 60% compression.

### Claim 40 (depends on 32)

The wood structure of claim 32, further comprising a coating on external surfaces, internal surfaces, or both external and internal surfaces of the piece of partially-delignified wood, wherein the coating has a thickness of 10 nm to 10 μm, inclusive.

### Claim at position 28

41-47. (canceled)

### Claim 48 (depends on 40)

The wood structure of claim 40, wherein the piece of partially-delignified wood has a porosity of at least 50%.

### Claim 49 (depends on 32)

The wood structure of claim 32, further comprising a natural or synthetic polymer disposed within or filling open lumina of the piece of partially-lignified wood, wherein the piece of partially-delignified wood has a porosity less than or equal to 10%.

### Claim 50

(canceled)

### Claim 51 (depends on 32)

The wood structure of claim 32, wherein a modulus of elasticity of the piece of partially-delignified wood along the tangential direction is at least an order of magnitude less than that along the radial direction or that along the longitudinal direction.

### Claim 52

(canceled)

### Claim 53 (depends on 32)

The wood structure of claim 32, wherein the structure is formed as footwear.

### Claim 54

(canceled)