# US 2024/0238767 A1 · Catalyst and method for sulfur-tolerant shift catalytic reaction

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0238767 A1
- Document ID: US20240238767A1
- Status: Published application
- Kind: A1
- Application number: 18/250,725
- Filed: 2021-09-15
- Published: 2024-07-18
- Earliest claimed: 2020-10-27
- Assignees: China Petroleum & Chemical Corporation; Sinopec Qilu Company
- Applicants: China Petroleum & Chemical Corporation; Sinopec Qilu Company
- Inventors: Min WANG; Jinshan XU; Hantao YU; Zhimin BAI; Hao WANG; Jianbo JIANG; Hongxia XUE
- Web page: https://patentgrep.com/patent/US20240238767A1

## CPC

- B01J 23/8871: {Rare earth metals or actinides}
- B01J 21/04: Alumina
- B01J 23/002: {Mixed oxides other than spinels, e.g. perovskite}
- B01J 23/28: Molybdenum
- B01J 23/882: and cobalt
- B01J 23/887: containing in addition other metals, oxides or hydroxides provided for in groups B01J23/02 - B01J23/36
- B01J 23/8872: {Alkali or alkaline earth metals}
- B01J 35/30: characterised by their physical properties
- B01J 35/60: characterised by their surface properties or porosity
- B01J 35/613: {10-100 m2/g}
- B01J 35/615: {100-500 m2/g}
- B01J 37/0236: {Drying, e.g. preparing a suspension, adding a soluble salt and drying}
- B01J 37/03: Precipitation; Co-precipitation
- B01J 37/031: {Precipitation}
- B01J 37/035: {Precipitation on carriers}
- B01J 37/036: {to form a gel or a cogel}
- B01J 37/08: Heat treatment {(B01J37/0009, B01J37/0018 take precedence)}
- B01J 37/088: {Decomposition of a metal salt}
- C01B 3/16: using catalysts
- C07C 1/04: from carbon monoxide with hydrogen
- C07C 9/04: Methane (production by treatment of sewage C02F11/04; natural gas, synthetic natural gas C10L3/06)
- C01B 2203/0283: containing a CO-shift step, i.e. a water gas shift step
- C01B 2203/1052: Nickel or cobalt catalysts
- C01B 2203/1082: Composition of support materials
- C10K 3/04: reducing the carbon monoxide content {, e.g. water-gas shift [WGS]}
- Y02P 20/52: using catalysts, e.g. selective catalysts
- B01J: CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOID CHEMISTRY; THEIR RELEVANT APPARATUS
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C07C: ACYCLIC OR CARBOCYCLIC COMPOUNDS
- C10K: PURIFYING OR MODIFYING THE CHEMICAL COMPOSITION OF COMBUSTIBLE GASES CONTAINING CARBON MONOXIDE
- Y02P: CLIMATE CHANGE MITIGATION TECHNOLOGIES IN THE PRODUCTION OR PROCESSING OF GOODS

## Abstract

A sulfur-tolerant catalyst can be used in the sulfur-tolerant shift catalytic reaction. The catalyst has a carrier and a molybdenum oxide, a cobalt oxide and a cobalt-molybdenum-based perovskite composite oxide carried thereon. The cobalt-molybdenum-based perovskite composite oxide contains a molybdenum element, a cobalt element, an A element, and an oxygen element. The A element is one or more selected from a group consisting of a rare-earth metal element, an alkali metal element and an alkaline earth metal element.

## Claims

### Claim 1

A catalyst comprising a carrier, and a molybdenum oxide, a cobalt oxide and a cobalt-molybdenum-based perovskite composite oxide carried thereon, the cobalt-molybdenum-based perovskite composite oxide comprises a molybdenum element, a cobalt element, an A element, and an oxygen element;
wherein the A element is one or more selected from a group consisting of a rare-earth metal element, an alkali metal element and an alkaline earth metal element.

### Claim 2 (depends on 1)

The catalyst of claim 1, wherein the A element is one or more selected from a group consisting of La, Ce, Nd, Gd, Na, K, Mg, Ca and Sr.

### Claim 3 (depends on 1)

The catalyst of claim 1, wherein the A element includes an A1 element being one or more of rare-earth metal elements and an A2 element being one or more of alkali metal elements and alkaline earth metal elements.

### Claim 4 (depends on 1)

The catalyst of claim 1, wherein the catalyst exhibits a characteristic peak at 27.9±0.2°.

### Claim 5 (depends on 1)

The catalyst of claim 1, wherein the catalyst has a main reduction peak temperature of 600° C. or more.

### Claim 6 (depends on 1)

The catalyst of claim 1, wherein the catalyst has two or more, preferably three or more adsorption-desorption peaks at a temperature of 200° C. or more in a programmed temperature rise sulfidation test.

### Claim 7 (depends on 1)

The catalyst of claim 1, wherein the content of A element in the catalyst is 0.4 mol or more and less than 1 mol, relative to the total content 1 mol of molybdenum element and cobalt element.

### Claim 8 (depends on 1)

The catalyst of claim 1, wherein the content of molybdenum in the catalyst is more than 0.4 mol and less than 1 mol, relative to the total content 1 mol of molybdenum element and cobalt element.

### Claim 9 (depends on 1)

The catalyst of claim 1, wherein the carrier is alumina, silica, titanium dioxide, zirconium dioxide, magnesium oxide, nickel oxide and a carbon-based carrier or a composite carrier formed from two or more thereof, alumina or a composite carrier formed with the alumina and one or more selected from a group consisting of silica, titanium dioxide, zirconium dioxide, magnesium oxide, nickel oxide and a carbon-based carrier.

### Claim 10 (depends on 1)

The catalyst of claim 1, wherein the catalyst comprises a carrier in an amount of 30-90% by mass.

### Claim 11 (depends on 1)

The catalyst of claim 1, wherein the catalyst has a specific surface area of 40 m2·g−1 or more.

### Claim 12 (depends on 1)

A method for sulfur-tolerant shift catalytic reaction, comprising: contacting CO in a feed gas with water vapor in the presence of a catalyst of claim 1;
wherein the feed gas comprises H2S in an amount of 100 ppm or more.

### Claim 13 (depends on 3)

The catalyst of claim 3, wherein the A1 element is one or more selected from a group consisting of La, Ce, Nd and Gd, the A2 element is one or more selected from a group consisting of Na, K, Mg, Ca and Sr.

### Claim 14 (depends on 3)

The catalyst of claim 3, wherein a molar ratio of the Al element to the A2 element is 1-99:99-1.

### Claim 15 (depends on 14)

The catalyst of claim 14, wherein a molar ratio of the Al element to the A2 element is 1-9:9-1.

### Claim 16 (depends on 4)

The catalyst of claim 4, wherein the catalyst exhibits characteristic peaks at 24.9±0.2°, 27.9±0.2° and 36.2±0.2° in the X-Ray Diffraction (XRD) pattern.

### Claim 17 (depends on 3)

The catalyst of claim 3, wherein the catalyst exhibits characteristic peaks at 24.9±0.2°.

### Claim 18 (depends on 17)

The catalyst of claim 17, wherein the catalyst exhibits characteristic peaks at 24.9±0.2°, 27.9±0.2° and 36.2±0.2° in the X-Ray Diffraction (XRD) pattern.

### Claim 19 (depends on 5)

The catalyst of claim 5, wherein the catalyst has a main reduction peak temperature within a range of 600-850° C. in the H2-TPR pattern.

### Claim 20 (depends on 12)

The method of claim 12, wherein the content of H2S is within a range of 100-1,500 ppm.