# US 2024/0218278 A1 · Powdery alternative fuel

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0218278 A1
- Document ID: US20240218278A1
- Status: Published application
- Kind: A1
- Application number: 18/558,561
- Filed: 2022-05-25
- Published: 2024-07-04
- Earliest claimed: 2021-05-25
- Assignees: Subcoal International B.V.
- Applicants: Subcoal International B.V.
- Inventors: Lars JENNISSEN
- Web page: https://patentgrep.com/patent/US20240218278A1

## CPC

- C10L 5/46: on sewage, house, or town refuse {(C10L5/403, C10L5/406 take precedence)}
- C10L 5/08: without the aid of extraneous binders
- C10L 5/40: essentially based on materials of non-mineral origin
- C10L 5/406: {on plastic}
- C10L 5/442: {Wood or forestry waste}
- C10L 5/363: {Pellets or granulates}
- C10L 2250/04: Additive or component is a polymer
- C10L 2250/06: Particle, bubble or droplet size
- C10L 2290/28: Cutting, disintegrating, shredding or grinding
- C10L 2290/30: Pressing, compressing or compacting
- C10L 2290/52: Hoppers
- Y02E 50/10: Biofuels, e.g. bio-diesel
- Y02E 50/30: Fuel from waste, e.g. synthetic alcohol or diesel
- C10L: FUELS NOT OTHERWISE PROVIDED FOR; NATURAL GAS; SYNTHETIC NATURAL GAS OBTAINED BY PROCESSES NOT COVERED BY SUBCLASSES C10G OR C10K; LIQUIFIED PETROLEUM GAS; USE OF ADDITIVES TO FUELS OR FIRES; FIRE-LIGHTERS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention relates to a method to produce powdery alternative fuel by milling pellets, which pellets are produced by: (i) providing waste material comprising one or more thermoplastic material(s) of more than 40%, based on the total dry weight of the waste and one or more cellulosic material(s) of more than 30%, based on the total dry weight of the waste, wherein the waste has a particle size distribution with more than 80 wt % larger than 5 mm and more than 95 wt % smaller than 60 mm, having a water content of about 8 wt % or less; (ii) subjecting the waste material through a pelletiser with holes between 4-8 mm, and a length ratio of more than 10, such that the output temperature is about 85° C. or lower, (iii) subjecting the pellets through a second pelletiser with holes between 2 and 8 mm, and a length ratio of more than 14, such that the output temperature is about 110° C. or higher; (iv) to provide pellets, (v) and the pellets are cooled to a temperature of about 30° C. or lower. The powdery alternative fuel can be transported in bulk and through blowing lines.

## Claims

### Claim 1

A method to produce pellets comprising the following steps:
(i) providing waste material comprising one or more thermoplastic material(s) of more than 40%, based on the total dry weight of the waste and one or more cellulosic material(s) of more than 30%, based on the total dry weight of the waste, wherein the waste which is provided to step (ii) has a particle size distribution with more than 80 wt % larger than 5 mm and more than 95 wt % smaller than 60 mm, having a water content of about 8 wt % or less;
(ii) subjecting the waste material through a pelletiser with holes between 4-8 mm, and a length ratio of more than 10, such that the output temperature is about 85° C. or lower, (iii) subjecting the pellets through a second pelletiser with holes between 2 and 8 mm, and a length ratio of more than 14, such that the output temperature is about 110° C. or higher;
(iv) to provide pellets with a diameter between 2 and 8 mm, and a length of about 3 mm or longer, wherein the output temperature of the pellets is in a range 110-130° C.; and
(v) cooling the pellets are cooled to a temperature of about 40° C. or lower.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the moisture content of the material fed to the first die is between about 2% and about 5%.

### Claim 3 (depends on 1)

The method according to claims 1, wherein the hole diameter in the first and/or second pelletizer is 4-6 mm.

### Claim 4 (depends on 1)

The method according to claim 1, wherein the diameter to thickness ratio of the first die is between 10-16.

### Claim 5 (depends on 1)

The method according to claim 1 any one of claims 1, wherein the diameter to thickness ratio of the second die is between 14 and 20.

### Claim 6 (depends on 1)

The method according to claim 1, wherein the first die is operated such that the temperature of the output is between 60 and 80° C.

### Claim 7 (depends on 1)

The method according claim 1, wherein the second die is operated such that the temperature of the output is between 115-125° C.

### Claim 8 (depends on 1)

The method according to claim 1, wherein the temperature increase of the output of the first die and the output of the second die is about 40° C. or more.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the temperature of the material fed to the first die is between about 30-50° C.

### Claim 10 (depends on 1)

The method according to claim 1, wherein the temperature of the material fed to the second die is between about 50-80° C.

### Claim 11 (depends on 1)

A method for providing powdery alternative fuel by milling pellets obtainable by the method of claim 1.

### Claim 12 (depends on 11)

The method according to claim 11, wherein milling is performed in a hammer mill, jet mill, roller or ball mil.

### Claim 13

A powdery alternative fuel, having the following properties:
a. a mixture of 40-70 wt % thermoplastic material and 30-50 wt % of one or more cellulosic materials, which is preferably substantially homogeneous;
b. a particle size distribution such that more than 50 wt % of the particles is between 1 and 3.5 mm, while more than 60 wt % is smaller than 2 mm;
c. an angle of repose between 41-43°; and
d. a bulk density (tapped) of 220 g/L or higher.

### Claim at position 14

14-15. (canceled)

### Claim 16 (depends on 1)

The method of claim 1, wherein the first die is operated such that the temperature of the output is between 60 and 80° C., wherein the second die is operated such that the temperature of the output is between 115-125° C., and wherein the temperature increase of the output of the first die and the output of the second die is about 40° C. or more.

### Claim 17 (depends on 16)

The method according to claim 16, wherein the temperature of the material fed to the first die is between about 30-50° C.