# US 2024/0216949 A1 · Abrasion-resistant, stable and flame-resistant superhydrophobic/superoleophobic coating, and preparation and application thereof

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0216949 A1
- Document ID: US20240216949A1
- Status: Published application
- Kind: A1
- Application number: 17/998,164
- Filed: 2022-05-20
- Published: 2024-07-04
- Earliest claimed: 2021-05-31
- Assignees: Qilu University of Technology; Zhuhai Tairan Technology Co. Ltd.
- Applicants: Qilu University of Technology; Zhuhai Tairan Technology Co., Ltd.
- Inventors: Libin LIU; Qing BAN; Haihui JIANG; XingXiang JI; Furong TAO; Ligang GAI; Hailong ZHANG; Xinyu BU
- Web page: https://patentgrep.com/patent/US20240216949A1

## CPC

- B05D 5/08: to obtain an anti-friction or anti-adhesive surface (rendering particulate materials free-flowing in general, e.g. making them hydrophobic B01J2/30)
- B05D 1/02: performed by spraying
- B05D 3/0272: {with ovens}
- B05D 7/24: for applying particular liquids or other fluent materials
- C09D 5/18: Fireproof paints {including high temperature resistant paints}
- C09D 7/61: inorganic
- C09D 7/63: organic
- C09D 163/00: Coating compositions based on epoxy resins; Coating compositions based on derivatives of epoxy resins
- C09D 183/06: containing silicon bound to oxygen-containing groups (C09D183/12 takes precedence)
- C09D 183/08: containing silicon bound to organic groups containing atoms other than carbon, hydrogen, and oxygen
- B05D 3/0254: {After-treatment}
- B05D 2201/02: Polymeric substrate
- B05D 2203/35: Glass
- B05D 2301/30: Acids
- B05D 2401/20: Aqueous dispersion or solution
- B05D 2504/00: Epoxy polymers
- B05D 2518/10: Silicon-containing polymers
- B05D 2601/22: Silica
- B05D 2602/00: Organic fillers
- C08G 77/24: halogen-containing groups
- B05D: PROCESSES FOR APPLYING FLUENT MATERIALS TO SURFACES, IN GENERAL (conveying articles or workpieces through baths of liquid B65G, e.g. B65G49/02)
- C09D: COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS; FILLING PASTES; CHEMICAL PAINT OR INK REMOVERS; INKS; CORRECTING FLUIDS; WOODSTAINS; PASTES OR SOLIDS FOR COLOURING OR PRINTING; USE OF MATERIALS THEREFOR (cosmetics A61K; processes for applying liquids or other fluent materials to surfaces, in general, B05D; staining wood B27K5/02; glazes or vitreous enamels C03C; natural resins, French polish, drying-oils, driers, turpentine, per se, C09F; polishing compositions other than French polish, ski waxes C09G; adhesives or use of materials as adhesives C09J; materials for sealing or packing joints or covers C09K3/10; materials for stopping leaks C09K3/12; processes for the electrolytic or electrophoretic production of coatings C25D)
- C08G: MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS

## Abstract

Provided are an abrasion-resistant, stable and flame-resistant superhydrophobic/superoleophobic coating, and a preparation and application thereof, belonging to the field of new materials; the preparation includes: taking a superhydrophobic/superoleophobic suspension as a top-layer spraying solution; dispersing epoxy resin in a solvent, and adding a fluorine-containing curing agent and a flame retardant for reaction to obtain a bottom-layer spraying solution; and first spraying the bottom-layer spraying solution to a surface of a substrate, then spraying the top-layer spraying solution, and drying the surface to obtain a bilayer abrasion-resistant superhydrophobic flame-resistant coating; the superhydrophobic/superoleophobic suspension contains multi-level micro nano structural particles, a fluorine-containing curing agent and fluorinated epoxy resin; the prepared single-layer coating and bilayer structure (BLC) have hydrophobicity, flame resistance, good mechanical properties and excellent corrosion resistance performance.

## Claims

### Claim 1

A preparation method for a superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material, comprising:
spraying a superhydrophobic/superoleophobic suspension onto a surface of a horizontally placed substrate with a spray gun at a distance of 15 cm in a vertical direction, and then drying the surface in an oven at 120° C. for 6 h; and finally obtaining the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material, wherein
a preparation method for the superhydrophobic/superoleophobic suspension comprises the following steps:
S1, dispersing 15 nm SiO2, 50 nm SiO2 and 25 μm α-cellulose in a mixed solution containing anhydrous ethanol and ammonia, and performing ultrasonic treatment for 30 min;
S2, dropwise adding tetraethyl orthosilicate and perfluorooctane trimethoxy silane to the solution formed in step S1, and stirring the same for 6 h in a water bath at 60° C. to obtain solution A;
S3, dissolving bisphenol A epoxy resin in the anhydrous ethanol solution, and performing ultrasonic oscillation for 30 min to obtain solution B;
S4, adding solution B to solution A in the water bath at 60° C.; after full mixing, quickly injecting the tetraethyl orthosilicate and the perfluorooctane trimethoxy silane into the suspension; and stirring the same at 60° C. for 2 h to obtain solution C, a volume ratio of solution B to solution A being solution A: solution B=8:1;
S5, adding a fluorine-containing curing agent into anhydrous ethanol, and dissolving the fluorine-containing curing agent with ultrasonic waves to obtain solution D; and
S6, adding solution D into solution C, and stirring the same for 20 min; and after full mixing, adding a flame retardant, and stirring the same to obtain a final uniform solution, a volume ratio of solution D to solution C being solution C: solution D=48:5, and the flame retardant being 9,10-dihydro-9-oxa-10-phosphophenanthrene-10-oxide (DOOP);
a preparation method for the fluorine-containing curing agent comprises the following steps:
1) respectively dissolving heptafluorobutyric acid and 3-(2-aminoethylamino) propyltrimethoxysilane in deionized water;
2) dropwise adding the heptafluorobutyric acid solution to the 3-(2-aminoethylamino) propyltrimethoxysilane solution; and
3) after the dropwise adding is completed, heating the solution to obtain light yellow colloid which is a fluorine-containing curing agent.

### Claim 2 (depends on 1)

The preparation method for the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 1, wherein the substrate is glass, PU foam or a PVC film.

### Claim 3 (depends on 1)

The preparation method for the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 1, wherein in step 3), the reaction was performed by heating at 100° C.

### Claim 4 (depends on 1)

The preparation method for the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 1, wherein in step S1, in the mixed solution of absolute ethanol and ammonia water, a volume ratio of the absolute ethanol to the ammonia water is (1-5):1.

### Claim 5 (depends on 4)

The preparation method for the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 4, wherein in step S1, the volume ratio of the anhydrous ethanol to the ammonia water is 3:1.

### Claim 6 (depends on 1)

The preparation method for the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 1, wherein in step S1, a mass ratio of the 15 nm SiO2, 50 nm SiO2 and 25 μm α-cellulose is 1:1:2.

### Claim 7 (depends on 1)

The preparation method for the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 1, wherein in step S2, a volume ratio of the tetraethyl orthosilicate to the perfluorooctane trimethoxy silane is 2:1.

### Claim 8 (depends on 1)

The preparation method for a superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 1, wherein in step S4, a volume ratio of the tetraethyl orthosilicate to the perfluorooctane trimethoxy silane is 1:1.

### Claim 9 (depends on 1)

The preparation method for the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 1, wherein in step S6, the amount of the DOPO is 1-6% of the total mass of the raw materials.

### Claim 10 (depends on 1)

The preparation method for the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 1, wherein the amount of 15 nm SiO2 is 25% of the total mass of the 15 nm SiO2, the 50 nm SiO2 and the 25 μm α-cellulose, and the content of the DOPO is 6%.

### Claim 11 (depends on 1)

The preparation method for the superhydrophobic/superoleophobic flame-resistant and abrasion-resistant coating material according to claim 1, wherein a mass ratio of the bisphenol A epoxy resin to the fluorine-containing curing agent is 1:1.066.

### Claim 12

(canceled)

### Claim 13

(canceled)