# US 2024/0208839 A1 · Lithium niobate solution and method for producing same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0208839 A1
- Document ID: US20240208839A1
- Status: Published application
- Kind: A1
- Application number: 18/289,477
- Filed: 2022-03-10
- Published: 2024-06-27
- Earliest claimed: 2021-04-28
- Assignees: Mitsui Mining & Smelting Co., Ltd.
- Applicants: Mitsui Mining & Smelting Co., Ltd.
- Inventors: Ryuji MOTONO; Syuhei HARA; Daiki ARAKAWA
- Web page: https://patentgrep.com/patent/US20240208839A1

## CPC

- C01G 33/003: {Preparation involving a liquid-liquid extraction, an adsorption or an ion-exchange}
- H01M 4/58: of inorganic compounds other than oxides or hydroxides, e.g. sulfides, selenides, tellurides, halogenides or LiCoFy; of polyanionic structures, e.g. phosphates, silicates or borates
- C01G 33/00: Compounds of niobium
- H01M 4/36: Selection of substances as active materials, active masses, active liquids
- H01M 4/366: {as layered products}
- H01M 4/485: of mixed oxides or hydroxides for inserting or intercalating light metals, e.g. LiTi2O4 or LiTi2OxFy (H01M4/505, H01M4/525 take precedence)
- H01M 4/505: of mixed oxides or hydroxides containing manganese for inserting or intercalating light metals, e.g. LiMn2O4 or LiMn2OxFy
- H01M 4/525: of mixed oxides or hydroxides containing iron, cobalt or nickel for inserting or intercalating light metals, e.g. LiNiO2, LiCoO2 or LiCoOxFy
- H01M 4/62: Selection of inactive substances as ingredients for active masses, e.g. binders, fillers
- H01M 10/052: Li-accumulators
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2004/51: Particles with a specific particle size distribution
- C01P 2004/64: Nanometer sized, i.e. from 1-100 nanometer
- C01P 2006/40: Electric properties
- C01P 2006/80: Compositional purity
- H01M 2004/028: {Positive electrodes}
- Y02E 60/10: Energy storage using batteries
- C01G: COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSES C01D OR C01F (metal hydrides {monoborane, diborane or addition complexes thereof} C01B6/00; salts of oxyacids of halogens C01B11/00; peroxides, salts or peroxyacids C01B15/00; thiosulfates, dithionites, polythionates C01B17/64; compounds containing selenium, or tellurium C01B19/00; binary compounds of nitrogen with metals C01B21/06; azides C01B21/08; {compounds containing nitrogen, other non-metals and metal C01B21/082}; metal amides C01B21/092; nitrites C01B21/50; {compounds of noble gases C01B23/0005}; phosphides C01B25/08; salts of oxyacids of phosphorus C01B25/16; carbides C01B32/90; compounds containing silicon C01B33/00; compounds containing boron C01B35/00; compounds having molecular sieve properties but not having base-exchange properties C01B37/00; compounds having molecular sieve and base-exchange properties, e.g. crystalline zeolites, C01B39/00; cyanides C01C3/08; salts of cyanamide C01C3/16; thiocyanates C01C3/20)
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

A lithium niobate solution is provided containing lithium niobate having a molar ratio of lithium and niobium Li/Nb of 0.8 or more and 2.0 or less and ammonium ions, and the particle size (D50) of the lithium niobate in the lithium niobate solution according to dynamic light scattering is 100 nm or less. A method for producing a lithium niobate solution is also provided and has a step of producing an acidic niobium solution containing niobium, a step of obtaining a precipitate slurry containing niobium by inverse neutralization by adding the acidic niobium solution to ammonia water and a step of obtaining a lithium niobate solution by maintaining a mixture of the precipitate slurry containing niobium and lithium hydroxide at 20° C. to 100° C. with stirring.

## Claims

### Claim at position 1

1-13. (canceled)

### Claim 14

A lithium niobate solution comprising:
lithium niobate having a molar ratio of lithium and niobium Li/Nb of 0.8 or more and 2.0 or less; and
ammonium ions,
wherein the particle size (D50) of the lithium niobate in the lithium niobate solution according to dynamic light scattering is 100 nm or less.

### Claim 15 (depends on 14)

The lithium niobate solution according to claim 14, wherein hydrogen peroxide is not contained in the lithium niobate solution.

### Claim 16 (depends on 14)

The lithium niobate solution according to claim 14, wherein the lithium niobate solution is an aqueous solution.

### Claim 17 (depends on 15)

The lithium niobate solution according to claim 15, wherein the lithium niobate solution is an aqueous solution.

### Claim 18 (depends on 14)

The lithium niobate solution according to claim 14, wherein the lithium niobate concentration of the lithium niobate solution is 0.1 to 30% by mass.

### Claim 19 (depends on 18)

The lithium niobate solution according claim 18, wherein the lithium niobate concentration of the lithium niobate solution is 5 to 20% by mass.

### Claim 20 (depends on 14)

The lithium niobate solution according to claim 14, wherein the particle size (D50) of the lithium niobate is 30 nm or less.

### Claim 21 (depends on 18)

The lithium niobate solution according claim 18, wherein the particle size (D50) of the lithium niobate is 30 nm or less.

### Claim 22 (depends on 19)

The lithium niobate solution according claim 19, wherein the particle size (D50) of the lithium niobate is 10 nm or less.

### Claim 23

A method for producing a lithium niobate solution comprising:
a step of producing an acidic niobium solution containing niobium;
a step of obtaining a precipitate slurry containing the niobium by inverse neutralization by adding the acidic niobium solution to ammonia water; and
a step of obtaining a lithium niobate solution by maintaining a mixture of the obtained precipitate slurry containing the niobium and lithium hydroxide at 20° C. to 100° C. with stirring.

### Claim 24 (depends on 23)

The method for producing a lithium niobate solution according to claim 23, wherein
the acidic niobium solution is an acidic niobium solution containing fluoride ions obtained by solvent extraction of a solution in which niobium is dissolved in an acidic solution containing hydrofluoric acid, and
that the method has a step of obtaining a niobium-containing precipitate by removing fluoride ions from the precipitate slurry containing the niobium,
a step of obtaining a lithium niobate solution by maintaining a mixture of the obtained niobium-containing precipitate and lithium hydroxide at 20° C. to 100° C. with stirring, and
a step of leaving the lithium niobate solution to cool to room temperature.

### Claim 25 (depends on 14)

A method for producing a cathode active material for a lithium-ion secondary cell coated with lithium niobate comprising:
a step of producing a cathode active material slurry for a cell containing lithium niobate by mixing the lithium niobate solution according to claim 14, a cathode active material and an aqueous lithium hydroxide solution; and
a step of drying the cathode active material slurry for a cell containing the lithium niobate.

### Claim 26 (depends on 15)

The lithium niobate solution according to claim 15, wherein the lithium niobate concentration of the lithium niobate solution is 0.1 to 30% by mass.

### Claim 27 (depends on 26)

The lithium niobate solution according claim 26, wherein the lithium niobate concentration of the lithium niobate solution is 5 to 20% by mass.

### Claim 28 (depends on 15)

The lithium niobate solution according to claim 15, wherein the particle size (D50) of the lithium niobate is 30 nm or less.

### Claim 29 (depends on 26)

The lithium niobate solution according claim 26, wherein the particle size (D50) of the lithium niobate is 30 nm or less.

### Claim 30 (depends on 27)

The lithium niobate solution according claim 27, wherein the particle size (D50) of the lithium niobate is 10 nm or less.

### Claim 31 (depends on 15)

A method for producing a cathode active material for a lithium-ion secondary cell coated with lithium niobate comprising:
a step of producing a cathode active material slurry for a cell containing lithium niobate by mixing the lithium niobate solution according to claim 15, a cathode active material and an aqueous lithium hydroxide solution; and
a step of drying the cathode active material slurry for a cell containing the lithium niobate.