# US 2024/0204246 A1 · Solid electrolyte composition excellent in stability against water and ion conductivity, and method for preparing the same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0204246 A1
- Document ID: US20240204246A1
- Status: Published application
- Kind: A1
- Application number: 18/534,858
- Filed: 2023-12-11
- Published: 2024-06-20
- Earliest claimed: 2022-12-14
- Assignees: Industry-Academic Cooperation Foundation of Sunchon National University; Industry Academy Cooperation Foundation of Sejong University
- Applicants: Industry-Academic Cooperation Foundation of Sunchon National University; Industry Academy Cooperation Foundation of Sejong University
- Inventors: Kee Sun SOHN; Myoung Ho PYO; Woon Bae PARK; Jung Yong SEO
- Web page: https://patentgrep.com/patent/US20240204246A1

## CPC

- H01M 10/0562: Solid materials
- H01M 10/052: Li-accumulators
- H01M 10/054: Accumulators with insertion or intercalation of metals other than lithium, e.g. with magnesium or aluminium
- H01M 2300/0068: inorganic
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

The invention relates to a solid electrolyte composition and a method for producing the same. The solid electrolyte composition according to the invention is characterized by including a material represented by [Formula 1] below. NaaZnbGacSd Formula 1 (wherein, 2.70≤a≤2.90, 0.70≤b≤0.90, and 1.10≤c≤1.30)

## Claims

### Claim 1

A solid electrolyte composition comprising a material represented by [Formula 1] below:
NaaZnbGacSd Formula 1
(wherein, 2.70≤a≤2.90, 0.70≤b≤0.90, and 1.10≤c≤1.30)

### Claim 2 (depends on 1)

The solid electrolyte composition according to claim 1, wherein the space group of the material represented by [Formula 1] above is I41/acd.

### Claim 3 (depends on 1)

The solid electrolyte composition according to claim 1, wherein the ion conductivity σion at room temperature (25° C.) of the material represented by [Formula 1] is at least 0.1 mScm−1.

### Claim 4 (depends on 1)

The solid electrolyte composition according to claim 1, wherein the material represented by [Formula 1] above is inert to water.

### Claim 5 (depends on 1)

The solid electrolyte composition according to claim 1, wherein in the material represented by [Formula 1] above, a is 2.75 to 2.85, b is 0.75 to 0.85, and c is 1.15 to 1.25.

### Claim 6 (depends on 1)

The solid electrolyte composition according to claim 1, wherein the material represented by [Formula 1] above is a tetragonal phase.

### Claim 7

A method for producing a solid electrolyte composition including a material represented by [Formula 1] below, the method comprising:
(a) mixing raw materials;
(b) heating the mixed materials to a predetermined temperature and maintaining the same for a predetermined period of time; and
(c) cooling the heated materials:
NaaZnbGacSd Formula 1
(wherein, 2.70≤a≤2.90, 0.70≤b≤0.90, and 1.10≤c≤1.30)

### Claim 8 (depends on 7)

The method according to claim 7, wherein the step (b) above is performed at 700° C. to 800° C. for 12 hours to 48 hours.