# US 2024/0204191 A1 · Synthetic graphite material, synthetic graphite material production method, negative electrode for lithium ion secondary battery, and lithium ion secondary battery

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0204191 A1
- Document ID: US20240204191A1
- Status: Published application
- Kind: A1
- Application number: 18/419,040
- Filed: 2024-01-22
- Published: 2024-06-20
- Earliest claimed: 2019-01-15
- Assignees: Eneos Corporation
- Applicants: Eneos Corporation
- Inventors: Takashi SUZUKI; Takashi Maeda; Mitsuo Karakane; Takahiro Shirai; Hiroshi Kawachi; Noriyuki Kiuchi
- Web page: https://patentgrep.com/patent/US20240204191A1

## CPC

- H01M 4/587: for inserting or intercalating light metals
- C01B 32/205: Preparation
- H01M 10/0525: Rocking-chair batteries, i.e. batteries with lithium insertion or intercalation in both electrodes; Lithium-ion batteries
- C01P 2002/60: Compounds characterised by their crystallite size
- C01P 2006/12: Surface area
- C01P 2006/19: Oil-absorption capacity, e.g. DBP values
- C01P 2006/40: Electric properties
- H01M 2004/021: {Physical characteristics, e.g. porosity, surface area}
- H01M 2004/027: {Negative electrodes}
- Y02E 60/10: Energy storage using batteries
- H01M: PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSION OF CHEMICAL ENERGY INTO ELECTRICAL ENERGY
- C01B: NON-METALLIC ELEMENTS; COMPOUNDS THEREOF; {METALLOIDS OR COMPOUNDS THEREOF NOT COVERED BY SUBCLASS C01C}
- C01P: INDEXING SCHEME RELATING TO STRUCTURAL AND PHYSICAL ASPECTS OF SOLID INORGANIC COMPOUNDS
- Y02E: REDUCTION OF GREENHOUSE GAS [GHG] EMISSIONS, RELATED TO ENERGY GENERATION, TRANSMISSION OR DISTRIBUTION

## Abstract

Provided is a synthetic graphite material, in which a size L (112) of a crystallite in a c-axis direction as calculated from a (112) diffraction line obtained by an X-ray wide angle diffraction method is in a range of 4 to 30 nm, a surface area based on a volume as calculated by a laser diffraction type particle size distribution measuring device is in a range of 0.22 to 1.70 m2/cm3, an oil absorption is in a range of 67 to 147 mL/100 g, and a nitrogen adsorption specific surface area is in a range of 3.1 to 8.2 m2/g.

## Claims

### Claim 1

A production method of the synthetic graphite material, comprising at least:
a step of performing a coking treatment on a raw material oil composition by performing a delayed coking process to generate a raw coke composition;
a step of pulverizing the raw coke composition to obtain heat-treated raw coke powder;
a step of performing a heat treatment on the heat-treated raw coke powder to obtain graphite powder; and
a step of pulverizing the graphite powder,
wherein the synthetic graphite material has:
a size L (112) of a crystallite in a c-axis direction as calculated from a (112) diffraction line obtained by an X-ray wide angle diffraction method being in a range of 4 to 30 nm,
a surface area based on a volume as calculated by a laser diffraction type particle size distribution measuring device being in a range of 0.22 to 1.70 m2/cm3,
an oil absorption being in a range of 67 to 147 mL/100 g, and
a nitrogen adsorption specific surface area being in a range of 3.1 to 8.2 m2/g.

### Claim 2 (depends on 1)

The production method according to claim 1,
wherein the raw material oil composition has a normal paraffin content of 5 to 20% by mass, and
an aromatic index fa acquired by a Knight method is in a range of 0.3 to 0.65.