# US 2024/0204128 A1 · High voltage and high-power diamond based junction-gate field effect transistor (jfet) switch with photo-controlled gate

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0204128 A1
- Document ID: US20240204128A1
- Status: Published application
- Kind: A1
- Application number: 18/428,200
- Filed: 2024-01-31
- Published: 2024-06-20
- Earliest claimed: 2022-10-05
- Applicants: Lawrence Livermore National Security, LLC
- Inventors: Qinghui Shao; Lars F. Voss; Soroush Ghandiparsi
- Web page: https://patentgrep.com/patent/US20240204128A1

## CPC

- H10F 30/2863: {Field-effect phototransistors having PN homojunction gates}
- H10F 77/122: comprising only Group IV materials
- H10F 77/306: {for devices having potential barriers}
- H10F 77/334: {for shielding light, e.g. light blocking layers or cold shields for infrared detectors}
- H10F: INORGANIC SEMICONDUCTOR DEVICES SENSITIVE TO INFRARED RADIATION, LIGHT, ELECTROMAGNETIC RADIATION OF SHORTER WAVELENGTH OR CORPUSCULAR RADIATION

## Abstract

Devices, methods and techniques related to high voltage and high-power diamond transistors are disclosed. In one example aspect, a switch operable under high-voltage and high-power includes a P-type diamond layer doped with an acceptor material and an N-type diamond region doped with a donor material. The P-type diamond layer is at least partially embedded the N-type diamond region. The switch includes a layer comprising one or more apertures configured to allow illumination from a light source to pass through to reach the N-type diamond region, a source contact and a drain contact that are at least partially in contact with the P-type diamond layer; and a gate in contact with at least an area of the N-type diamond region.

## Claims

### Claim 1

A switch operable under high-voltage and high-power, comprising:
an N-type diamond region doped with a donor material;
a P-type diamond layer doped with an acceptor material and at least partially positioned within the N-type diamond region;
one or more apertures configured to allow illumination from a light source to reach an internal region of the switch;
a source contact and a drain contact that are at least partially in contact with the P-type diamond layer; and
a gate in contact with at least an area of the N-type diamond region, wherein the N-type diamond region, upon receiving the illumination and application of a first bias voltage, is configured to generate a conduction current that remains on in an absence of the illumination.

### Claim 2 (depends on 1)

The switch of claim 1, wherein the P-type diamond layer is positioned in one or more trenches in the N-type diamond region such that a bottom surface and at least part of side surfaces of the P-type diamond layer are in contact with the N-type diamond region.

### Claim 3 (depends on 2)

The switch of claim 2, wherein each of the side surfaces in its entirety is in contact with the N-type diamond region.

### Claim 4 (depends on 1)

The switch of claim 1, wherein the P-type diamond layer is positioned in one or more trenches in the N-type diamond region such that all surfaces of the P-type diamond layer are in contact with N-type diamond.

### Claim 5 (depends on 1)

The switch of claim 1, wherein the donor material comprises nitrogen, and wherein the acceptor material comprises boron.

### Claim 6 (depends on 1)

The switch of claim 1, further comprising:
a passivation layer in contact with the N-type diamond region and the gate.

### Claim 7 (depends on 1)

The switch of claim 1, further comprising:
a passivation layer; and
a contact layer between the passivation layer and the N-type diamond region, the contact layer comprising a doped P+ diamond layer.

### Claim 8 (depends on 1)

The switch of claim 1, wherein a thickness of the P-type diamond layer is between 0.1 um to 10 μm.

### Claim 9 (depends on 1)

The switch of claim 1, configured to switch between an ON state having the conduction current and an OFF state within 1 us upon an intensity of the illumination from the light source is in a range of 5 to 15 W/cm2.

### Claim 10 (depends on 1)

The switch of claim 1, comprising:
one or more gradient masks surrounding the one or more apertures and a light blocking material.

### Claim 11 (depends on 10)

The switch of claim 10, wherein the one or more gradient masks comprise at least one of:
a gradually increasing thickness from the one or more apertures towards the source contact or the drain contact, or
a material having a gradually changing absorption coefficient.

### Claim 12

A switch operable under high-voltage and high-power, comprising:
a P-type diamond layer doped with an acceptor material;
an N-type diamond region doped with a donor material, wherein the P-type diamond layer is at least partially in contact with the N-type diamond region;
a layer comprising an aperture configured to allow illumination from a light source to pass through to reach the N-type diamond region; and
one or more gradient masks at least partially surrounding the aperture from multiple sides to allow variable absorption or transmission of illumination from the light source to reach an internal region of the switch;
wherein the N-type diamond region, upon receiving the illumination and application of a first bias voltage, is configured to generate a conduction current that remains on in an absence of the illumination.

### Claim 13 (depends on 12)

The switch of claim 12, wherein at least one of the one or more gradient masks has a geometrical structure with a variable thickness that monotonically increases away from the aperture.

### Claim 14 (depends on 12)

The switch of claim 12, wherein at least one of the one or more gradient masks comprises a step-shaped geometry to obtain a gradual increase of light absorption away from the aperture.

### Claim 15 (depends on 12)

The switch of claim 12, wherein at least one of the one or more gradient masks comprises a material having a gradually changing absorption coefficient to obtain a gradual increase of light absorption away from the aperture.

### Claim 16 (depends on 12)

The switch of claim 12, wherein gradient masks are positioned to fully surround the aperture such that a gradually reduced electron concentration is formed around where the illumination interfaces the N-type diamond region and the P-type diamond layer.

### Claim 17 (depends on 12)

The switch of claim 12, wherein the donor material comprises nitrogen, and wherein the acceptor material comprises boron.

### Claim 18 (depends on 12)

The switch of claim 12, wherein a thickness of the P-type diamond layer is between 0.1 um to 10 um.

### Claim 19 (depends on 12)

The switch of claim 12, further comprising:
a passivation layer; and
a contact layer between the passivation layer and the N-type diamond region, the contact layer comprising a doped P+ diamond layer.

### Claim 20 (depends on 12)

The switch of claim 12, configured to switch between an ON state having the conduction current and an OFF state within 1 us upon an intensity of the illumination from the light source is in a range of 5 to 15 W/cm2.

### Claim 21 (depends on 12)

The switch of claim 12, wherein the one or more gradient masks are positioned to partially surround the aperture such that a gradually reduced electron concentration is formed along one side of where the illumination interfaces the N-type diamond region and the P-type diamond layer.

### Claim 22 (depends on 12)

The switch of claim 12, wherein a bottom surface of the P-type diamond layer is in contact with the N-type diamond region.