# US 2024/0203745 A1 · Silicon wafer manufacturing method

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0203745 A1
- Document ID: US20240203745A1
- Status: Published application
- Kind: A1
- Application number: 18/286,691
- Filed: 2022-03-16
- Published: 2024-06-20
- Earliest claimed: 2021-04-21
- Assignees: Shin-Etsu Handotai Co., Ltd.
- Applicants: Shin-Etsu Handotai Co., Ltd.
- Inventors: Tatsuo ABE; Yuki TANAKA
- Web page: https://patentgrep.com/patent/US20240203745A1

## CPC

- H10P 52/00: Grinding, lapping or polishing of wafers, substrates or parts of devices
- H10P 50/242: {of Group IV materials}
- H10P 90/126: {by chemical etching}
- H10P 90/129: {by polishing}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

The present invention is a silicon wafer manufacturing method including a grinding step of grinding front and back surfaces of a raw wafer to obtain a wafer having an arithmetic surface roughness Sa per 2 μm2 of 10 nm or less; a dry-etching step of subjecting the wafer obtained in the grinding step to isotropic whole-surface dry-etching with an etching removal of 1 μm or less per surface to remove a mechanically damaged layer introduced into each of front and back surfaces of the wafer in the grinding step; and a double-side polishing step of, after the dry-etching step, polishing both surfaces of the wafer with a stock removal of 3 μm or less per surface. Thus, the silicon wafer manufacturing method that enables to manufacture a wafer having high flatness can be provided.

## Claims

### Claim 1

A silicon wafer manufacturing method comprising:
a grinding step of grinding front and back surfaces of a raw wafer to obtain a wafer having an arithmetic surface roughness Sa per 2 μm2 of 10 nm or less;
a dry-etching step of subjecting the wafer obtained in the grinding step to isotropic whole-surface dry-etching with an etching removal of 1 μm or less per surface to remove a mechanically damaged layer introduced into each of front and back surfaces of the wafer in the grinding step; and
a double-side polishing step of, after the dry-etching step, polishing both surfaces of the wafer with a stock removal of 3 μm or less per surface.

### Claim 2 (depends on 1)

The silicon wafer manufacturing method according to claim 1, wherein in the dry-etching step, an etching rate is 0.3 μm/min or less.

### Claim 3 (depends on 1)

The silicon wafer manufacturing method according to claim 1, wherein in the dry-etching step, a front-and-back surfaces oxidation treatment with ozone gas is performed as a pre-treatment of the isotropic whole-surface dry-etching.

### Claim 4 (depends on 2)

The silicon wafer manufacturing method according to claim 2, wherein in the dry-etching step, a front-and-back surfaces oxidation treatment with ozone gas is performed as a pre-treatment of the isotropic whole-surface dry-etching.

### Claim 5 (depends on 1)

The silicon wafer manufacturing method according to claim 1, wherein in the dry-etching step, a front-and-back surfaces oxidation treatment with ozone gas is performed as a post-treatment of the isotropic whole-surface dry-etching.

### Claim 6 (depends on 2)

The silicon wafer manufacturing method according to claim 2, wherein in the dry-etching step, a front-and-back surfaces oxidation treatment with ozone gas is performed as a post-treatment of the isotropic whole-surface dry-etching.

### Claim 7 (depends on 3)

The silicon wafer manufacturing method according to claim 3, wherein in the dry-etching step, a front-and-back surfaces oxidation treatment with ozone gas is performed as a post-treatment of the isotropic whole-surface dry-etching.

### Claim 8 (depends on 4)

The silicon wafer manufacturing method according to claim 4, wherein in the dry-etching step, a front-and-back surfaces oxidation treatment with ozone gas is performed as a post-treatment of the isotropic whole-surface dry-etching.