# US 2024/0203742 A1 · Contact layer formation with microwave annealing for nmos devices

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0203742 A1
- Document ID: US20240203742A1
- Status: Published application
- Kind: A1
- Application number: 18/387,732
- Filed: 2023-11-07
- Published: 2024-06-20
- Earliest claimed: 2022-12-14
- Assignees: Applied Materials, Inc.
- Applicants: Applied Materials, Inc.
- Inventors: Nicolas Louis BREIL; Wolfgang R. ADERHOLD; Shashank SHARMA; Nilay Anil PRADHAN
- Web page: https://patentgrep.com/patent/US20240203742A1

## CPC

- H10P 14/432: {using selective deposition}
- H01J 37/32357: {Generation remote from the workpiece, e.g. down-stream}
- H10D 64/0112: {using conductive layers comprising silicides}
- H10P 70/27: {during, before or after processing of conductive materials, e.g. polysilicon or amorphous silicon layers}
- H10W 20/033: {in openings in dielectrics}
- H10W 20/081: {by forming openings in the dielectric parts}
- H01J 37/321: {the radio frequency energy being inductively coupled to the plasma}
- H01J 2237/335: Cleaning
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)
- H10D: INORGANIC ELECTRIC SEMICONDUCTOR DEVICES
- H10W: GENERIC PACKAGES, INTERCONNECTIONS, CONNECTORS OR OTHER CONSTRUCTIONAL DETAILS OF DEVICES COVERED BY CLASS H10

## Abstract

A method of forming an electrical contact in semiconductor structure includes performing a selective deposition process on a semiconductor structure having a semiconductor region and a dielectric layer having a trench therewithin, the selective deposition process comprising epitaxially forming a contact layer on the semiconductor region within the trench of the dielectric layer, and performing a microwave anneal process to activate dopants in the epitaxially formed contact layer.

## Claims

### Claim 1

A method of forming an electrical contact in semiconductor structure, comprising:
performing a selective deposition process on a semiconductor structure having a semiconductor region and a dielectric layer having a trench therewithin, the selective deposition process comprising epitaxially forming a contact layer on the semiconductor region within the trench of the dielectric layer; and
performing a microwave anneal process to activate dopants in the epitaxially formed contact layer.

### Claim 2 (depends on 1)

The method of claim 1, wherein
the selective deposition process and the microwave anneal process are performed without breaking vacuum environment.

### Claim 3 (depends on 1)

The method of claim 1, wherein
the semiconductor region comprises silicon doped with n-type dopants, and
the contact layer comprises silicon doped with n-type dopants.

### Claim 4 (depends on 3)

The method of claim 3, wherein
the contact layer comprises silicon doped with phosphorous (P) with a concentration of between 1019 cm−3 and 5·×1021 cm−3.

### Claim 5 (depends on 1)

The method of claim 1, wherein
the selective deposition process is performed at a temperature of between 200° C. and 800° C.

### Claim 6 (depends on 1)

The method of claim 1, further comprising:
prior to the selective deposition process,
performing a pre-clean process to remove contaminants formed on a exposed surface of the semiconductor region within the trench; and
performing a cavity shaping process to form a cavity on the exposed surface of the semiconductor region within the trench.

### Claim 7 (depends on 1)

The method of claim 1, further comprising:
subsequent to the microwave anneal process,
performing a blanket deposition process to form a metal layer on the contact layer; and
performing a metal fill process to form a contact plug in the trench.

### Claim 8

A method of forming an electrical contact in semiconductor structure, comprising:
performing a pre-clean process on a semiconductor structure having a semiconductor region and a dielectric layer having a trench therewithin, the pre-clean process comprising removing contaminants formed on an exposed surface of the semiconductor region within the trench;
performing a cavity shaping process to form a cavity on the exposed surface of the semiconductor region within the trench;
performing a selective deposition process, the selective deposition process comprising epitaxially forming a contact layer in the cavity in the semiconductor region within the trench of the dielectric layer; and
performing a microwave anneal process to activate dopants in the epitaxially formed contact layer.

### Claim 9 (depends on 8)

The method of claim 8, wherein
the pre-clean process, the cavity shaping process, the selective deposition process, and the microwave anneal process are performed without breaking vacuum environment.

### Claim 10 (depends on 8)

The method of claim 8, wherein
the semiconductor region comprises silicon doped with n-type dopants, and
the contact layer comprises silicon doped with n-type dopants.

### Claim 11 (depends on 10)

The method of claim 10, wherein
the contact layer comprises silicon doped with phosphorous (P) with a concentration of between 1019 cm−3 and 5·×1021 cm−3.

### Claim 12 (depends on 8)

The method of claim 8, wherein
the selective deposition process is performed at a temperature of between 200° C. and 800° C.

### Claim 13 (depends on 8)

The method of claim 8, further comprising:
subsequent to the microwave anneal process,
performing a blanket deposition process to form a metal layer on the contact layer; and
performing a metal fill process to form a contact plug in the trench.

### Claim 14

A processing system, comprising:
a first processing chamber;
a second processing chamber; and
a system controller configured to cause the processing system to:
perform, in the first processing chamber, a selective deposition process on a semiconductor structure having a semiconductor region and a dielectric layer having a trench therewithin, the selective deposition process comprising epitaxially forming a contact layer on the semiconductor region within the trench of the dielectric layer; and
perform, in the second processing chamber, a microwave anneal process to activate dopants in the epitaxially formed contact layer.

### Claim 15 (depends on 14)

The processing system of claim 14, wherein
the semiconductor region comprises silicon doped with n-type dopants, and
the contact layer comprises silicon doped with n-type dopants.

### Claim 16 (depends on 15)

The processing system of claim 15, wherein
the contact layer comprises silicon doped with phosphorous (P) with a concentration of between 1019 cm−3 and 5·×1021 cm−3.

### Claim 17 (depends on 14)

The processing system of claim 14, wherein
the selective deposition process is performed at a temperature less of between 200° C. and 800° C.

### Claim 18 (depends on 14)

The processing system of claim 14, further comprising:
a third processing chamber; and
a fourth processing chamber, wherein the system controller is further configured to cause the processing system to:
prior to the selective deposition process,
perform, in the third processing chamber, a pre-clean process to remove contaminants formed on a exposed surface of the semiconductor region within the trench; and
perform, in the fourth processing chamber, a cavity shaping process to form a cavity on the exposed surface of the semiconductor region within the trench.

### Claim 19 (depends on 18)

The processing system of claim 18, further comprising:
a fifth processing chamber; and
a sixth processing chamber, wherein the system controller is frther configured to cause the processing system to:
subsequent to the microwave anneal process,
perform, in the fifth processing chamber, a blanket deposition process to form a metal layer on the contact layer; and
perform, in the sixth processing chamber, a metal fill process to form a contact plug in the trench.

### Claim 20 (depends on 14)

The processing system of claim 14, wherein the system controller is further configured to cause the processing system to perform the selective deposition process and the microwave anneal process without breaking vacuum environment.