# US 2024/0203731 A1 · Method of manufacturing an electronic device

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0203731 A1
- Document ID: US20240203731A1
- Status: Published application
- Kind: A1
- Application number: 18/537,875
- Filed: 2023-12-13
- Published: 2024-06-20
- Earliest claimed: 2022-12-19
- Assignees: Commissariat à I'Énergie Atomique et aux Énergies Alternatives
- Applicants: Commissariat à I'Énergie Atomique et aux Énergies Alternatives
- Inventors: Rémy Gassilloud; Julien Patouillard; Bérangére Hyot; Amélie Dussaigne; Stéphane Cadot; Matthew Charles; François Martin; Nicolas Gauthier; Christine Raynaud
- Web page: https://patentgrep.com/patent/US20240203731A1

## CPC

- H10P 14/3236: {being chalcogenide semiconducting materials not being oxides, e.g. ternary compounds}
- H10P 14/3416: {Nitrides}
- H10P 14/22: using physical deposition, e.g. vacuum deposition or sputtering
- H10P 14/3251: {consisting of three or more layers}
- H10P 14/3408: {Silicon carbide}
- H10P 14/3436: {being chalcogenide semiconductor materials not being oxides, e.g. ternary compounds}
- H10P 14/3446: {Transition metal elements; Rare earth elements}
- H10P 14/38: {characterised by treatments done after the formation of the materials}
- H10P 14/3802: {Crystallisation or recrystallisation of non-monocrystalline semiconductor materials, e.g. regrowth}
- H10P 14/24: using chemical vapour deposition [CVD]
- H10P 14/2905: {Silicon, silicon germanium or germanium}
- H10P 14/3256: {Microstructure}
- H10P: GENERIC PROCESSES OR APPARATUS FOR THE MANUFACTURE OR TREATMENT OF DEVICES COVERED BY CLASS H10

## Abstract

A method including the following successive steps: a) forming, on a surface of a support substrate, a first layer made of a material selected from among a lamellar dichalcogenide or a lamellar chalcogenide including a stack of sheets; b) forming, by physical vapor deposition on the side of said surface of the support substrate, a second layer made of a first III-N semiconductor material coating the first layer; and c) carrying out a thermo-chemical treatment of the first layer resulting, in the first layer, in a conversion of van der Waals bonds between the sheets of the first layer into covalent bonds.

## Claims

### Claim 1

Method comprising the following successive steps:
a) forming, on a surface of a support substrate, a first layer made of a material selected from among a lamellar dichalcogenide or a lamellar chalcogenide comprising a stack of sheets;
b) forming, by physical vapor deposition on the side of said surface of the support substrate, a second layer made of a first III-N semiconductor material coating the first layer; and
c) carrying out a thermo-chemical treatment of the first layer resulting, in the first layer, in a conversion of van der Waals bonds between the sheets of the first layer into covalent bonds.

### Claim 2 (depends on 1)

Method according to claim 1, wherein, at step c), the thermo-chemical treatment is an anneal carried out under a reducing atmosphere.

### Claim 3 (depends on 1)

Method according to claim 1, wherein, at step c), the thermo-chemical treatment is carried out under a nitrogenous atmosphere, preferably under an ammonia or nitrogen atmosphere.

### Claim 4 (depends on 1)

Method according to claim 1, wherein, at step c), the thermo-chemical treatment is carried out under a hydrogen atmosphere.

### Claim 5 (depends on 1)

Method according to claim 1, wherein, at step c), the thermo-chemical treatment further results in a conversion of van der Waals bonds into covalent bonds between the first layer and the support substrate.

### Claim 6 (depends on 1)

Method according to claim 1, wherein the first semiconductor material is aluminum nitride.

### Claim 7 (depends on 1)

Method according to claim 1, wherein the first III-N semiconductor material is doped, preferably with scandium atoms.

### Claim 8 (depends on 1)

Method according to claim 1, further comprising, after step c), a step d) of forming of a third layer made of a second semiconductor material coating the second layer, the third layer having a thickness greater than that of the second layer.

### Claim 9 (depends on 8)

Method according to claim 8, wherein the second semiconductor material is a III-V, preferably III-N, semiconductor material.

### Claim 10 (depends on 8)

Method according to claim 8, wherein the second semiconductor material is silicon carbide.

### Claim 11 (depends on 8)

Method according to claim 8, wherein the second semiconductor material is identical to the first semiconductor material.

### Claim 12 (depends on 8)

Method according to claim 8, wherein the third layer is doped.

### Claim 13 (depends on 8)

Method according to claim 8, further comprising, after step d), a step e) of forming of at least one fourth layer coating the third layer.

### Claim 14 (depends on 1)

Method according to claim 1, wherein, at step c), the thermo-chemical treatment is accompanied by a plasma treatment.

### Claim 15 (depends on 1)

Method according to claim 1, wherein the first layer is made of a transition metal dichalcogenide, preferably of molybdenum disulfide or of tungsten disulfide.

### Claim 16 (depends on 1)

Method according to claim 1, wherein, at step c), the thermo-chemical treatment is carried out at a temperature in the range from 300 to 1,500° C., preferably in the range from 800 to 1,000° C.

### Claim 17 (depends on 1)

Method according to claim 1, wherein the second layer has a thickness in the range from 0.15 to 50 nm, preferably in the range from 1 to 6 nm.