# US 2024/0201586 A1 · Precursors and methods for producing tin-based photoresist

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0201586 A1
- Document ID: US20240201586A1
- Status: Published application
- Kind: A1
- Application number: 18/068,732
- Filed: 2022-12-20
- Published: 2024-06-20
- Earliest claimed: 2022-12-20
- Assignees: Intel Corporation
- Applicants: Intel Corporation
- Inventors: James Blackwell; Charles Cameron Mokhtarzadeh; Lauren Elizabeth Doyle; Eric Mattson; Patrick Theofanis; John J. Plombon; Michael Robinson; Marie Krysak; Paul Meza-Morales; Scott Semproni; Scott B. Clendenning
- Web page: https://patentgrep.com/patent/US20240201586A1

## CPC

- G03F 7/0042: {with inorganic or organometallic light-sensitive compounds not otherwise provided for, e.g. inorganic resists (G03F7/075 takes precedence)}
- G03F 7/0043: {Chalcogenides; Silicon, germanium, arsenic or derivatives thereof; Metals, oxides or alloys thereof (G03F7/0044 takes precedence)}
- G03F 7/038: Macromolecular compounds which are rendered insoluble or differentially wettable (G03F7/075 takes precedence; macromolecular azides G03F7/012; macromolecular diazonium compounds G03F7/021)
- G03F 7/167: {from the gas phase, by plasma deposition (G03F7/2035 takes precedence)}
- G03F 7/168: {Finishing the coated layer, e.g. drying, baking, soaking}
- G03F 7/2004: {characterised by the use of a particular light source, e.g. fluorescent lamps or deep UV light}
- G03F 7/38: Treatment before imagewise removal, e.g. prebaking {(G03F7/265 takes precedence)}
- G03F: PHOTOMECHANICAL PRODUCTION OF TEXTURED OR PATTERNED SURFACES, e.g. FOR PRINTING, FOR PROCESSING OF SEMICONDUCTOR DEVICES; MATERIALS THEREFOR; ORIGINALS THEREFOR; APPARATUS SPECIALLY ADAPTED THEREFOR; (phototypographic composing devices B41B; photosensitive materials or processes for photographic purposes G03C; electrophotography, sensitive layers or processes therefor G03G)

## Abstract

Precursors and methods related to a tin-based photoresist are disclosed herein. In some embodiments, a method for forming a tin-based photoresist may include exposing a tin-containing precursor and a co-reagent to a substrate to form a photoresist having tin clusters; selectively exposing the photoresist to extreme ultraviolet radiation (EUV); and exposing the photoresist to heat to form, in the region, crosslinking between the tin clusters. In some embodiments, the precursor has a formula R1R2Sn(N(CH3)2)2, and R1 and R2 are selected from the group consisting of neo-silyl, neo-pentyl, phenyl, benzyl, methyl-bis(trimethylsilyl), methyl, ethyl, isopropyl, tert-butyl, n-butyl, N,N-dimethylpropylamine, and N, N-dimethlybutylamine. In other embodiments, the precursor includes a chelating alkyl-amine or alkyl-amide ligand featuring a 5 membered or 6 membered tin-based heterocycle bound κ2-C,N with an alkyl group on the ligand backbone, wherein the alkyl group includes methyl, ethyl, vinyl, hydrogen, or tert-butyl.

## Claims

### Claim 1

A method for forming a tin-based photoresist, comprising:
forming a photoresist on a substrate by exposing a precursor and a co-reagent to the substrate, wherein:
the precursor has a formula R1R2Sn(N(CH3)2)2, and R1 and R2 are selected from the group consisting of neo-silyl, neo-pentyl, phenyl, benzyl, methyl-bis(trimethylsilyl), methyl, ethyl, isopropyl, tert-butyl, n-butyl, N,N-dimethylpropylamine, and N,N-dimethlybutylamine;
the co-reagent includes water, carboxylic acid, phosphonic acid, sulphonic acid, or hydrogen peroxide; and
the photoresist includes tin clusters;
selectively exposing the photoresist to extreme ultraviolet radiation (EUV); and
exposing the photoresist to heat to form crosslinking between the tin clusters in an EUV exposed region.

### Claim 2 (depends on 1)

The method of claim 1, wherein R1 and R2 are alkyl groups and the precursor is a dialkyl tin bisamide.

### Claim 3 (depends on 1)

The method of claim 1, wherein selectively exposing the photoresist to EUV includes using a mask to create exposed and unexposed regions of the photoresist.

### Claim 4 (depends on 1)

The method of claim 1, wherein exposing the photoresist to heat includes baking the photoresist at a temperature between 70 degrees Celsius and 250 degrees Celsius.

### Claim 5 (depends on 1)

The method of claim 1, wherein the tin clusters in the photoresist have a drum-shaped structure.

### Claim 6 (depends on 1)

The method of claim 1, wherein the tin clusters are crosslinked by a carbonate bond, a hydroxyl bond, an oxygen bond, or an R—R group bond, the R group including one or more of R1 and R2.

### Claim 7 (depends on 3)

The method of claim 3, further comprising:
developing the photoresist; and
removing the unexposed regions of the photoresist.

### Claim 8 (depends on 1)

The method of claim 1, wherein forming the photoresist includes a chemical vapor deposition (CVD) processor or an atomic layer deposition (ALD) process.

### Claim 9 (depends on 1)

The method of claim 1, wherein a thickness of the photoresist is between 10 nanometers and 100 nanometers.

### Claim 10

A method for forming a tin-based photoresist, comprising:
forming a photoresist on a substrate by exposing a precursor and a co-reagent to the substrate, wherein:
the precursor includes a chelating alkyl-amide ligand, or a chelating alkyl-amine ligand, featuring a 5 or 6 membered tin-based heterocycle bound κ2-C, N with an alkyl group on the ligand backbone;
the co-reagent includes water, carboxylic acid, phosphonic acid, sulphonic acid, or hydrogen peroxide, and
the photoresist includes tin clusters;
selectively exposing the photoresist to extreme ultraviolet radiation (EUV); and
exposing the photoresist to heat to form crosslinking between the tin clusters in an EUV exposed region.

### Claim 11 (depends on 10)

The method of claim 10, wherein the alkyl group includes methyl, ethyl, vinyl, hydrogen, or tert-butyl.

### Claim 12 (depends on 10)

The method of claim 10, wherein the tin clusters in the photoresist have a football-shaped structure.

### Claim 13 (depends on 10)

The method of claim 10, wherein the tin clusters are crosslinked by a carbonate bond, a hydroxyl bond, an oxygen bond, or an R—R group bond, the R group including one or more of an alkyl group, an aryl group, CH2(CHR′)(CH2)nNMeH, and CH2(CHR′)(CH2)nNMe2.

### Claim 14 (depends on 10)

The method of claim 10, wherein selectively exposing the photoresist to EUV includes using a mask to create exposed and unexposed regions of the photoresist, and the method further comprising:
developing the photoresist; and
removing the unexposed regions of the photoresist.

### Claim 15 (depends on 10)

The method of claim 10, wherein forming the photoresist includes a chemical vapor deposition (CVD) process or an atomic layer deposition (ALD) process.

### Claim 16

An apparatus, comprising:
a substrate; and
a photoresist on the substrate, wherein the photoresist includes tin clusters having a drum-shaped structure or a football-shaped structure, and wherein a region of the photoresist includes crosslinked tin clusters.

### Claim 17 (depends on 16)

The apparatus of claim 16, wherein the tin clusters are crosslinked by a carbonate bond, a hydroxyl bond, an oxygen bond, or an R—R group bond, the R group including one or more of neo-silyl, neo-pentyl, phenyl, benzyl, methyl-bis(trimethylsilyl), methyl, ethyl, isopropyl, vinyl, tert-butyl, n-butyl, N,N-dimethylpropylamine, N,N-dimethlybutylamine, CH2(CHR′)(CH2)nNMeH, and CH2(CHR′)(CH2)nNMe2.

### Claim 18 (depends on 16)

The apparatus of claim 16, wherein a thickness of the photoresist is between 10 nanometers and 100 nanometers.

### Claim 19 (depends on 16)

The apparatus of claim 16, wherein the substrate includes a semiconductor material.

### Claim 20 (depends on 16)

The apparatus of claim 16, wherein the photoresist is a negative-type photoresist.