# US 2024/0201422 A1 · Low index of refraction thin film with high hardness coating and method and apparatus to produce same

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0201422 A1
- Document ID: US20240201422A1
- Status: Published application
- Kind: A1
- Application number: 18/391,113
- Filed: 2023-12-20
- Published: 2024-06-20
- Earliest claimed: 2022-12-20
- Applicants: Intevac, Inc.
- Inventors: Thomas P. Nolan; Alexander Vassilievich Demtchouk; Samuel D. Harkness, IV; Jae Ha Choi
- Web page: https://patentgrep.com/patent/US20240201422A1

## CPC

- G02B 1/14: Protective coatings, e.g. hard coatings
- C23C 14/0676: {Oxynitrides}
- C23C 14/35: by application of a magnetic field, e.g. magnetron sputtering {(C23C14/3457 takes precedence)}
- C23C 14/352: {using more than one target (C23C14/56 takes precedence)}
- G02B 1/11: Anti-reflection coatings
- G02B 1/115: Multilayers
- H01J 37/345: {Magnet arrangements in particular for cathodic sputtering apparatus (material of magnets or magnets in general H01F1/00, H01F7/00)}
- G02B: OPTICAL ELEMENTS, SYSTEMS OR APPARATUS
- C23C: COATING METALLIC MATERIAL; COATING MATERIAL WITH METALLIC MATERIAL; SURFACE TREATMENT OF METALLIC MATERIAL BY DIFFUSION INTO THE SURFACE, BY CHEMICAL CONVERSION OR SUBSTITUTION; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATION OR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL (making metal-coated products by extrusion B21C23/22; covering with metal by connecting pre-existing layers to articles, see the relevant places, e.g. B21D39/00, B23K; metallising of glass C03C; metallising mortars, concrete, artificial stone, ceramics or natural stone C04B41/00; enamelling of, or applying a vitreous layer to, metals C23D; treating metal surfaces or coating of metals by electrolysis or electrophoresis C25D; single-crystal film growth C30B; by metallising textiles D06M11/83; decorating textiles by locally metallising D06Q1/04)
- H01J: ELECTRIC DISCHARGE TUBES OR DISCHARGE LAMPS (spark-gaps H01T; electric arc lamps H05B31/00; particle accelerators H05H)

## Abstract

A coated article comprising: a transparent substrate and a protective coating comprising: an adhesion layer formed over the substrate; a protective layer formed over the adhesion layer and may have refractive index of from 1.6 to 1.8; and an anti-reflective layer formed over the protective layer, the anti-reflective layer comprises a plurality of sublayers, wherein at least one sublayer has a refractive index higher than index of said protective layer and at least one sublayer has a refractive index lower than the index of said protective layer.

## Claims

### Claim 1

An optical coating film is provided, comprising an oxynitride of a base cation material, the film having refractive index lower than 1.8, hardness greater than 18 GPa, and thickness above 500 nm but below 3 microns.

### Claim 2 (depends on 1)

The optical coating film of claim 1, wherein the cation material includes silicon, aluminum or silicon and aluminum.

### Claim 3 (depends on 2)

The optical coating film of claim 2, having a density that is higher at the center depth-wise than towards one surface or towards both surfaces.

### Claim 4 (depends on 2)

The optical coating film of claim 2, having one of: a refractive index between n=1.9 to n=2.05 and film layer hardness greater than 20 GPa, a refractive index between n=1.8 to n=1.9 and film layer hardness greater than 18 GPa, a refractive index between n=1.7 to n=1.8 and film layer hardness greater than 15 GPa, a refractive index between n=1.6 to n=1.7 and film layer hardness greater than 12 GPa, a refractive index between n=1.5 to n=1.6 and film layer hardness greater than 10 GPa, and a refractive index between n=1.3 to n=1.5 and film layer hardness greater than 6 GPa.

### Claim 5 (depends on 3)

The optical coating film of claim 3, having one of: a refractive index between n=1.9 to n=2.05 and film layer hardness is greater than 22 GPa, a refractive index between n=1.8 to n=1.9 and film layer hardness is greater than 20 GPa, a refractive index between n=1.7 to n=1.8 and film layer hardness is greater than 17 GPa, a refractive index between n=1.6 to n=1.7 and film layer hardness is greater than 14 GPa, a refractive index between n=1.5 to n=1.6 and film layer hardness is greater than 12 GPa, and a refractive index between n=1.3 to n=1.5 and film layer hardness is greater than 8 GPa.

### Claim 6 (depends on 2)

The optical coating film of claim 2, having compressive stresses below 300 MPa.

### Claim 7 (depends on 3)

The optical coating film of claim 3, having compressive stresses below 100 MPa.

### Claim 8 (depends on 2)

The optical coating film of claim 2, having modulated density throughout film thickness.

### Claim 9

A coated article comprising: a transparent substrate and a protective coating, the protective coating comprising an adhesion layer formed over the substrate; a protective layer formed over the adhesion layer having refractive index of from 1.6 to 1.8; and an anti-reflective layer formed over the protective layer, the anti-reflective layer comprises a plurality of sublayers, wherein at least one sublayer has a refractive index higher than index of said protective layer and at least one sublayer has a refractive index lower than the index of said protective layer.

### Claim 10 (depends on 9)

The coated article of claim 9, further comprising a stress relieving intermediate layer consisting of an oxide containing layer having refractive index n higher than index of the adhesion layer and lower than index of the protective layer.

### Claim 11 (depends on 10)

The coated article of claim 10, wherein the adhesion layer consists of an oxide containing layer having refractive index matching index of the transparent substrate.

### Claim 12 (depends on 10)

The coated article of claim 10, wherein the protective layer has a thickness at least three times greater than the adhesion layer and a refractive index higher than index of the substrate.

### Claim 13 (depends on 9)

The coated article of claim 9, wherein at least one anti-reflective sublayer may have a refractive index below 1.46.

### Claim 14 (depends on 9)

The coated article of claim 9, wherein the anti-reflective layer comprises three sublayers, a first sublayer abutting the protective layer and has a refractive index higher than the protective layer, a second sublayer abutting the first sublayer and has a refractive index higher than the first sublayer, and a third sublayer abutting the second sublayer and has a refractive index lower than the protective layer.

### Claim 15 (depends on 9)

The coated article of claim 9, wherein the anti-reflective layer comprises four sublayers, a first sublayer abutting the protective layer has a refractive index higher than the protective layer, a second sublayer abutting the first sublayer has a refractive index higher than the protective layer but lower than the first sublayer, a third sublayer abutting the second sublayer has a refractive index higher than the second sublayer, and a fourth sublayer abutting the third sublayer has a refractive index lower than the protective layer.

### Claim 16 (depends on 9)

The coated article of claim 9, wherein optical transmittance through said protective coating and said substrate is higher than optical transmittance through said substrate without said protective coating.

### Claim 17 (depends on 9)

The coated article of claim 9, wherein at least one layer of the protective coating has one of: a refractive index between n=1.9 to n=2.05 and film layer hardness is greater than 20 GPa, a refractive index between n=1.8 to n=1.9 and film layer hardness is greater than 18 GPa, a refractive index between n=1.7 to n=1.8 and film layer hardness is greater than 15 GPa, a refractive index between n=1.6 to n=1.7 and film layer hardness is greater than 12 GPa, a refractive index between n=1.5 to n=1.6 and film layer hardness is greater than 10 GPa, and a refractive index between n=1.3 to n=1.5 and film layer hardness is greater than 6 GPa.

### Claim 18 (depends on 9)

The coated article of claim 9, wherein at least one layer of the protective coating has one of: a refractive index between n=1.9 to n=2.05 and film layer hardness is greater than 22 GPa, a refractive index between n=1.8 to n=1.9 and film layer hardness is greater than 20 GPa, a refractive index between n=1.7 to n=1.8 and film layer hardness is greater than 17 GPa, a refractive index between n=1.6 to n=1.7 and film layer hardness is greater than 14 GPa, a refractive index between n=1.5 to n=1.6 and film layer hardness is greater than 12 GPa, and a refractive index between n=1.3 to n=1.5 and film layer hardness is greater than 8 GPa.

### Claim 19 (depends on 9)

The coated article of claim 9, wherein the protective layer has a hardness greater than 18 GPa.

### Claim 20 (depends on 9)

The coated article of claim 9, wherein the protective layer has compressive film stress less than 100 MPa.