# US 2024/0201080 A1 · Method for Determining Adhesive Penetration Into at Least One Porous Coating Material

> Agents: this data is available as JSON from the patentgrep API and MCP server — see https://patentgrep.com/llms.txt

- Number: US 2024/0201080 A1
- Document ID: US20240201080A1
- Status: Published application
- Kind: A1
- Application number: 18/287,366
- Filed: 2022-04-08
- Published: 2024-06-20
- Earliest claimed: 2021-04-19
- Assignees: Flooring Technologies Ltd.
- Applicants: Flooring Technologies Ltd.
- Inventors: Norbert Kalwa
- Web page: https://patentgrep.com/patent/US20240201080A1

## CPC

- G01N 21/3563: for analysing solids; Preparation of samples therefor
- G01N 21/359: using near infrared light
- G01N 21/8422: {Investigating thin films, e.g. matrix isolation method}
- G01N 33/0003: {Composite materials}
- G01N 21/274: {Calibration, base line adjustment, drift correction}
- G01N 2021/8427: {Coatings}
- G01N 2021/8472: {Investigation of composite materials}
- G01N 2201/127: Calibration; base line adjustment; drift compensation
- G01N 2201/129: Using chemometrical methods
- G01N: INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIR CHEMICAL OR PHYSICAL PROPERTIES (measuring or testing apparatus or processes other than immunoassay, involving enzymes or microorganisms C12M, C12Q)

## Abstract

Provided is a method for determining the adhesive penetration into at least one porous coating material which is pressed with at least one carrier plate and at least one adhesive layer arranged on the carrier plate. The adhesive penetrates or rises into the at least one porous coating material during the pressing process.

## Claims

### Claim 1

A method for determining the adhesive penetration into at least one porous coating material which is pressed with at least one carrier plate and at least one adhesive layer arranged on the carrier plate, wherein the adhesive penetrates or rises into the at least one porous coating material during the pressing process,
comprising the steps of:
recording at least one NIR spectrum of several reference samples, each having different values for adhesive penetration into a porous coating material, using at least one NIR measuring head in a wavelength range between 500 nm and 2500 nm, preferably between 700 nm and 2000 nm, particularly preferably between 900 nm and 1700 nm, and especially advantageously between 1000 nm and 1300 nm and/or between 1400 nm and 1550 nm;
determining of adhesive penetration into the porous coating material of said reference samples by means of a mechanical removal of the porous material surface;
correlating of the adhesive penetration determined by mechanical removal with the recorded NIR spectra of said reference samples; and
establishing of a calibration model for the relationship between the spectral data of the NIR spectra and the corresponding adhesive penetrations of the reference samples using multivariate data analysis;
pressing of at least one porous coating material with at least one carrier plate and at least one adhesive layer arranged on the carrier plate,
recording at least one NIR spectrum of the porous coating material pressed with the carrier plate and the adhesive layer using the at least one NIR measuring head in a wavelength range between 500 nm and 2500 nm, preferably between 700 nm and 2000 nm, in particular preferably between 900 nm and 1700 nm and especially advantageously between 1000 nm and 1300 nm and/or between 1400 nm and 1550 nm; and
determining the adhesive penetration into the at least one porous coating material by comparing the NIR spectrum recorded for the porous coating material with the calibration model created.

### Claim 2 (depends on 1)

The method according to claim 1, wherein the NIR spectrum is recorded in a wavelength range between 1100 and 1250 nm and 1400 and 1550 nm.

### Claim 3 (depends on 1)

The method according claim 1, wherein the at least one adhesive is a polyurethane adhesive.

### Claim 4 (depends on 3)

The method according to claim 3, wherein the polyurethane adhesive is based on aromatic polyisocyanates, in particular polydiphenylmethane diisocyanate (PMDI), toluylene diisocyanate (TDI) and/or diphenylmethane diisocyanate (MDI), PMDI being particularly preferred.

### Claim 5 (depends on 1)

The method according to claim 1, wherein the adhesive is a polyvinyl ester adhesive, in particular a polyvinyl acetate adhesive.

### Claim 6 (depends on 1)

The method according to claim 1, wherein in at least one additive is applied to the at least one adhesive layer.

### Claim 7 (depends on 6)

The method according to claim 6, wherein the at least one additive is selected from the following group comprising dyes (e.g. ink), pigments (e.g. color pigments, metallic pigments or reflective pigments) flame retardants (e.g. ammonium polyphosphate, tris(tri-bromo neopentyl) phosphate, zinc borate or boric acid complexes of polyhydric alcohols), agents for increasing conductivity, UV stabilizers, bleaching agents, hydrophobing agents or antimicrobial agents.

### Claim 8 (depends on 6)

The method according to claim 6, wherein the at least one additive is a dye.

### Claim 9 (depends on 1)

The method according to claim 1, wherein the at least one carrier plate is a plate made of a wood material, in particular a particleboard, medium-density fiberboard (MDF), high-density fiberboard (HDF), (OSB) or plywood board, made of plastic, a wood material-plastic mixture or a composite material, a cement fiberboard, gypsum fiberboard or a WPC board (Wood Plastic Composites) or an SPC board (Stone Plastic Composites).

### Claim 10 (depends on 1)

The method according to claim 1, wherein the at least one porous coating material comprises at least one veneer layer, leather material, felt material, nonwoven material and/or such materials which have a porosity in which liquid adhesive can rise during pressing and which are at least partially plastically deformable.

### Claim 11 (depends on 1)

The method according to claim 1, wherein the at least one carrier plate, the at least one adhesive layer disposed on the carrier plate, and the at least one porous coating material are compressed at temperatures between 150 and 200° C., preferably between 170 and 180° C., at a pressure of 30 to 50 kg/cm2, preferably 40 kg/cm2 for 30-120 seconds, preferably 60 to 90 seconds.

### Claim 12 (depends on 1)

The method according to claim 1, wherein spectral data from the entire recorded spectral range are used to create the calibration model.

### Claim 13 (depends on 1)

The method according to claim 1, wherein spectral data from the NIR spectral range between 1000 nm and 1300 nm and/or between 1400 nm and 1550 nm, which are pretreated by means of suitable mathematical methods and are subsequently fed to the multivariate data analysis, are used to create the calibration model.

### Claim 14 (depends on 1)

The method according to claim 1, wherein the determination of the adhesive penetration into the porous coating material is performed continuously and online.